论文

HOT DEFORMATION BEHAVIOR OF A HIGH STRENGTH CONTAINER STEEL COMPOUNDED WITH Nb-B

  • SONG Ren-Ba
Expand
  • 1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2) Hot Rolling Strip Plant, Anshan Iron & Steel Co., Ltd., Anshan 114000

Received date: 2010-04-18

  Revised date: 2010-07-05

  Online published: 2011-01-11

Abstract

Hot deformation behaviors of high strength container steel compounded with Nb-B have been systematically studied through high temperature compression tests on the Gleeble-1500 thermal-mechanical simulator. In the present deformation conditions, there are different relationships between the strain hardening exponent (n) and the true strain (ε) under different strain rates at the deformation temperature of 1423 K; n-ε curves have single peak and single valley at the strain rates of 0.1 s-1 and 1 s-1, while n-ε curves have double peaks and double valleys at the strain rates of 5 s-1 and 15 s-1. During the heat work-hardening process, dislocation strengthening, twin strengthening and precipitation strengthening are the major work-hardening mechanisms of the tested steel. According to Zener-Hollomon and Ludwik equation, the experimental data have been regressed by using nonlinear method, the apparent deformation activation energy (Q) and stress exponent (n) were obtained to be about (428.188±20.109) kJ/mol and 4.923 in the temperature range of 1123 K-1423 K, respectively. Finally, an expression of Z parameter, hot deformation equation and dynamic recrystallization model diagram of the tested steel are established.

Cite this article

SONG Ren-Ba . HOT DEFORMATION BEHAVIOR OF A HIGH STRENGTH CONTAINER STEEL COMPOUNDED WITH Nb-B[J]. Acta Metall Sin, 2011 , 47(1) : 34 -40 . DOI: 10.3724/SP.J.1037.2010.00189

References

[1] Prasad S N, Mediratta S R, Sarma D S. Mater Sci Eng, 2003; A358: 288

[2] He X L, Shang C J, Yang S W. High–performance Low– carbon Bainitic Steel. Beijing: Metallurgical Industry Press, 2008: 6

(贺信莱, 尚成嘉, 杨善武. 高性能低碳贝氏体钢. 北京: 冶金工业出版社, 2008: 6)

[3] Zhang C L, Cai D Y, Zhao T C. Mater Lett, 2004; 58: 1524

[4] Zhao Y T, Yang S W, Shang C J, Wang X M, Liu W, He X L. Mater Sci Eng, 2007; A454–455: 695

[5] Yang S W, Chen Y S. J Mater Sci Eng, 1994; 12(2): 49

(杨善武, 陈钰珊. 材料科学与工程, 1994; 12(2): 49

[6] Shang C J, Wang X M, He X L. Acta Metall Sin, 2008; 44: 287

(尚成嘉, 王学敏, 贺信莱. 金属学报, 2008; 44: 287)

[7] Monteiro S N, Reed–Hill R E. Metall Trans, 1973; 4: 1011

[8] Crussard C. Rev Metall, 1953; 10: 697

[9] Song R B, Xiang J Y, Hou D P. Acta Metall Sin, 2010; 46: 57

(宋仁伯, 项建英, 侯东坡. 金属学报, 2010; 46: 57)

[10] Liu Y Z, Ren X P, Wang Z D. Material Forming Theory.Beijing: National Defence Industry Press, 2004: 337

(刘雅政, 任学平, 王自东. 材料成形理论基础. 北京: 国防工业出版社, 2004: 337)

[11] Bai D Q, We S, Sun W P, Jonas J J. Metall Trans, 1993; 24A: 2151

[12] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 684

[13] Abbs N, Jonas J J. ISIJ Int, 2006; 46: 1679

[14] Ryan N D, McQueen H J. Can Metall Q, 1990; 29(2): 147

[15] Mecking H, Kocks U F. Acta Metall, 1981; 29: 1865

[16] Zener C, Hollomon J H. Appl Phys, 1944; 15: 22

[17] Mcqueen H J. Metall Mater Trans, 2002; 22A: 345

[18] Karhausen K, Kopp R. Steel Res, 1992; 63: 249

[19] Sellars C M, Tegart W J M. Mem Sci Rev Met, 1966; 63: 731

[20] Srinivasan N, Prasad Y R K. J Mater Process Technol, 1995; 51: 171

[21] Lan S H, Lee H J, Lee S H, Ni J, Lai X M, Lee H W, Song J H, Lee M G. Mater Des, 2009; 30: 3879
Outlines

/

〈 〉