Abstract

The high efficiency tungsten inert gas (TIG) welding process has been developed, including active flux welding process, mixed shielded welding process and double shielded welding process, to increase the weld depth/width ratio (D/W$) of conventional TIG welding method. Compared to the active flux method, mixed shielding method can make penetration deeper and the industrialization can be realized easily due to the simplification in operation. Double shielded method can avoid the oxidation of tungsten electrode. The results of experiment and simulation show that the change of the Marangoni convection direction which arises from the adjustment of the oxygen content in the weld pool is one of the main factors contributing to the increase in TIG weld penetration, and the large D/W ratio can be obtained by adjusting the active element content in the liquid pool. High efficiency TIG welding process is not sensitive to welding parameters (welding speed, welding current and electrode gap) and therefore is suitable to be applied in industry easily.

Cite this article

LU Shan-Beng , DONG Wen-Tiao , LI Dian-Zhong , LI Yi-Yi . HIGH EFFICIENCY WELDING PROCESS FOR STAINLESS STEEL MATERIALS[J]. Acta Metall Sin, 2010 , 46(11) : 1347 -1364 . DOI: 10.3724/SP.J.1037.2010.00437

References

[1] Gurevich S M, Zamkov V N, Kushmienko N A. Avtom Svarka, 1965; 9: 1 [2] Gurevich S M, Zamkov V N. Avtom Svarka, 1966; 12: 13 [3] Ludwig H C. Weld J, 1968; 47: 234s [4] Lucas W, Howse D S. Weld Met Fabr, 1996; 64: 11 [5] Howse D S, Lucas W. Sci Technol Weld Joi, 2000; 15: 189 [6] Tanaka M, Shimizu T, Terasaki H, Ushio M, Koshi–ishi F, Yang C L. Sci Technol Weld Join, 2000; 5: 397 [7] Anderson P C J, Wiktorowicz R. Weld Met Fabr, 1996; 64: 108 [8] Paskell T, Lundin C, Castner H. Weld J, 1997; 76: 57s [9] Modenesi P J, Apolinario E R, Pereira I M. J Mater Proc Technol, 2000; 9: 260 [10] Kou M, Sun Z, Pan D. Sci Technol Weld Join, 2001; 6: 17 [11] Savitskii M M, Leskov G I. Avtom Svarka, 1980; 9: 17 [12] Lowke J J, Tanaka M, Ushio M. The 57th Annual Assembly of International Institute of Welding. Osaka, Japan, 2004, IIW Doc. 212–1053–04 [13] Heiple C R, Burgardt P. Weld J, 1985; 64: 159s [14] Heiple C R, Roper J R. Weld J, 1982; 61: 97s [15] Heiple C R, Roper J R, Stagner R T, Aden R J. Weld J, 1983; 62: 72s [16] Heiple C R, Roper J R. Weld J, 1981; 60: 143s [17] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2006; 11: 389 [18] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2007; 12: 120 [19] Lu S P, Fujii H, Sugiyama H, Nogi K. Metall Mater Trans, 2003; 34A: 1901 [20] Lu S P, Fujii H, Sugiyama H, Tanaka M, Nogi K. ISIJ Int, 2003; 43: 1590 [21] Lu S P, Fujii H, Nogi K. Scr Mater, 2004; 51: 271 [22] Lu S P, Fujii H, Nogi K. Sci Technol Weld Join, 2004; 9: 272 [23] Lu S P, Fujii H, Nogi K. Mater Sci Eng, 2004; A380: 290 [24] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2006; 22: 359 [25] Lu S P, Fujii H, Nogi K, Sato T. Sci Technol Weld Join, 2007; 12: 689 [26] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2010; 26: 170 [27] Wu C H, Hao D Q. Physical Chemistry. 1st Ed., Beijing: Machine Building Press, 1988: 138, 287 (吴长春, 郝德庆. 物理化学. 第一版, 北京: 机械工业出版社, 1988: 138, 287) [28] Kraus H G. Weld J, 1989; 68: 269s [29] Bad’yanov B N, Davdov V A, Ivanov V A. Avtom Svarka, 1974; 1: 11 [30] Bad’yanov B N. Avtom Svarka, 1975; 1: 74 [31] Palmer T A, DebRoy T. Weld J, 1996; 75: 197s [32] Sato Y, Dong W, Kokawa H, Kuwana T. ISIJ Int Suppl, 2000; 40: S20 [33] Wada H, Pehlke R D. Metall Trans, 1977; 8B: 675 [34] Dong W, Kokawa H, Sato Y, Tsukamoto S. Metall Mater Trans, 2003; 34B: 75 [35] Katz J D, Kiong T B. Metall Trans, 1989; 20B: 175 [36] Palmer T A, DebRoy T. Sci Technol Weld Join, 1998; 3: 190 [37] Zhu P Y, Lowke J J, Morrow R. J Phys, 1992; 25D: 1221 [38] Lowke J J, Kovitya P, Schmidt H P. J Phys, 1992; 25D: 1601 [39] Zhu P Y, Lowke J J, Morrow R, Haidar J. J Phys, 1995; 28D: 1369 [40] Lowke J J, Morrow R, Haidar J. J Phys, 1997; 30D: 2033 [41] Scott D A, Kovitya P, Haddad G N. J Appl Phys, 1989; 66: 5232 [42] McKelliget J, Szekely J. Metall Trans, 1986; 17A: 1139 [43] Bini R, Monno M, Boulos M I. J Phys, 2006; 39D: 3253 [44] Ushio M, Szekely J, Chang C W. Iron Steel, 1981; 6: 279 [45] Wu C S, Ushio M, Tanaka M. Compt Mater Sci, 1997; 7: 308 [46] Lu S P, Dong W C, Li D Z, Li Y Y. Compt Mater Sci, 2009; 45: 327 [47] Sahoo P, DebRoy T, McNallan M J. Metall Mater Trans, 1988; 19B: 483 [48] DongWC, Lu S P, Li D Z, Li Y Y. Acta Metall Sin, 2008; 44: 249 (董文超, 陆善平, 李殿中, 李依依. 金属学报, 2008; 44: 249) [49] Lu S P, Dong W C, Li D Z, Li Y Y. Sci Tech Weld Join, 2009; 14: 509 [50] Hsu K C, Etemadi K, Pfender E. J Appl Phys, 1983; 54: 1293 [51] Nestor O H. J Appl Phys, 1962; 33: 1638
Outlines

/

〈 〉