论文

STUDY ON THE RUSTING EVOLUTION AND THE PERFORMANCE OF RESISTING TO ATMOSPHERIC CORROSION FOR Mn-Cu STEEL

  • KE Wei ,
  • DONG Jun-Hua
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2010-09-20

  Revised date: 2010-09-29

  Online published: 2010-11-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50499336 and 50971120)

Abstract

The rust evolutions of the corrosion mass gain, the corrosion rate, the chemical composition, and the cross-section of the rust layer versus cycles of dry/wet alternate corrosion test were summarized on the basis of the study progress on the rust layer of Mn-Cu weathering steel. The validity of the cyclic dry/wet corrosion acceleration test simulating the atmospheric corrosion has also been discussed. Moreover, we have described the principle of synergistically improving the corrosion resistance of the rust layer resisting to both coastal atmospheric corrosion and industrial acidic rain atmospheric corrosion through adding alloying elements Cu, Mn and P. Meanwhile, the mechanism of P in the rust layer and the relationship of the ion-selectivity of Mn-Cu steel rust layer and its structure have been discussed.

Cite this article

KE Wei , DONG Jun-Hua . STUDY ON THE RUSTING EVOLUTION AND THE PERFORMANCE OF RESISTING TO ATMOSPHERIC CORROSION FOR Mn-Cu STEEL[J]. Acta Metall Sin, 2010 , 46(11) : 1365 -1378 . DOI: 10.3724/SP.J.1037.2010.00489

References

[1] KeW. China Corrosion Survey Report. Beijing: Chemical Industry Press, 2003: 1 (柯 伟. 中国腐蚀调查报告. 北京: 化学工业出版社, 2003: 1) [2] Cao C N. Material Corrosion in Natural Environment of China. Beijing: Chemical Industry Press, 2005: 2 (曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2005: 2) [3] Liang C F, Hou W T. J Chin Soc Corros Prot, 1998; 18: 1 (梁彩凤, 侯文泰. 中国腐蚀与防护学报, 1998; 18: 1) [4] Committee Membership of Chinese Corrosion and Protection Society. Handbook of Metal Corrosion. Shanghai: Shanghai Science and Technology Press, 1987: 272 (中国腐蚀与防护学会金属腐蚀手册编缉委员会~编. 金属腐蚀手册. 上海: 上海科学技术出版社, 1987: 272) [5] http://en.wikipedia.org/wiki/Weathering steel [6] Masuko N. Tale of Rust. Tokyo: Japanese Standards Association Press, 1990: 47 (增子 升 著, さびのおはなし. 东京: 财团法人日本规格协会, 1990: 47) [7] Matsushima I, Translated by Jin Y K. Low–Alloy Corrosion Resistant Steels. Beijing: Metallurgical Industry Press, 2004: 7 (松岛 岩 著, 靳裕康 译. 低合金耐蚀钢. 北京: 冶金工业出版社, 2004: 7) [8] Hou H R, Fu J Y. Iron Steel, 2004; 39: 72 (侯豁然, 付俊岩. 钢铁, 2004; 39: 72) [9] Leygraf C, Graedel T. Atmospheric Corrosion. NewYork: John Wiley & Sons, 2000: 91 [10] Townsend H E. Outdoor Atmospheric Corrosion. West Conshohocken, PA: American Society for Testing and Materials, 2002: 292 [11] G 85–1998, Standard Practice for Modified Salt Spray (Fog) Testing. American Society for Testing and Materials [12] G 87–1997, Standard Practice for Conducting Moist S02 Tests. American Society for Testing and Materials [13] Japan Industrial Standards JIS K 5621 [14] TB/T 2375–1993, Cyclic Wet/Dry Corrosion Test of Weathering Steel Using for Railway. The Industry Standard of Railway Ministry of China, 1994T (TB/T 2375-1993, 铁路用耐候钢周期浸润腐蚀试验方法, 中华人民共和国铁道部, 1994T) [15] JIS Steel Standards, G3125, Superior Atmospheric Corrosion Resisting Rolled Steels [16] Nishimura T, Katayama H, Noda K, Kodama T. Corrosion, 2000; 56: 935 [17] Dunn D S, Bogart M B, Brossia C S, Cragnolino G A. Corrosion, 2000; 56: 470 [18] Liang C F, Hou W T. J Chin Soc Corros Prot, 2005; 25: 1 (梁彩凤, 侯文泰. 中国腐蚀与防护学报, 2005; 25: 1) [19] Liang C F, Hou W T. J Chin Soc Corros Prot, 2006; 26: 129 (梁彩凤, 侯文泰. 中国腐蚀与防护学报, 2006; 26: 129) [20] Hou W T, Liang C F. Corrosion, 2004; 60: 313 [21] Suzuki I, Masuko N, Hisamatsu Y. Corros Sci, 1979; 19: 521 [22] H. Thomshov, Translated by Hua B D, et al, Theory of Metal Corrosion and Protection. Beijing: Chinese Industrial Press, 1964: 251 (H.д.托马晓夫 著; 华保定 等译, 金属腐蚀及其保护的理论. 北京: 中国工业出版社, 1964: 251) [23] He J X, Qin X Z. Yi P, Yang D M, Li Z H, Lai L Q. Surf Technol, 2006; 35(4): 21 (何建新, 秦晓洲, 易平, 杨德模, 李泽华, 赖丽勤. 表面技术, 2006; 35(4): 21) [24] Kimura M, Kihira H, Ishi Y, Mizoguchi T. 13th Asian–Pacific Corrosion Control Conference, Osaka University, Japan, 16–21 November, 2003 [25] Yamashita M, Shimizu T, Konishi H, Mizuki J. Corros Sci, 2003; 45: 381 [26] Suzuki S, Shinoda K, Sato M, Fujimoto S, Yamashita M, Konishi H, Doi T, Kamimura T, Inoue K, Waseda Y. Corros Sci, 2008; 50: 1761 [27] Kamimura T, Hara S, Miyuki H, Yamashita M, Uchida H. Corros Sci, 2006; 48: 2799 [28] Yamashita M, Konishi H, Kozakura T, Mizuki J, Uchida H. Corros Sci, 2005; 47: 2492 [29] Yamashita M, Miyuki H, Matsuda Y, Nagano H, Misawa T. Corros Sci, 1994; 36: 283 [30] Yan J, Xiong C Q. J Chin Soc Corros Prot, 1986; 6: 1 (严谨, 熊长清. 中国腐蚀与防护学报, 1986; 6: 1) [31] Leygraf C, Graedel T, Translated by Han E H, et al. Atmospheric Corrosion. Beijing: Chemical Industry Press, 2005: 7 (Leygraf C, Graedel T著; 韩恩厚 等译. 大气腐蚀. 北京: 化学工业出版社, 2005: 7) [32] Evans U R. Nature, 1965; 206: 980 [33] Misawa T, Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1974; 14: 279 [34] Townsend H E, Zoccola J C. In: Dean S W, Rhea E C, eds., Atmospheric Corrosion of Metals. Baltimore: ASTM STP 767, 1982: 45 [35] Cao C N. Principle of Electrochemistry on Corrosion. 2nd Ed., Beijing: Chemical Industry Press, 2004: 25 (曹楚南. 腐蚀电化学原理. 第二版, 北京: 化学工业出版社, 2004: 25) [36] Yang X Z, Yang W. Electrochemical Thermodynamics on Metal Corrosion, Potential–pH Diagram and Its Applications. 1st Ed., Beijing: Chemical Industry Press, 1991: 85 (杨熙珍, 杨 武. 金属腐蚀电化学热力学、电位-pH图及其应用. 第一版, 北京: 化学工业出版社, 1991: 85) [37] Dong J H, Han E H, Ke W, MITS Meeting 2006—International Conference of Corrosion, Tokyo, 2006: 43 [38] Dong J, Dong J H, Han E H, Ke W, Liu C M. Corros Sci Prot Technol, 2006; 18: 414 (董 杰, 董俊华, 韩恩厚, 柯伟, 刘春明. 腐蚀科学与防护技术, 2006; 18: 414) [39] Dong J, Dong J H, Han E H, Liu C M, Ke W. Corrs Sci Prot Technol, 2009; 21: 1 (董杰, 董俊华, 韩恩厚, 刘春明, 柯 伟. 腐蚀科学与防护技术, 2009; 21: 1) [40] Dong J H. Corrs Sci Prot Technol, 2010; 22: 261 (董俊华. 腐蚀科学与防护技术, 2010; 22: 261) [41] Dong J H, Han E H, Ke W. Sci Technol Adv Mater, 2007; 8: 559 [42] Dong J H, Ke W. Electrochemistry, 2009; 15: 170 (董俊华, 柯伟. 电化学, 2009; 15: 170) [43] Liang C F, Hou W T, Chen B W, Liang Z J, Luo H S. J Chin Soc Corros Prot, 2000; 20: 135 (梁彩凤, 侯文泰, 陈邦文, 梁泽基, 罗汉生. 中国腐蚀与防护学报, 2000; 20: 135) [44] Ma Y T, Li Y, Wang F H. Mater Chem Phys, 2008; 112: 844 [45] Hou W T, Liang C F. Corrosion, 1999; 55: 65 [46] Han W, Yu G C,Wang Z Y. Corros Sci, 2007; 49: 2920 [47] Han E H, Dong J H, Ke W. Proc 3rd Int Conf Advanced Structural Steels, Gyeongju, 2006: 602 [48] Dong J H, Chen X H, Han E H, Ke W. Iron Steel, 2005; 40: 127 [49] Townsend H E. Corrosion, 2001; 57: 497 [50] Dong J H, Ke W. 2009 Int Symp Steels for Infrasture, Beijing. 2009: 18 (董俊华, 柯伟. 2009年公共用钢国际论坛, 北京, 2009: 18) [51] Hao L, Dong J H, Ke W. Proc 7th Cross–Strait Conference on Materials Corrosion and Protection. Kunming, Aug. 2010 (郝龙, 董俊华, 柯伟. 第七届海峡两岸腐蚀研讨会论文集, 昆明, 2010年8月) [52] Dong J H, KeW. Proc JSCE Materials and Environments 2009, Shibawura, May 2009 [53] Liang C F, Hou W T. Chin J Corros Prot, 1997; 17: 87 (梁彩凤, 侯文泰. 中国腐蚀与防护学报, 1997; 17: 87) [54] Musi´c S, Krehula S, Popovi´c S. Mater Lett, 2004; 58: 444 [55] Dong J H, Ai M R, Han E H, Ke W. Proc 6th Cross–Strait Conference on Materials Corrosion and Protection, Taiwan, Nov. 2008 (董俊华, 艾美蓉, 韩恩厚, 柯伟. 第六届海峡两岸材料腐蚀与防护研讨会, 台湾, 花莲, 2008年11月) [56] Chen X H, Dong J H, Han E H, Ke W. Mater Lett, 2007; 61: 4050 [57] Nishimura T, Katayama H, Noda K, Kodama T. Corros Sci, 2000; 42: 1611 [58] Noda K, Nishimura T, Masuda H, Kodama T. J Jpn Inst Met, 1999; 63: 1133 [59] Konishi H, Yamashita M, Hashida S, Mizuki J, Uchida H. Photon Factory Activity Report 2002, Vol.20, Part B, User’s report, 2003: 125 [60] Tzafaras N, Adlhart W, Jagodzinski H. Acta Crystallogr, 1981; 37A: 104 [61] Donald D W, William H E, Vivian B P, Schumm R H, Halow I. J Phys Chem Ref Data, 1982; 11: 154 [62] Hiroyuki K, Masato Y, Hitoshi U, Jun’ichiro M. Mater Trans, 2005; 46: 337 [63] Hiroyuki K, Masato Y, Hitoshi U, Jun’ichiro M. Mater Trans, 2005; 46: 329 [64] Hiroyuki K, Masato Y, Hitoshi U, Jun’ichiro M. Mater Trans, 2005; 46: 136 [65] Masato Y, Hiroyuki K, Takayuki K, Jun’ichiro M, Hitoshi U. Mater Trans, 2005; 46: 1004 [66] Masato Y, Shuichi H, Takayuki K, Hideaki M, Masugu S. Mater Trans, 2007; 48: 579 [67] Shuichi H, Masato Y, Takayuki K, Masugu S. J Jpn Inst Met, 2007; 71: 346 [68] Masato Y, Hiroyuki Ki, Jun’ichiro M, Hitoshi U. Mater Trans, 2004; 45: 1920 [69] Hiroyuki K, Masato Y, Hitoshi U, Jun’ichiro M. Mater Trans, 2004; 45: 3356 [70] Suzuki S, Shinoda K, Sato M, Fujimoto S, Yamashita M, Konishi H, Doi T, Kamimura T, Hashimoto T, Inoue K. Zairyo–to–Kankyo, 2008; 57: 353