论文

FINITE ELEMENT MODELLING OF TENSILE TEST FOR MICRO–ALLOYED LOW CARBON STEEL AT HIGH TEMPERATURE

  • ZHANG Zhang-Li ,
  • CHEN Hou-Fa ,
  • LIU Bai-Cheng
Expand
  • 1. Key Laboratory for Advanced Materials Processing Technology, Department of Mechanical Engineering, Tsinghua
    University, Beijing 100084
    2. Mines–ParisTech, Centre de Mise en Forme des Mat´eriaux (CEMEF), Sophia Antipolis, France 06904
    3. ArcelorMittal, Research and Development, Maizi`eres–l`es–Metz, France 57823

Received date: 2010-06-13

  Revised date: 2010-08-10

  Online published: 2010-10-11

Supported by

Supported by National Science & Technology Major Project (No.2009ZX04014–082)

Abstract

In view of the numerical inverse identification of constitutive models, a forward numerical modelling of Gleeble tension tests is conducted. A coupled electrical–thermal–mechanical model is proposed for the resolution of electrical, energy and momentum conservation equations by means of finite element method. In momentum equation, the mixed rheological model in multi–phase region (e.g. δ–ferrite and γ austenite (δ+γ mixture)) is developed to consider the δ/γ phase transformation phenomenon for micro–alloyed low carbon steel at high temperature. Experimental and numerical results reveal that significant thermal gradients exist in specimen along longitudinal and radial directions. Such thermal gradients will lead to phase fraction gradient in specimen at high temperature, such as δ fraction gradient or liquid fraction gradient. All these gradients will contribute to the heterogeneous deformation of specimen and severe stress non–uniform distribution, which is the major difficulty for the identification of constitutive models, especially for the simple identification method based on nominal stress–strain. The proposed model can be viewed as an important achievement for further inverse identification methods, which should be used to identify constitutive parameters for steel at hgh temperature in the presence of thermal gradients.

Cite this article

ZHANG Zhang-Li , CHEN Hou-Fa , LIU Bai-Cheng . FINITE ELEMENT MODELLING OF TENSILE TEST FOR MICRO–ALLOYED LOW CARBON STEEL AT HIGH TEMPERATURE[J]. Acta Metall Sin, 2010 , 46(10) : 1206 -1214 . DOI: 10.3724/SP.J.1037.2010.00286

References

[1]Eskin D G, Katgerman L.A quest for a new hot tearing criterion[J].Metallurgical and Materials Transactions A,2007,38(7):1511-1519 [2]Won Y M, Yeo T J, Seol D J, Oh K H.A new criterion for internal crack formation in continuously cast steels[J].Metallurgical and Materials Transactions B,2000,31(4):779-794 [3]Bellet M, Cerri O, Bobadilla M, Chastel Y.Modeling Hot Tearing during Solidification of Steels: Assessment and Improvement of Macroscopic Criteria through the Analysis of Two Experimental Tests[J].Metallurgical and Materials Transactions A,2009,40(11):2705-2717 [4]Rappaz M, Drezet J M, Gremaud M.A new hot-tearing criterion[J].Metallurgical and Materials Transactions A,1999,30(2):449-455 [5]Suzuki M, Yu C H, Emi T.In-situ measurement of fracture strength of solidifying steel shells to predict upper limit of casting speed in continuous caster with oscillating mold[J].ISIJ International,1997,37(4):375-382 [6]Bernhard C, Xia G.Influence of alloying elements on the thermal contraction of peritectic steels during initial solidification[J].,2006,33(1):52-56 [7]Kim K, Oh K H, Lee D N.Mechanical behavior of carbon steels during continuous casting[J].Scripta Materialia,1996,34(2):301-307 [8]Seol D J, Won Y M, Yeo T J, Oh K H, Park J K.High temperature deformation behavior of carbon steel in the austenite and delta-ferrite regions[J].ISIJ International,1999,39(1):91-98 [9]Seol D J, Won Y M, Oh K H, Shin Y C, Yim C H.Mechanical behavior of carbon steels in the temperature range of mushy zone[J].ISIJ International,2000,40(4):356-363 [10]Brown S G R, James J D, Spittle J A.A 3D numerical model of the temperature-time characteristics of specimens tested on a Gleeble thermomechanical simulator[J].Modelling and Simulation in Materials Science and Engineering,1997,5(6):539-548 [11]Norris S D, Wilson I.Application of 3D numerical modelling for thermal profile optimization on the Gleeble thermomechanical simulator[J].Modelling and Simulation in Materials Science and Engineering,1999,7(3):297-309 [12]Solek K, Mitura Z, Kuziak R.A numerical model of the resistance heating system for material tests on a Gleeble simulator[J].Proc. 3rd MIT Conference on Computational Fluid and Solid Mechanics, June 14-17,2005, K.J. Bathe (ed.),2005,:1001-1003 [13]Bellet M, Fachinotti V D.ALE method for solidification modelling[J].,2004,193:4355-4381 [14]Thomas B G, Bellet M.Modeling of stress, distrotion and hot tearing[J].ASM Handbook Volume 15, Casting Division 4: Modeling and Analysis of Casting Processes, American Society of Metals,2008,15:449-461 [15]Bellet M, Heinrich A.A two-dimensional finite element thermomechanical approach to a global stress-strain analysis of steel continuous casting[J].ISIJ International,2004,44(10):1686-1695 [16]Bellet M, Decultieux F, Menai M, Bay F, Levaillant C, Chenot J L, Schmidt P, Svensson I L.Thermomechanics of the cooling stage in casting processes: Three-dimensional finite element analysis and experimental validation[J].Metallurgical and Materials Transactions B,1996,27(1):81-99 [17]Wray P J.Plastic deformation of delta-ferritic iron at intermediate strain rates[J].Metallurgical Transactions A,1976,7(11):1621-1627 [18]Ankem S, Margolin H, Greene C A, Neuberger B W, Oberson P G.Mechanical properties of alloys consisting of two ductile phases[J].Progress in Materials Science,2006,51(5):632-709 [19]Wray P J. PLASTIC-FLOW AND FAILURE OF PLAIN CARBON-STEELS IN FERRITE+AUSTENITE REGION[J].Metals Technology,1981,8(12):466-471 [20]Harste K, Schwerdtfeger K.Thermomechanical properties of iron: Viscoplasticity of ferrite and of austenite-ferrite mixtures[J].,1996,12(5):378-384 [21]Kozlowski P F, Thomas B G, Azzi J A, Hao W.Simple constitutive-equations for steel at high-temperature[J].Metallurgical Transactions A,1992,23(3):903-918 [22]Mizukami H, Shirai Y, Yamanaka A.Prediction of tensile strength and elongation of high alloy steels during solidification[J].ISIJ International,2006,46(7):1040-1046 [23]Koric S, Thomas B G.Thermo-mechanical models of steel solidification based on two elastic visco-plastic constitutive laws[J].,2008,197:408-418