论文

SIMULATION OF SCALE DEPENDENCY ON TENSILE MECHANICAL PROPERTIES OF SINGLE CRYSTAL COPPER NANO–ROD

  • BO Qing-Shun ,
  • ZHONG Zhen ,
  • LIANG Ying-Chun ,
  • CHEN Jia-Xian ,
  • YU Yi-Guo
Expand
  • School of Mechatronics Engineering, Harbin Institute of Technology, Harbin 150001

Received date: 2010-06-03

  Revised date: 2010-08-04

  Online published: 2010-10-11

Supported by

Supported by National Funds for Distinguished Young Scholars (No.50925521) and National Natural Science Foundation of China (No.50705023) and Natural Scientific Research Innovation Foundation in Harbin Institute of Technology (No.HIT.NSRIF.2009012) and Natural Science Foundation of Heilongjiang Province in China (No.E200903)

Abstract

The tension process of single crystal Cu nano–rods with different cross section shapes were simulated by molecular dynamics at atomic scale. Based on centrosymmetry parameter method and combined with the dislocation nucleation theory, the effect of cross–section shape, cross–sectional area and slenderness ratio on the tensile mechanical properties of the nano–rods were analyzed, and the scale dependency of tensile mechanical properties of the single crystal Cu nano–rods has been revealed. The results show that after first yield, the nano–rods produce plastic deformation under the "dislocation nucleation–extended dislocation and sliding–lattice atom cross–slip" mechanism of the alternating cycle. The geometry of cross-section has negligible effects on the tensile initial plasticity of the nano–rods, while it shows apparent effects on the tensile mechanical properties. With the increase of cross–sectional area, two types of nano–rods have the phenomenon of early yield point, yield strength decreases and young’modulus increases. Compared with that of the square cross–sectional nano–rod, the variable rate of yield stess of the circular cross-sectional nano–rod is smaller while the variable rate of young’s modulus is lager. As the cross–sectional area increases to 500 nm2, the young’s modulus of the two types of nano–rods become stable, and is close to the theoretical value of 84 GPa. Moreover, the slenderness ratio of the nano–rods has a slight effect on the tensile mechanical properties when the simulation size increased.

Cite this article

BO Qing-Shun , ZHONG Zhen , LIANG Ying-Chun , CHEN Jia-Xian , YU Yi-Guo . SIMULATION OF SCALE DEPENDENCY ON TENSILE MECHANICAL PROPERTIES OF SINGLE CRYSTAL COPPER NANO–ROD[J]. Acta Metall Sin, 2010 , 46(10) : 1173 -1180 . DOI: 10.3724/SP.J.1037.2010.00266

References

[1] Craihead HG. Science, 2000; 290(24): 1532 [2] Michalske TA, Houston JE. Acta Mater, 1998; 46(2): 391 [3] Greer JR, Oliver WC, Nix WD. Acta Mater, 2005; 53: 1821 [4] R. Komanduri, R. N. Chandrasekaran, L. M. Raff. Science. 2001; 43: 2237 [5] LING Haiyi, NI Xianggui, WANG Xiuxi. Acta Metall Sin, 2001; 37(8): 833 (梁海弋,倪向贵,王秀. 金属学报,2001; 37(8): 833) [6] Liang Haiyi, Wang Xiuxi, Wu Hengan. Acta Mech Sin, 2002; 34(2): 208 (梁海弋,王秀喜,吴恒安,王宇. 力学学报,2002; 34(2): 208) [7] XU Zhou, WANG Xiuxi, LIANG Haiyi. Chinese Journal of Materials Research, 2003; 17(3): 262 (徐洲,王秀喜,梁海弋. 材料研究学报,2003; 17(3): 262) [8] Doyama M, Kogure Y, Nozaki T, Kato Y. Phys Rev, 2003; 202B: 64 [9] T. Nozaki, Masao Doyama, Y. Kogure. Mater Sci Eng A, 2003; 350: 233 [10] Huang Dan, Tao Weiming, Guo Yimu. Acta Mech Solida Sin, 2005; 26(2): 241 (黄丹,陶伟明,郭乙木. 固体力学学报,2005; 26(2): 241) [11]LIANG Yingchun, CHEN Jiaxuan, BAI Qingshun. Acta Metall Sin, 2008; 44(8): 119 (梁迎春,陈家轩,白清顺,唐玉兰,陈明君. 金属学报,2008; 44(8): 119) [12] M. A. Tschopp, D.L. McDowell. J Mech Phys Solids, 2008; 56: 1806 [13] Ning Zhang, Xinhua Yang, Chuanyao Chen. Acta Mech Solida Sin, 2009; 30(3): 231 (张宇,杨新华,陈传尧. 固体力学学报,2009; 30(3): 231) [14] Daw M S, Baskes M I. Phys Rev B, 1984; 29(12): 8486 [15] Diao J K, Gall K, Dunn M L, Zimmerman J A. Acta Mater, 2006; 54: 643 [16] Swope W C, Anderson H C, Berens P H, Wilson K R. J Chem Phys, 1982; 76:637 [17] Nose S A. J Chem Phys, 1984; 84: 511 [18] Hoover W G. Phys Rev, 1985; 31A: 1695 [19] Kelchner C L, Plimpton S J, Hamilton J C. Phys Rev, 1998; 58B: 11085 [20] Guo Yu, Zhuang Zhuo, Li Xiaoyan. Chin J Theoretical and Applied Mech, 2006; 38(3): 398 (郭宇,庄茁,李晓雁. 力学学报,2006; 38: 398) [21] Hirth JP, Lothe J. Theory of Dislocations. New York: John Wiley and Sons, 1982; 757 [22] Mizubayashi H, Matsuno J, Tanimoto H. Scripta Materialia, 1999; 41(4): 443
Outlines

/

〈 〉