论文

RESEARCH PROGRESS ON PLASTIC DEFORMATION MECHANISM OF Mg ALLOYS

  • LIU Qiang
Expand
  • National Engineering Research Centre for Mg Alloys, School of Materials Science and Engineering, Chongqing University, Chongqing 400030

Received date: 2010-09-06

  Revised date: 2010-09-14

  Online published: 2010-11-11

Supported by

Supported by National Basic Research Program of China (No.2007CB613700) and National Natural Science Foundation of China (Nos.50620130096 and  50231030)

Abstract

Possible slip and twinning systems and their critical resolved shear stresses of Mg alloys with hcp structure were described. Research works on plastic deformation behavior and micro-mechanism of different kinds of Mg alloys were reviewed. Both microstructure and texture evolutions during different thermomechanical processes, both dynamic and static recrystallization mechanisms of Mg alloys were described and discussed. Deformation and strengthening mechanisms of precipitates hardening Mg alloys were also addressed with emphasis on the interaction between precipitates and twinning/slip.

Cite this article

LIU Qiang . RESEARCH PROGRESS ON PLASTIC DEFORMATION MECHANISM OF Mg ALLOYS[J]. Acta Metall Sin, 2010 , 46(11) : 1458 -1472 . DOI: 10.3724/SP.J.1037.2010.00446

References

[1] Agnew S R, Duygulu  O. Int J Plast, 2005; 21: 1161 [2] Obara T, Yoshinga H, Morozumi S. Acta Metall, 1973; 21: 845 [3] Stohr J F, Poirier J P. Philos Mag, 1972; 25: 1313 [4] Yoo M H, Agnew S R, Morris J R, Ho K M. Mater Sci Eng, 2001; A319–321: 87 [5] Styczynski A, Hartig C, Bohlen J, Letzig D. Scr Mater, 2004; 50: 943 [6] Agnew S R, Yoo M H, Tome C N. Acta Mater, 2001; 49: 4277 [7] Agnew S R, Tom C N, Brown D W, Holden T M, Vogel S C. Scr Mater, 2003; 48: 1003 [8] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1 [9] Yoo M. Metall Mater Trans, 1981; 12A: 409 [10] Nave M D, Barnett M R. Scr Mater, 2004; 51: 881 [11] Chen Y J, Wang Q D, Roven H J, Liu M P, Karlsen M, Yu Y D, Hjelen J. Scr Mater, 2008; 58: 311 [12] Jiang J, Godfrey A, Liu W, Liu Q. Scr Mater, 2008; 58: 122 [13] Jiang J, Godfrey A, Liu Q. Key Eng Mater, 2007; 353–358: 627 [14] Yang P, Yu Y, Chen L, Mao W. Scr Mater, 2004; 50: 1163 [15] Barnett M R, Keshavarz Z, Beer A G, Ma X. Acta Mater, 2008; 56: 5 [16] Kelly E W, Hosford W F. Trans Metall Soc AIME, 1968; 242: 5 [17] Reed–Hill R E, Robertson W D. Acta Metall, 1957; 5: 728 [18] Wonsiewicz B C, Backofen W A. Metall Soc AIME, 1967; 239: 1422 [19] Yi S B, Davies C H J, Brokmeier H G, Bolmaro R E, Kainer K U, Homeyer J. Acta Mater, 2006; 54: 549 [20] Kleiner S, Uggowitzer P J. Mater Sci Eng, 2004; A379: 258 [21] Jiang J, Godfrey A, Liu Q. Mater Sci Technol, 2005; 21: 1417 [22] Choi S H, Shin E J, Seong B S. Acta Mater, 2007; 55: 4181 [23] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A488: 406 [24] Yin D L, Wang J T, Liu J Q, Zhao X. J Alloys Compd, 2009; 478: 789 [25] Jiang J, Godfrey A, Liu W, Liu Q. Mater Sci Eng, 2008; A483–484: 576 [26] Yan H, Chen R S, Han E H. Mater Sci Eng, 2010; A527: 3317 [27] Jiang L, Jonas J J, Luo A A, Sachdev A K, Godet S. Scr Mater, 2006; 54: 771 [28] Jiang L, Jonas J J, Mishra R K, Luo A A, Sachdev A K, Godet S. Acta Mater, 2007; 55: 3899 [29] Barnett M R, Keshavarz Z, Beer A G, Atwell D. Acta Mater, 2004; 52: 5093 [30] Jain A, Agnew S R. Mater Sci Eng, 2007; A462: 29 [31] Al–Samman T, Li X, Chowdhury S G. Mater Sci Eng, 2010; A527: 3450 [32] Prasad Y V R K, Rao K P. Mater Sci Eng, 2008; A487: 316 [33] Tucker MT, HorstemeyerMF, Gullett PM, El Kadiri H, Whittington W R. Scr Mater, 2009; 60: 182 [34] Wu L, Jain A, Brown D W, Stoica G M, Agnew S R, Clausen B, Fielden D E, Law P K. Acta Mater, 2008; 56: 688 [35] Agnew S R, Duygulu  O. Int J Plast, 2005; 21: 1161 [36] Zeng R C, Han E H, KeW, Dietzel W, Kainer K U, Atrens A. Int J Fatigue, 2010; 32: 411 [37] Barnett M R. Mater Sci Eng, 2007; A464: 1 [38] Barnett M R, Jacob S, Gerard B F, Mullins J G. Scr Mater, 2008; 59: 1035 [39] Walde T, Riedel H. Mater Sci Eng, 2007; A443: 277 [40] Perez–Prado M T, del Valle J A, Contreras J M, Ruano O A. Scr Mater, 2004; 50: 661 [41] del Valle J A, Perez–Prado M T, Ruano O A. Mater Sci Eng, 2003; A355: 68 [42] Fatemi–Varzaneh S M, Zarei–Hanzaki A, Haghshenas M. J Alloys Compd, 2009; 475: 126 [43] Chang L L, Shang E F, Wang Y N, Zhao X, Qi M. Mater Charact, 2009; 60: 487 [44] Koh H, Sakai T, Utsunomiya H, Minamiguchi S. Mater Trans, 2007; 48: 2023 [45] Li H, Hsu E, Szpunar J, Utsunomiya H, Sakai T. J Mater Sci, 2008; 43: 7148 [46] Utsunomiya H, Sakai T, Minamiguchi S, Koh H. High–Speed Heavy Rolling of Magnesium Alloy Sheets, Minerals. Warrendale: Metals & Materials Soc, 2006: 201 [47] Watanabe Y, Sakai T, Utsunomiya H. J Iron Steel Res Int, 2008; 15: 712 [48] Kim W J, Park J D, Wang J Y, Yoon W S. Scr Mater, 2007; 57: 755 [49] Kim W J, Lee J B, Kim W Y, Jeong H T, Jeong H G. Scr Mater, 2007; 56: 309 [50] Kim W J, Jeong H G, Jeong H T. Scr Mater, 2009; 61: 1040 [51] Huang X, Suzuki K, Watazu A, Shigematsu I, Saito N. Scr Mater, 2009; 60: 964 [52] Chino Y, Sassa K, Kamiya A, Mabuchi M. In: 5th Int Conf Processing and Manufacturing of Advanced Materials. Vancouver, Canada: Trans Tech Publications Ltd, 2007: 1615 [53] Chen X P, Shang D, Xiao R, Huang G J, Liu Q. Trans Nonferr Metal Soc, 2010; 20: 589 [54] Lim H K, Lee J Y, Kim D H, Kim W T, Lee J S, Kim D H. Mater Sci Eng, 2009; A506: 63 [55] Shahzad M, Wagner L. Mater Sci Eng, 2009; A506: 141 [56] Chang L L, Wang Y N, Zhao X, Huang J C. Mater Sci Eng, 2008; A496: 512 [57] Liang S J, Liu Z Y, Wang E D. Mater Lett, 2008; 62: 4009 [58] Mishra R K, Gupta A K, Rao P R, Sachdev A K, Kumar A M, Luo A A. Scr Mater, 2008; 59: 562 [59] Park S S, Tang W N, You B S. Mater Lett, 2010; 64: 31 [60] Stanford N, Barnett M R. Mater Sci Eng, 2008; A496: 399 [61] Park S S, You B S, Yoon D J. J Mater Process Technol, 2009; 209: 5940 [62] Uematsu Y, Tokaji K, Kamakura M, Uchida K, Shibata H, Bekku N. Mater Sci Eng, 2006; A434: 131 [63] Azeem M A, Tewari A, Mishra S, Gollapudi S, Ramamurty U. Acta Mater, 2010; 58: 1495 [64] Bohlen J, Yi S B, Swiostek J, Letzig D, Brokmeier H G, Kainer K U. Scr Mater, 2005; 53: 259 [65] Mabuchi M, Iwasaki H, Yanase K, Higashi K. Scr Mater, 1997; 36: 681 [66] Mabuchi M, Ameyama K, Iwasaki H, Higashi K. Acta Mater, 1999; 47: 2047 [67] Mukai T, Yamanoi M,Watanabe H, Higashi K. Scr Mater, 2001; 45: 89 [68] Kim W J, An C W, Kim Y S, Hong S I. Scr Mater, 2002; 47: 39 [69] KimW J, Hong S I, Kim Y S, Min S H, Jeong H T, Lee J D. Acta Mater, 2003; 51: 3293 [70] Perez–Prado M T, del Valle J A, Ruano O A. Scr Mater, 2004; 51: 1093 [71] Perez–Prado M T, del Valle J A, Ruano O A. Mater Lett, 2005; 59: 3299 [72] del Valle J A, P´erez–Prado M T, Ruano O A. Mater Sci Eng, 2005; A410–411: 353 [73] Tan J C, Tan M J. Mater Sci Eng, 2003; A339: 124 [74] Fatemi–Varzaneh S M, Zarei–Hanzaki A, Beladi H. Mater Sci Eng, 2007; A456: 52 [75] Sitdikov O, Kaibyshev R. Mater Trans, 2001; 42: 1928 [76] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843 [77] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A490: 411 [78] Xu S W, Kamado S, Honma T. Scr Mater, 2010; 63: 293 [79] del Valle J A, Ruano O A. Mater Sci Eng, 2008; A487: 473 [80] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199 [81] Zhang Y, Zeng X, Lu C, Ding W. Mater Sci Eng, 2006; A428: 91 [82] Barnett M R. J Light Met, 2001; 1: 167 [83] Yang X Y, Ji Z S, Miura H, Sakai T. Trans Nonferr Met Soc, 2009; 19: 55 [84] Xin R L, Wang B S, Chen X P, Huang G J, Liu Q. Sci China, 2009; 52E: 176 [85] Wang Q, Li D, Blandin J J, Su´ery M, Donnadieu P, Ding W. Mater Sci Eng, 2009; A516: 189 [86] Li X, Yang P, Wang L N, Meng L, Cui F. Mater Sci Eng, 2009; A517: 160 [87] Jager A, Luk´ac P, Gartnerov´a V, Haloda J, Dopita M. Mater Sci Eng, 2006; A432: 20 [88] Perez–Prado M T, Ruano O A. Scr Mater, 2002; 46: 149 [89] Perez–Prado M T, Ruano O A. Scr Mater, 2003; 48: 59 [90] Yang X Y, Zhu Y K, Miura H, Sakai T. Trans Nonferr Met Soc, 2010; 20: 1269 [91] Nie J F. Scr Mater, 2003; 48: 1009 [92] Hutchinson C, Nie J, Gorsse S. Metall Mater Trans, 2005; 36A: 2093 [93] Zhang M X, Kelly P M. Scr Mater, 2003; 48: 379 [94] Matsuda M, Ii S, Kawamura Y, Ikuhara Y, Nishida M. Mater Sci Eng, 2004; A386: 447 [95] Hantzsche K, Bohlen J, Wendt J, Kainer K U, Yi S B, Letzig D. Scr Mater, 2010; 63: 725 [96] Ball E A, Prangnell P B. Scr Metall Mater, 1994; 31: 111 [97] Mackenzie L W F, Davis B, Humphreys F J, Lorimer G W. Mater Sci Technol, 2007; 23: 1173 [98] Senn J W, Agnew S R. Magnesium Technology 2008. New Orleans: TMS, 2008: 153 [99] Senn J W, Agnew S R. Proc Magnesium Technology in the Global Age. Montreal: Canadian Institute of Mining, Metallurgy and Petroleum, 2006: 115 [100] Mackenzie L W F, Pekguleryuz M O. Scr Mater, 2008; 59: 665 [101] Cottam R, Robson J, Lorimer G, Davis B. Mater Sci Eng, 2008; A485: 375
Outlines

/

〈 〉