INFLUENCES ON MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS BY Al CLAD ACCUMULATION

  • KANG Xu ,
  • SHI Qing-Yu ,
  • XUN Kai
Expand
  • 1.Key Laboratory for Advanced Materials Processing Technology, Department of Mechanical Engineering, Tsinghua
    University, Beijing 100084
    2.Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing 100084

Received date: 2010-06-10

  Revised date: 2010-08-17

  Online published: 2010-11-11

Supported by

Supported by National Natural Science Foundation of China (No.50875146)

Abstract

Friction stir welding (FSW) is increasingly used in joining the high strength aluminum alloys. Compared to traditional fusion welding methods, one of advantages of FSW is to obtain defect–free joints more easily. Besides the forms of FSW tools and welding parameters, certain characteristics of the base material can also affect the quality of welded joints. There is usually a protective layer on aluminum alloy surface to prevent corrosion, called Al clad. Generally the mechanical properties of Al clad are significantly lower than those of the base metal. In this paper, tensile and three–point bending tests were applied to investigate the influence of accumulated Al clad on mechanical properties of joints. The mechanism of reducing the mechanical properties of joints, caused by the accumulated Al clad was analyzed by OM, SEM and EDS. The results show that the mechanical properties of the welded joints are lower than those of the joint with which the bottom Al clad on the base material is removed before or after welding. The Al clad tiled on bottom of the base material is squeezed to both sides of the onion ring in the role of the FSW tool and gathered in the bottom after welding. Due to the poorer mechanical properties of Al clad than the base metal, the Al clad aggregation positions become the weak areas in the joints, leading to the formation of the micro cracks in the joints under tensile stress where the micro cracks continue extending to generate macro cracks under the continuous tensile stress. This is the main eason of joint breaking more easily under low strss.

Cite this article

KANG Xu , SHI Qing-Yu , XUN Kai . INFLUENCES ON MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS BY Al CLAD ACCUMULATION[J]. Acta Metall Sin, 2010 , 46(12) : 1517 -1521 . DOI: 10.3724/SP.J.1037.2010.00276

References

[1] Thomas W M, Nicholas E D, Needham J C, Murch M G, Templesmith P, Dawes C J. Gr Br Pat Appl No. 9125978.8, 1991 [2] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1 [3] Colegrove P A, Shercliff H R. Sci Technol Weld Joining, 2003; 8(5): 360 [4] Threadgill P L, Leonard A J, Shercliff H R, Withers P J. Int Mater Rev, 2009; 54(2): 49 [5] Lombard H, Hattingh D G, Steuwer A, James M N. Eng Fract Mech, 2008; 75: 341 [6] Zhou P Z, Li D H, He D Q, Deng H. Trans Chin Weld Inst, 2007; 28(10): 5 (周鹏展, 李东辉, 贺地求, 邓航. 焊接学报, 2007; 28(10): 5) [7] Wang W, Shi Q Y, Li T, Li Hong Ke. Trans Chin Weld Inst, 2008; 29(5): 77 (王伟, 史清宇, 李亭, 李红克. 焊接学报, 2008; 29(5): 77) [8] Zhao J J, Zhang P, Wang W X, Ma L, Hu W W. Trans Chin Weld Inst, 2005; 26(5): 61 (赵军军, 张平, 王卫欣, 马琳, 胡卫伍. 焊接学报, 2005; 26(5): 61) [9] Fu Z H, He D Q, Zhou P Z, Hu A W. Trans Chin Weld Inst, 2006; 27(5): 65 (傅志红, 贺地求, 周鹏展, 胡爱武. 焊接学报, 2006; 27(5): 65) [10] Zhou P Z, Zhong J, He D Q. Chin J Nonferr Metals, 2006; 16(6): 964 (周鹏展, 钟掘, 贺地求. 中国有色金属学报, 2006; 16(6): 964) [11] Elangovan K, Balasubramanian V. Mater Des, 2008; 29: 362 [12] Ke L M, Pan J L, Xing L, Wang S L. Trans Chin Weld Inst, 2007; 28(5): 33 (柯黎明, 潘际銮, 邢丽, 王善林. 焊接学报, 2007; 28(5): 33) [13] Dong C L, Shen C B, Wang Z Z. J Dalian Jiaotong Univ, 2009; 30(6): 42 (董春林, 沈长斌, 王忠志. 大连交通大学学报, 2009; 30(6): 42) [14] Yan K, Ma Z X, Zhang J. J Mater Eng, 2008; 9: 44 (严铿, 马志新, 张健. 材料工程, 2008; 9: 44) [15] Kang X. Bachelor Thesis, Tsinghua University, Beijing, 2008 (康旭. 清华大学学士学位论文, 北京, 2008) [16] Wang X. Master Thesis, Tsinghua University, Beijing, 2008 (王鑫. 清华大学硕士学位论文, 北京, 2009)
Outlines

/

〈 〉