RESEARCH AND APPLICATIONS OF MAGNESIUM IN CHINA

  • ZENG Xiao-Qi
Expand
  • School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240

Received date: 2010-08-09

  Revised date: 2010-09-06

  Online published: 2010-11-11

Abstract

After more than fifty years developing, China has become the largest raw magnesium production country. In the year of 2000, Shi Changxu and his four colleagues, all are academicians of Chinese Academic of Science (CAS), sent a suggestion letter to Minister of Science and Technology (MOST) of China titled “A proposal for speeding up the development of magnesium research and applications”. The suggestion was thus approved by MOST quickly and a major science and technology developing program titled “Developing and industrializing of magnesium alloy” was launched in China during ten--five period. After the ten years development, a great deal of achievements have been attained on advanced magnesium alloys, surface treatment technology and processing technology in our country, and China is stepping for the strong country in magnesium research and applications.

Cite this article

ZENG Xiao-Qi . RESEARCH AND APPLICATIONS OF MAGNESIUM IN CHINA[J]. Acta Metall Sin, 2010 , 46(11) : 1450 -1457 . DOI: 10.3724/SP.J.1037.2010.00386

References

[1] Han W. J World Non–Ferrous, 2002; (3): 19 (韩薇. 世界有色金属, 2002; (3): 19) [2] He L J, Li P J. Cast Technol, 2003; (3): 161 (何良菊, 李培杰. 铸造技术, 2003; (3): 161) [3] Zeng X Q, Wang Q D, Lu Y Z, Ding W J. Mater Sci Eng, 2001; A301: 154 [4] Fu P H. PhD Thesis. Shanghai Jiao Tong University, 2008 (付彭怀. 上海交通大学博士学位论文, 2008) [5] Zhang X M, Xiao Y, Chen J M, Jiang H. Trans Nonferrous Met Soc China, 2006; 16: 518 (张新明, 肖阳, 陈健美, 蒋 浩. 中国有色金属学报, 2006; 16: 518) [6] He S M. PhD Thesis, Shanghai Jiao Tong University, 2007 (何上明. 上海交通大学博士学位论文, 2007) [7] Xu Y W. Proc 12nd Annual Conference of China Magnesium Association, Sep.12, 2009, Hebi, Henan, 2009: 225 (许月旺. 镁业分会第十二届年会论文集, 2009年9月, 河南鹤壁, 2009: 225) [8] Shi C M. Master Dissertation, Shanghai Jiao Tong University, 2010 (石春梅. 上海交通大学硕士学位论文, 2010) [9] J¨urgen O, Besenhard, Martin W. Chem Phys Chem, 2002; 3: 155
Outlines

/

〈 〉