Abstract

The hardening behavior of five Cu–bearing steels during continuous cooling has been studied with the aid of thermo–simulation technique. Optical microscope (OM) and high resolution transmission electron microscopy (HRTEM) were employed to investigate the influence of cooling rate on the precipitation behavior in these steels and their hardness. The results show that during the continuous cooling the second phase precipitates occur in these steels and cause the precipitation hardening. These precipitates are proved to be Cu–rich phases and formed by the way of inter–phase precipitation. The precipitation behavior and hardening effect could be affected by cooling rate and copper content in these steels. When the steels are cooled at a cooling rate between 0.1—1 ℃/s, the second phase precipitates become finer and denser with the increase of cooling rate. Only when the cooling rate is 1 ℃/s the density of the second phase precipitates is the largest. When the cooling rate is quicker than 1 ℃/s, increasing the cooling rate leads to the precipitates being finer and fewer. When the samples are cooled at a rate of 10 ℃/s, there are few precipitates in samples. The Cu–rich phase is the main cause to strengthen these steels. It is also found that when the copper content is less than 1%, the precipitation behavior is unobvious.

Cite this article

LI Chen , YU Hua-Min , CHANG Cheng-Jia , HE Shen-Lai , ZHENG Zhang-An . STUDY ON PRECIPITATION BEHAVIOR OF PHASES CONTAINING Cu IN THE Cu–BEARING STEEL IN CONTINUOUS COOLING PROCESS[J]. Acta Metall Sin, 2010 , 46(12) : 1488 -1494 . DOI: 10.3724/SP.J.1037.2010.00227

References

[1]S. S. Ghasemi Banadkouki, D. P. Dunne. ISIJ Int, 2006; 46: 759 [2]D. P. Dunne, S. S. Ghasemi Banadkouki, D. Yu. ISIJ Int, 1996; 36: 324 [3] Wang X M, Shang C J, Yang S W. Acta Metall Sin, 2005; 41: 1256 (王学敏, 尚成嘉, 杨善武. 金属学报, 2005; 41: 1256. ) [4] Tompson S W, Krauss G. Metall Trans A, 1996; 27A: 1573 [5] S. K. Dhua, Amitava Ray a, D.S. Sarma. Mater Sci EngA. 2001;318: 197 [6] M. T. Miglin, J. P. Hirth, A. R. Rosenfield et al. Metall Trans A, 1986; 17A: 791 [7] Honeycombe W K. translated by FU J Y. Steel-microstructure and properties. Beijing: Metallurgical Industry Press, 1985:77 (Honeycombe W K著,傅俊岩,译. 钢的显微组织和性能. 北京:冶金工业出版社, 1985: 77) [8] Shi D K, Li D C, Meng Q K. Journal of Xi’an Jiaotong University, 1994; 28: 32 (石德坷, 李涤尘, 孟庆奎. 西安交通大学学报, 1994; 28: 32) [9] Thompson S W, Krauss G, Tseng C C. Journal of Materials Science Letters, 1998, 17: 2075 [10] Li H Y, Zhang J F, Geng J F. Material & Heat Treatment. 2006, 35: 38 (李红英,张建飞,耿进峰.热加工工艺, 2006, 35: 38)
Outlines

/

〈 〉