EFFECTS OF HIGH MAGNETIC FIELD ON THE PRECIPITATE AND PROPERTY OF Cu-25%Ag ALLOY

  • LI Gui-Mao ,
  • ZHANG Lin ,
  • YU En-Gang ,
  • ZUO Xiao-Wei ,
  • SHI Ji-Cheng
Expand
  • Key Laboratory of National Education Ministry for Electromagnetic Processing of Material, Northeastern University, Shenyang 110004
WANG Engang

Received date: 2010-05-06

  Revised date: 2010-07-05

  Online published: 2010-09-11

Supported by

Supported by National High Technology Research and Development Program of China (No.2007AA03Z519) and Program of Introducing Talents of Discipline to University (No.B07015)

Abstract

The solidification experiment of Cu-25%Ag alloy used in high field magnet was carried out under high magnetic field, the precipitation of Ag in Cu-rich dendrites, the hardness and the electrical conductivity were investigated. It was found that the Ag phase precipitated exhibites continuous rod-like morphology in the larger Cu-rich dendrites, and exhibites discontinuous particle-like morphology in the smaller Cu-rich dendrites; the number of the Ag particles is more and the size is thinner in the sample solidified under 0 T than under 12 T high magnetic field. The hardness and electrical conductivity of the alloy have changed due to the size variance of Ag precipitates.

Cite this article

LI Gui-Mao , ZHANG Lin , YU En-Gang , ZUO Xiao-Wei , SHI Ji-Cheng . EFFECTS OF HIGH MAGNETIC FIELD ON THE PRECIPITATE AND PROPERTY OF Cu-25%Ag ALLOY[J]. Acta Metall Sin, 2010 , 46(9) : 1128 -1132 . DOI: 10.3724/SP.J.1037.2010.00218

References

[1] Liu J B, Zeng Y W, Meng L. J Alloys and Compd, 2009; 468: 73 [2] Hong S I, Song J S. Metall Mater Trans A, 2001; 32: 985 [3] Gao H Y, Wang J, Shu D, Sun B D. Mater Sci Eng ,A, 2007; 452-453: 367 [4] Mattissen D. Raabe D. Heringhaus F. Acta Metall, 1999; 47: 1627 [5] Sakai Y, Schneider-Muntau H -J. Acta Metall, 1997; 45: 1017 [6] Han K, Embury J D, Sims J R, Campbell L J, Schneider-Muntau H –J, Pantsyrnyi V I, Shikov A, Nikulin A, Vorobieva A. Mater Sci Eng ,A, 1999; 267: 99 [7] Han K, Vasquez A A, Xin Y, Kalu P N. Acta Mater, 2003; 51: 767 [8] Zhang L, Meng L. Mate lett, 2004; 58: 3888 [9] Lin J, Meng L. J Alloys and Compd, 2008; 454: 150 [10] Zhang L, Wang E G, Zuo X W, He J C. Acta Metal Sin, 2008; 44: 165 (张林, 王恩刚, 左小伟, 赫冀成. 金属学报, 2008; 44: 165) [11] Zuo X W, Wang W G, Han H, Zhang L, He J C. Acta Metall Sin, 2009; 44: 1219 (左小伟, 王恩刚, 韩欢, 张林, 赫冀成. 金属学报, 2009; 44: 1219) [12] Li Z F, Dong J, Zeng X, Lu C, Ding W J, Ren Z M. J Alloys and Compd, 2008; 455: 231 [13] Ren X, Chen G Q, Zhou W L, Wu C W, Yuan C, Zhang J S. J Mater Sci Technol, 2009; 25: 379 [14] Duly D, Brechet Y, Chenal B. Acta Metall Mater, 1995; 43: 101 [15] Liu T, Wang Q, Zhang H F, Wang K, Pang X J, He J C. J Alloys and Compd ,2009; 469: 258 [16] Molodov D A, Gottstein G, Heringhaus F, Shvindleman L S. Scripta Mater, 1997; 37: 1207 [17] Sheikh-Alia A D, Molodov D A, Garnestani H. Appl Phys Lett, 2003, 83: 3005 [18] Bevk J, Harbison J P, Bell J L. J Appl Phys, 1978; 49: 6031