论文

MICROSTRUCTURE AND MECHANICAL PROPERTY OF Ti-80%Ni ALLOY PREPARED BY LASER SOLID FORMING

  • XU Xiao-Jing ,
  • LIN Xin ,
  • HUANG Wei-Dong
Expand
  • 1) State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
    2) Aerospace Research Institute of Materials & Processing Technology, Beijing 100076

Received date: 2010-04-21

  Revised date: 2010-06-28

  Online published: 2010-09-11

Supported by

Supported by National Natural Science Foundation of China (No.50971102), National High Technology Research and Development Program of China (No.2006AA03Z0449), National Basic Research Program of China (No.2007CB613805), Program for New Century Excellent Talents in University of China (No.NCET-06-0879), Programme of Introducing Talents of Discipline to Universities (No.08040)

Abstract

Ti-80%Ni alloy was prepared by laser solid forming (LSF) under different processing parameters. The microstructure of the alloy consists of η-TiNi3 phase under low scanning rate v and power P. With the increase of scanning rate, TiNi(B2)+η eutectic appeared, and with the increase of laser power, η laths were broken into bulks and distributed along certain orientation, and (TiNi(B2)+η) devoiced eutectic+inter-lath (TiNi(B2)+η) eutectic appeared. The higher the power is, the finer the η bulks are. And the enhanced power leads to a growing up of (TiNi(B2)+η) eutectic volume fraction. The microstructure became much fine with increasing v and P, while the volumn fraction of hard-brittle η lath decreased, as a result, the laser formability and plasticity of Ti-80%Ni both increased.

Cite this article

XU Xiao-Jing , LIN Xin , HUANG Wei-Dong . MICROSTRUCTURE AND MECHANICAL PROPERTY OF Ti-80%Ni ALLOY PREPARED BY LASER SOLID FORMING[J]. Acta Metall Sin, 2010 , 46(9) : 1081 -1085 . DOI: 10.3724/SP.J.1037.2010.00190

References

[1] Chen B Y. Aero Sci Technol, 1998; 2:13
(陈炳贻. 航空科学技术, 1998; 2: 13)
[2] Suryanarayana C, Fores F H, Rowe R G. Int Mater Rev, 1991; 36: 85
[3] Abbott D H, Arcella F G. Adv Mater Process, 1998; 5: 29
[4] Baughman M S. Rapid Prototyping J, 2005; 11: 41
[5] Lin X, Yue T M, Yang H O, Huang W D. Acta Mater, 2006; 54: 1901
[6] Huang W D, Lin X, Chen J, Liu Z X, Li Y M. Laser Solid Forming. Beijing: National Defense Industry Press, 2007: 107
(黄卫东, 林 鑫, 陈 静, 刘振侠, 李延民. 激光立体成形. 北京: 国防工业出版社, 2007: 107)
[7] Krishnamurthy S, Froes F H. Int Mater Rev, 1989; 34: 297
[8] Radojevic B. Mater Sci Eng, 2001; A304–306: 385
[9] Otsuka K, Ren X. Prog Mater Sci, 2005; 50: 516
[10] Nagarajan R, Ranganathan S, Aoki K, Chattopadhyay K. Mater Trans, JIM, 1997; 138: 406
[11] Li Y M. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2001
(李延民. 西北工业大学博士学位论文, 西安, 2001)
[12] Li Y M, Li J G, Yang H O, Lin X, Chen J, Huang W D. Appl Laser, 2002; 22: 140
(李延民, 李建国, 杨海欧, 林鑫, 陈静, 黄卫东. 应用激光, 2002; 22: 140)
[13] Huang W D, Li Y M, Feng L P, Chen J, Yang H O, Lin X. J Mater Eng, 2002; 3: 40
(黄卫东, 李延民, 冯丽萍, 陈 静, 杨海欧, 林鑫. 材料工程, 2002; 3: 40)
[14] Trived R, Somboonsuk K. Mater Sci Eng, 1984; 65: 65
[15] Kurz W, Fisher D J. Fundamentals of Solidification. Aedermannsdorf, Switzerland: Trans. Tech. 1981: 36

Outlines

/

〈 〉