论文

SIMULATION OF THE PRE-PRECIPITATE IN Ni75Al5Cr20 ALLOY BY MICROSCOPIC PHASE-FIELD METHOD

  • TANG Hong-Kui ,
  • YU Yong-Xin ,
  • CHEN Zheng ,
  • DONG Wei-Beng ,
  • LIU Xiao-Feng ,
  • YU Yong-Biao
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2010-04-21

  Revised date: 2010-06-21

  Online published: 2010-09-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50941020, 10902086 and 50875217), National Natural Science Foundation of Shaanxi Province (Nos.SJ08-ZT05 and SJ08-B14) and Graduate Student Seed Funding of Northwestern Polytechnical University (No.Z2010014)

Abstract

DO22 phase with long period ordered structure is the main strengthening phase in Ni-Al-Cr alloy applied in high temperatures, as it hinders the slipping of dislocations during the deformation. Structure transformation from fcc to DO22 during the ordering process and phase separation have been studied extensively, but there are only a few of reports on the phase transformation in early precipitation stage, especially on the phase transformation of metastable pre-precipitate. In this paper, the microscopic phase--field method was employed to study the pre-precipitate during the transformation from fcc to DO22 in Ni75Al5Cr20 alloy. The early ordering process of Ni75Al5Cr20 alloy are simulated at four different temperatures, and the relationship between the order parameter evolutions of Cr and Al atoms on (001) and (002) planes of disordered fcc solid solution and structure evolution will be investigated. The simulation results demonstrate that the parent phase transformed into L10(M=1) pre-precipitate with long period ordered structure before DO22  phase formed. At the early aging stage, the atomic ordering is proceeded on each plane as the atoms migrate on planes only, and the L10(M=1) pre-precipitate formed in the way of congruent ordering. Then, the further ordering of atoms on (001) plane was induced by the migration of atoms between different planes, and the pre-precipitate with L10(M=1) structure is gradually transformed into DO22 phase. The incubation period and existent time of L10(M=1) phase are prolonged with the temperature increasing, as a result, the incubation period of DO22 phase is longer when the aging temperature is higher, and the formation of L10(M=1) pre--precipitate is easier when the temperature is lower.

Cite this article

TANG Hong-Kui , YU Yong-Xin , CHEN Zheng , DONG Wei-Beng , LIU Xiao-Feng , YU Yong-Biao . SIMULATION OF THE PRE-PRECIPITATE IN Ni75Al5Cr20 ALLOY BY MICROSCOPIC PHASE-FIELD METHOD[J]. Acta Metall Sin, 2010 , 46(9) : 1147 -1152 . DOI: 10.3724/SP.J.1037.2010.00186

References

[1] Reinhard L, Turchi P E A. Phys Rev Lett, 1994; 72: 120
[2] Ni J, Gu B L. Phys Rev Lett, 1997; 79: 3922
[3] Sirota E B, Herhold A B. Science, 1999; 283: 529
[4] Bertrand V D M, Reynard B, McMillan F P, Wilson M, Beck P, Gillet P, Jahn S. Earth Planet Sci Lett, 2007; 261: 469
[5] Wang C, Nuhfer N T, Sridhar S. Metall Mater Trans, 2009; 40B: 1022
[6] Razumov I K. J Eng Phys Thermophys, 2008; 81: 826
[7] Hagihara K, Yokotani N, Umakoshi Y. Intermetallics, 2010; 18: 267
[8] Liu K, Zhang J H, Tang D X, Rokhlin L L, Elkin F M, Meng J. Mater Chem Phys, 2009; 117: 107
[9] Wu Y J, Zeng X Q, Lin D L, Peng L M, Ding W. J Alloys Compd, 2009; 477: 193
[10] Marteau L, Pqreige C, Blavette D. J Microscopy, 2001; 204: 247
[11] Zapolsky H, Ferry S, Sauvage X, Blavette D, Chen L Q. Philos Mag, 2010; 90: 337
[12] Lu Y L, Chen Z, Zhang J. J Central South Univ Technol, 2008; 15: 443
[13] Miao S F, Chen Z, Wang Y X, Xu C, Ma R, Zhang M Y. Acta Metall Sin, 2009; 45: 630
(苗树芳, 陈铮, 王永欣, 徐 聪, 马锐, 张明义. 金属学报, 2009; 45: 630
[14] Kizhner R M, Golosov N S. Russ Phys J, 1979; 22: 290
[15] Clapp P C. Phys Rev, 1971; 4B: 255
[16] Khachaturyan A G. Theory of Structural Transformations in Solids. New York: Wiley, 1983: 129
[17] Poduri R, Chen L Q. Acta Mater, 1998; 46: 1719
[18] Chen L Q. Scr Metall Mater, 1993; 29: 683

Outlines

/