论文

MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH

  • MIN Zhi-Xian ,
  • LIU Lin ,
  • CHEN Jun ,
  • FENG Zhou-Rong ,
  • YU Ling-Shui ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2010-04-21

  Revised date: 2010-06-16

  Online published: 2010-09-11

Supported by

Supported by National Natural Science Foundation of China (No.50827102), National Basic Research Program of China (No.2010CB631202) and the Research Fund of State Key Laboratory of Solidification Processing (NWPU) (No.28-TP-2009)

Abstract

By using liquid metal cooling method, the Ni-based superalloy DZ125 was directionally solidified under planar interface growth condition of drawing rate of 1.5 μm/s. The microstructures at different solidified fractions were examined by OM and SEM. The results showed that the solid/liquid interface is planar and the microstructure evolution undergoes three stages: the γ phase was formed as solidified fraction (fs) was not more than 0.26, and the fine HfC phase sparsely distributed in γ matrix; the coupled γ/MC growth appeared as fs ranged from 0.26 to 0.86, and the morphology of MC was fibrous or plate-like shapes; the γ/γ´ eutectic was obtained as fs was more than and equaled 0.86 0.86, in which the octahedral MC was precipitated simultaneously. EPMA was used to determine the solute distribution along the longitudinal direction of the sample. The contents of Al, Ti, Ta and Mo increased with fs increasing, while the contents of W, Cr and Co decreased. The analysis showed that the microstructure transformation is attributed to macro-scale non-uniform solute distribution which resulted from solute redistribution during directional solidification.

Cite this article

MIN Zhi-Xian , LIU Lin , CHEN Jun , FENG Zhou-Rong , YU Ling-Shui , FU Heng-Zhi . MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH[J]. Acta Metall Sin, 2010 , 46(9) : 1075 -1080 . DOI: 10.3724/SP.J.1037.2010.00185

References

[1] Fu H Z. J Aeronaut Mater, 1998; 18(4): 52
(傅恒志. 航空材料学报, 1998; 18(4): 52)
[2] McLean M. Directionally Solidified Materials for High Temperature Service. UK: The Metals Society, 1983: 11
[3] Liu L, Huang T W, Zhang J, Fu H Z. Mater Lett, 2007; 61: 227
[4] Versnyder F I, Shank M E. Mater Sci Eng, 1970; A6: 213
[5] Tien J K, Gamble R P. Mater Sci Eng, 1971; A8: 152
[6] Bae J S, Lee J H, Kim S S, Jo C Y. Scr Mater, 2001; 45: 50
[7] Sellamuthu R, Giamei A F. Metall Mater Trans, 1986; 16A: 419
[8] Seo S M, Lee J H, Yoo Y S, Jo C Y, Miyahara H, Ogi K. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A. eds, Superalloys 2008, Warrendale, PA: TMS, 2008: 2773
[9] Stefanescu D M. Science and Engineering of Casting Solidification. New York: Kluwer Academic/Plenum Publishers, 2002: 33
[10] Trivedi R, Minyahara H, Mazumder P, Simsek E, Tewari S N. J Cryst Growth, 2001; 222: 365
[11] Tiller W A. Trans TMS–AIME, 1959; 215: 555
[12] Liu L, Sommer F, Fu H Z. Scr Metall Mater, 1994; 30: 584
[13] ZhangWG. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2009
(张卫国. 西北工业大学博士论文, 西安, 2009)
[14] Li R J. Ceramic–Metal Composites. Beijing: Metallurgical Industry Press, 2004: 39
(李荣久. 陶瓷-金属复合材料, 北京: 冶金工业出版社, 2004: 39)
[15] Bhambri A K, Kattamis T Z, Morral J E. Metall Mater Trans, 1986; 6B: 523
[16] Chen J, Lee J H, Jo C Y, Choe S J, Lee Y T. Mater Sci Eng, 1998; A247: 113

Outlines

/

〈 〉