INFLUENCE OF QUENCHING TEMPERATURE ON MARTENSITE TYPE IN Ti-4Al-4.5Mo ALLOY
Received date: 2010-04-03
Revised date: 2010-05-25
Online published: 2010-09-11
There are many discrepancies in the literatures concerning the martensite constitution in the α+β double phase titanium alloys after quenching, so the Ti-4Al-4.5Mo alloy was selected to analysis further the martensite phase transformation in the alloy. The results show that when the quenching temperature is above the (α+β)/β transformation temperature (925 ℃), the hexagonal martensite (α´) formed. With the decrease of quenching temperature, another kind of martensite with orthorhombic structure (α´´) appeared which can coexist with α´ in a certain temperature range. In the sample quenched at 800 ℃, the α´´ disappeared, and the alloy only contains α and β phases. The α´´ martensite reduced the hardness of martensite transformed structure remarkably. EDS analysis indicated that the content of β stabilized element (Mo) is not the only factor determining the martensitic type.
Key words: titanium alloy; quenching; martensitic phase; microhardness
LI Zhang-Fu , LI Ge-Beng , YANG Xi , YANG Ke . INFLUENCE OF QUENCHING TEMPERATURE ON MARTENSITE TYPE IN Ti-4Al-4.5Mo ALLOY[J]. Acta Metall Sin, 2010 , 46(9) : 1061 -1065 . DOI: 10.3724/SP.J.1037.2010.00157
/
| 〈 |
|
〉 |