MICROSTRUCTURE AND RELIABILITY OF LASER JET SOLDER BALL BONDING SOLDER JOINTS

  • YU Xiao-Lin ,
  • LI Meng-Yu ,
  • YU Chun-Jing
Expand
  • 1) Department of Materials Science, Harbin Institute of Technology Shenzhen Graduate School, Shenzhen 518055
    2) State Key Laboratory of Advanced Welding Production Technology, Harbin Institute of Technology, Harbin 150001

Received date: 2010-03-26

  Revised date: 2010-06-15

  Online published: 2010-09-11

Supported by

Supported by High Technology Research and Development Program of China (No.2007AA217022)

Abstract

Laser jet solder ball bonding (LJSBB) technology is a special soldering method developed in cooperation by Fraunhofer Ltd and PacTech Ltd in 1998 to fulfill the specific needs in the packaging of micro-electro-mechanical system (MEMS) and other functional micro-devices. However, the metallurgy characteristics and reliability of the solder joint produced by LJSBB has not been broadly reported. In the present paper, the commonly used Au/Ni/Cu soldering pads were bonded by LJSBB with Sn3.0Ag0.5Cu lead free solder. The effect of laser energy on the interfacial microstructure of solder joint was investigated by SEM and EDS. The reliability of solder joints was also evaluated by thermal cycle treatment and strength test. Results show that due to the limited heat provided by laser beam,  the Au layer of the commonly used Au/Ni/Cu soldering pad cannot completely dissolve into solder during LJSBB process, which leads to the formation of multilayered reactive structure of Au+AuSn+AuSn2+AuSn4 in the interface of solder joint. The AuSn4 locates at the most outside of the reactive structure and presents a needle-like shape. In despite of the brittle nature of Au-Sn intermetallics, the as-soldered joints present a comparatively high strength. However, the strength of solder joint decreases significantly after 100 thermal cycle treatment and keeps nearly unchanged after even more thermal cycle treatment. Metallurgy analysis of joint interface reveals that the thermal cycle treatment plays the roles of promoting the dissipation of residual Au in joint interface through solid state inter-diffusion, and leading to the formation of a quaternary phase of (Au, Ni, Cu, Sn) in interface, which results in weakening of LJSBB solder joint.

Cite this article

YU Xiao-Lin , LI Meng-Yu , YU Chun-Jing . MICROSTRUCTURE AND RELIABILITY OF LASER JET SOLDER BALL BONDING SOLDER JOINTS[J]. Acta Metall Sin, 2010 , 46(9) : 1115 -1120 . DOI: 10.3724/SP.J.1037.2010.00146

References

[1] Ho C E, Tsai S Y, and Kao C R. IEEE Trans Adv Packag, 2001; 24(4): 493-498 [2] Liu W, Wang C Q, Tian Y H, Li M Y. J Alloys Compd, 2008; 458(1-2): 323-329 [3] Tian Y H, Wang C Q, Ge X S. Mat Sci Eng B Solid, 2002; 95(3): 254-262 [4] Jiang C W, Yang S W, Chi Y. Machinery Manufacturing Engineer, 2005; 6: 46-48 (蒋传文, 杨圣文, 池勇. 现代制造工程, 2005; 6: 46-48) [5] Liu X K, Yang S W, Jiang C W. Transactions of the China Welding Institution, 2006; 27(8): 83-87 (刘小康, 杨圣文, 蒋传文. 焊接学报, 2006; 27(8): 83-87) [6] Yin L, Meschter S J, Singler T J. Acta Mater, 2004; 52(10): 2873-2888 [7] Liu Y Y. Master Thesis, Harbin Institute of Technology, 2007. (刘永岳. 哈尔滨工业大学硕士学位论文, 2007) [8] Zribi A, Chromik R R, Presthus R. IEEE Trans Compon Packag Technol, 2000; 23(2): 383-387 [9] Tang W M, He A Q, Liu Q, Ivey D G. Acta Mater, 2008; 56(19): 5818-5827