论文

MICROSTRUCTURES AND MECHANICAL PROPERTIES OF LASER SOLID FORMED NICKLE BASE SUPERALLOY INCONEL 718 PREPARED IN DIFFERENT ATMOSPHERES

  • LIU Kang-Cheng ,
  • LIN Xin ,
  • CHEN Jing ,
  • HUANG Wei-Dong ,
  • YANG Gao-Lin ,
  • HUANG Chun-Beng
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2010-01-26

  Revised date: 2010-05-19

  Online published: 2010-09-11

Supported by

Supported by Program for New Century Excellent Talents in University (No.{\footnotesize\it NCET-06-0879}), National Natural Science Foundation of China (No.50971102) and Program of Introducing  Talents of Discipline to Universities (No.08040)

Abstract

Due to the rapid melting and solidification in laser molten pool, the laser solid forming (LSF) samples have generally much finer microstructure than that of the conventional cast, and are also free of macrosegregation. To date, more and more researchers have reported the application of LSF technology in the forming of superalloy, which contains some easily segregated elements such as Nb, Ti and Al. To prevent the molten pool from oxidation, the LSF process usually should be performed within a protective atmosphere. But in practice, the forming of oxidation-resistant metals are always performed in the air atmosphere and only the molten pool is protected by noble gas. Therefore, it is important to investigate the microstructures and properties of LSF materials prepared in the air and noble gas. In the present study, the microstructures, tensile properties and high cycle fatigue properties of LSF Inconel 718 alloy samples prepared in the air and argon atmospheres were investigated. It is indicated that the microstructures in as-deposited and heat-treated LSF Inconel 718 alloy samples prepared in both atmospheres are similar. The as-deposited microstructure consists of columnar dendrites grew epitaxially along the deposition direction from the substrate, and changes to the equiaxed grains after solution heat treatment due to the recrystallization. The tensile properties of the two kinds of the samples after heat treatment reached the standard for wrought Inconel 718 alloy. The tensile strength of the sample prepared in air is slightly higher than that of the sample prepared in the argon atmosphere, and the high cycle fatigue lifetime of the latter is 30% higher than that of the former, which is related to the fewer defects such as micro pores and small size oxide inclusions existed in the former. The lower high cycle fatigue property of LSF Inconel 718 alloy than that of wrought Inconel 718 alloy is attributed to the metallurgical defects and the coarsening and uneven distribution of the recrystallized grains.

Cite this article

LIU Kang-Cheng , LIN Xin , CHEN Jing , HUANG Wei-Dong , YANG Gao-Lin , HUANG Chun-Beng . MICROSTRUCTURES AND MECHANICAL PROPERTIES OF LASER SOLID FORMED NICKLE BASE SUPERALLOY INCONEL 718 PREPARED IN DIFFERENT ATMOSPHERES[J]. Acta Metall Sin, 2010 , 46(9) : 1047 -1054 . DOI: 10.3724/SP.J.1037.2010.00046

References

[1] Huang W D. Laser Solid Forming. Xi’an: Northwestern Polytechnical University Press, 2007: 10 (黄卫东. 激光立体成形. 西安: 西北工业大学出版社, 2007: 10) [2] Gaumann M, Henry S, Cleton F, Wagniere J D, Kurz W. Mat Sci Eng A, 1999; 271: 232 [3] Blackwell P L. J Mater Process Tech, 2005; 170: 240 [4] Zhao X M, Lin X, Chen J, Xue L, Huang W D. Mat Sci Eng A, 2009; 504: 129 [5] Sun H Q, Zhong M L, Liu W J, He J J, Li X L. In: Deng S S, Matsunawa A, Yao Y L, Zhong M L, eds., Proceeding of Lasers in Material Processing and Manufacturing II, Bellingham WA: SPIE-The International Society for Optical Engineering, 2005: 84 [6] Zhong M L, Yang L, Liu W J, Huang T, He J J. In: Deng S S, Matsunawa A, Yao Y L, Zhong M L, eds., Proceeding of Lasers in Material Processing and Manufacturing II, Bellingham WA: SPIE-The International Society for Optical Engineering, 2005: 59 [7] Zhang F Y, Chen J, Tan H, Lin X, Huang W D. Opt Laser Technol, 2009;41:601 [8] Zhao X M, Chen J, Lin X, Huang W D. Mat Sci Eng A, 2008; 478:119 [9] Lin X, Yang H O, Chen J, Huang W D. Acta Metall Sin, 2006; 42: 361 (林鑫, 杨海鸥, 陈静, 黄卫东. 金属学报,2006; 42: 361) [10] Azadian S, Wei L Y, Warren R. Mater Charact, 2004; 53: 7 [11] Sundararaman M, Mukhopadhyay P, Banerjee S. Metall Trans A, 1988; 19A: 453 [12] Hong S J, Chen W P, Wang T W. Metall Mater Trans A, 2001; 32A: 1887 [13] Slama C, Abdellaoui M. J Alloy Compd, 2000; 306: 277 [14] Editor committee of Chinese Aerospace Material Manual. Chinese Aerospace Material Manual: Deforming Superalloy and Casting Superalloy. 2nd ed. Beijing: Standards Press of China, 2001: 323 (《中国航空材料手册》编辑委员会编. 中国航空材料手册: 变形高温合金、铸造高温合金. 第2版. 北京: 中国标准出版社, 2001: 323) [15] Zhuang J Y, Du J H, Deng Q, Qv J L, Lv X D. Wrought Superalloy GH4169. Beijing: Metallurical Industry Press,2006: 59 (庄景云, 杜金辉,邓群,曲敬龙,吕旭东.变形高温合金GH4169. 北京: 冶金工业出版社, 2006: 59) [16] Murakami Y. Metal Fatigue. Oxford: Elsevier; 2002: 75 [17] Kobayashi K, Yamaguchi K, Hayakawa M, Kimura M. Acta Metall Sin (English lett), 2004; 17: 345 [18] Wang C Z. Materials Properties. Beijing: Beijing University of Technology Press, 2001: 90 (王曾增.材料性能学. 北京: 北京工业大学出版社,2001:90) [19] Rostoker W, Dvorak J R, translated by Liu Y K, Wei F M, Zhou L, Xv Z R. Interpretation of Metallographio Structures. 2nd ed. Shanghai: Shanghai scientific and Technical Publishers, 1984:46 (Rostoker W, Dvorak J R著,刘以宽,魏馥铭,周莲,徐佐仁译. 金相组织解说. 第2版. 上海:上海科学技术出版社, 1984: 46) [20] Merrick H F. Metall Trans. 1974; 5: 891