论文

STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE

  • YANG Wen-Tiao ,
  • WANG Meng-Piao ,
  • ZHANG Qian ,
  • CHENG Xiao-Fei ,
  • YU Zheng-An
Expand
  • 1.School of Materials Science and Engineering, Central South University, Changsha 410083
    2.Key laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University,
    Changsha 410083

Received date: 2010-05-11

  Revised date: 2010-08-23

  Online published: 2010-11-11

Supported by

Supported by High Technology Research and Development Program of China (No.2006AA03Z517)

Abstract

The single–stage aging process, microstructure evolution during the precipitation process and crystal structure and orientation relationships between the β′′ phase and matrix were studied by means of conventional transmission electron microscopy (TEM), high resolution transmission electron microscopy (HRTEM) and hardness testing in 6005A aluminum alloy used for rail traffic vehicle. The results show that 6005A alloy can reach its peak hardness after aging at 175 for 12 h, and maintain it for a longer time. It is found that there exist clusters or GP zones in this alloy at early stage of aging and the β′′  phase at the peak–aging stage. After the peak–aging, the β′′  phase as a main strengthening phase in 6005A aluminum alloy continues being precipitated from matrix for a long time. β′′  phase has a C–centered monoclinic lattice with the lattice parameters a=(1.52±0.04) nm, b=0.405 nm, c=(0.67±0.04) nm, β=105.26?. The crystallographic orientation relationship between the β′′  phase and matrix is found as follows: (010)β′′ //(001)Al, [200]β′′ //[230]Al, [002]β′′ //[¯310]Al. And, the precipitation sequence with aging time in 6005A aluminum alloy can be described: super saturated solid solution (SSS) →clusters→GP zone→ metastable β′′  phase→ metastable β′  phase+Q′ phase→ stable β(Mg2Si) phase+Q phase.

Cite this article

YANG Wen-Tiao , WANG Meng-Piao , ZHANG Qian , CHENG Xiao-Fei , YU Zheng-An . STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE[J]. Acta Metall Sin, 2010 , 46(12) : 1481 -1487 . DOI: 10.3724/SP.J.1037.2010.00223

References

[1] Hirsch J. Mater Sci Forum, 1997; 242:33 [2] Miller W S, Zhuang L, Bottema J, Wittebrood A J, De Smet P, Haszler A, Vieregge A. Mat Sci Eng A-Struct,2000; 250(1):37 [3]Moons T, Ratchev P, De Smet P, Verlinden B, Van Houtte P. Scripta Mater, 1996; 35(8):937 [4] Birol Y. Eng Fail Anal, 2010; 17(5):1110 [5] Xiao C W, Wang M P, Wang Z A, Li Z, Guo M X. Chin J Nonferrous Met, 2003;13(3):635 (肖从文, 汪明朴, 王正安, 李周, 郭明星. 中国有色金属学报,2003;13(3):635) [6] Buha J, Lumley R Crosky A G, Hono K. Acta Mater, 2007; 55(9):3015 [7] Yang C G, Shan J G, Xiong W. Welding & Joining, 2009; 10:13 (杨成功 ,单际国, 熊伟. 焊接, 2009; 10:13) [8] Birol Y. Scripta Mater, 2005; 52(3):169 [9] Andersen S J. Metall Mater Trans A, 1995; 26:1931 [10] Zandergen H W, Andersen S J, Jansen J. Science, 1997; 277:1221 [11] Andersen S J, Zandergen H W, Jansen J, Tr?holt C, Tundal U, Reiso O. Acta Mater,1998; 46(9):3283 [12] Edwards G A, Stiller K, Dunlop G L, Couper M J.Acta Mater, 1998; 46(11):3893 [13] Chakrabarti D J,Yingguo P, Laughlin DE. Mater Sci Forum, 2002; 392:857 [14] Wang X, Esmaeili D, Lloyd D J. Metall Mater Trans A, 2006; 37:2691 [15] Marioara C D, Andersen S J, Zandbergen H W, Holmestad R. Metall Mater Trans A, 2005;36:691 [16] Murayama M, Hono K. Acta Mater, 1999; 47(5):1537 [17] Gaber A, Mossad A, Matsuda K, Kawabata T, Yamazaki T, Ikeno S. J Alloy Compd, 2007; 432:149 [18] Yassar R S, Field D P, Weiland H. Scripta Mater, 2005; 53: 299 [19] Matsuda K, Ikeno S, Matsui H, Sato T. Metall Mater Trans A, 2005; 36:2007