Reverted DZ40M alloy was refined by melting treatment (MT) which tensile, stress–rupture and creep properties were measured. MT can reduce the content of N from 0.0078% to 0.0024%, as well as the content of S from 0.0015% to 0.0007%. It makes impurity elements such as N, O and S being removed, and the shrinkage area being decreased. MT improves the tensile strength and ductility of reverted DZ40M alloy, especially elongations at room temperature and 1000 ℃ are increased about twice as high as those by regular melting (RM). In addition MT prolongs the stress–rupture lives, and improves the creep properties of reverted DZ40M alloy. Therefore stress–rupture and creep properties of reverted DZ40M alloys are upgraded greatly.
YANG Jin-Xia
,
XUN Xiao-Feng
,
HU Zhuang-Qi
,
SANG Zhi-Ru
,
ZHENG Qi
,
LANG Hai-Xia
. EFFECTS OF MELTING TREATMENTS ON THE MECHANICAL PROPERTIES OF REVERTED DZ40M ALLOY[J]. Acta Metall Sin, 2010
, 46(12)
: 1511
-1516
.
DOI: 10.3724/SP.J.1037.2010.00142
[1] Li Z J. Master Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2005
(李志军. 中国科学院金属研究所硕士学位论文, 沈阳, 2005)
[2] Li Z J, Zhou L Z, Yao J. Mater Eng, 2005; (8): 24
(李志军, 周兰章, 姚俊. 材料工程, 2005; (8): 24)
[3] Huang X B. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1997
(黄学兵. 中国科学院金属研究所博士学位论文, 沈阳, 1997)
[4] Yuan C, Wang T L. Acta Metall Sin, 2000; 36: 961
(袁超, 王铁利. 金属学报, 2000; 36: 961)
[5] Yuan C, Guo J T, Zang Z X, Lai W H, Liu Y M, Li H L. Trans Nonferrous Met Soc China, 2006; 16: 453
(袁超, 郭建亭, 藏志新, 赖万慧, 刘一鸣, 李洪亮. 中国有色金属学报, 2006; 16: 453)
[6] Zhou B, Zhao M H, Zhao J C. J Iron Steel Res, 2003; 15(7): 196
(周 波, 赵明汉, 赵京晨. 钢铁研究学报, 2003; 15(7): 196)
[7] Yu Q, Song J X, Wang D G, Qu S Y, Li Q. Mater Eng, 2006; (6): 10
(余乾, 宋尽霞, 王定刚, 曲士昱, 李青. 材料工程, 2006; (6): 10)
[8] Niu J P. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2002
(牛建平. 中国科学院金属研究所博士学位论文, 沈阳, 2002)
[9] Niu J P, Yang K N, Jin T, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2001; 37: 499
(牛建平, 杨克努, 金涛, 孙晓峰, 管恒荣, 胡壮麒. 金属学报, 2001; 37: 499)
[10] Niu J P, Yang K N, Sun X F, Jin T, Guan H R, Hu Z Q. Rare Met Mater Eng, 2003; 32: 63
(牛建平, 杨克努, 孙晓峰, 金涛, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2003; 32: 63)
[11] Wang T L. PhD Thesis, Northeastern University, Shenyang, 2000
(王铁利. 东北大学博士学位论文, 沈阳, 2000)
[12] Yin F S, Guan H R, Sun X F, Hu Z Q. Acta Metall Sin, 2005, 41: 1190
(殷凤仕, 管恒荣, 孙晓峰, 胡壮麒. 金属学报, 2005, 41: 1190)
[13] Jiang W H. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1999
(姜文辉. 中国科学院金属研究所博士学位论文, 沈阳, 1999)
[14] Yao X D. China Aeronautical Materials Handbook. Beijing: China Standard Press, 2001: 765
(姚向东. 中国航空材料手册. 北京: 中国标准出版社, 2001: 765)