论文

EFFECT OF ULTRASONIC VIBRATION ON THE DIRECTIONAL SOLIDIFICATION OF SCN-3%ETH MODEL ALLOY

  • DUAN Meng-Meng ,
  • CHEN Zhang-Le
Expand
  • Shaanxi Key Laboratory of Condensed Matter Structures and Properties, School of Science, Northwestern Polytechnical University, Xi'an 710072

Received date: 2010-02-25

  Revised date: 2010-05-04

  Online published: 2010-07-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50331040 and 60171034)

Abstract

The directional solidification process of SCN-3%ETH model alloy under 27.5 kHz ultrasonic vibration is studied in this paper. The results show that the interface growth is restrained because of the effect of ultrasonic vibration. The radius of curvature on the interface increases as the ultrasonic action time increase. When the ultrasonic vibration is removed from the melt, the refined cellular structure is formed. Because the impact of transient high temperature and pressure generated by the cavitation effect and stirring action of the acoustic streaming and shearing action caused by forced vibration, part of the dendrite tips are fractured. The interface growth rate decreases as the ultrasonic action time increase. Cavitation effects and high-frequency forced vibration caused by ultrasonic vibration in the melt are main reasons for interface growth rate change.

Cite this article

DUAN Meng-Meng , CHEN Zhang-Le . EFFECT OF ULTRASONIC VIBRATION ON THE DIRECTIONAL SOLIDIFICATION OF SCN-3%ETH MODEL ALLOY[J]. Acta Metall Sin, 2010 , 46(7) : 885 -889 . DOI: 10.3724/SP.J.1037.2010.00095

References

[1] Ning S B. Master Thesis, Dalian University of Technology, 2006
(宁韶斌. 大连理工大学硕士学位论文, 2006)
[2] Gao S L, Zhai Q J, Qi F P, Fu Z Y, Gong Y Y. Mater Rev, 2002; 16: 5
(高守雷, 翟启杰, 戚飞鹏, 富知愚, 龚永勇. 材料导报, 2002; 16: 5)
[3] Olmo A, Baena R, Risco R. Int J Refrigeration, 2008; 31: 262
[4] Li T, Lin X, Huang W D. Acta Mater, 2006; 54: 4815
[5] Nakagawa K, Hottot A, Vessot S, Andrieu J. J Chem Eng Process, 2006; 45: 783
[6] Ramirez A, Qian M, Davis B, Wilks T, StJohn D H. Scr Mater, 2008; 59: 19
[7] Taghavi F, Saghafian H, Kharrazi Y H K. Mater Des, 2009; 30: 1604
[8] Li X T, Gao X P, Li T J, Li X M, Jin J Z, Yin G M. Rare Met Mater Eng, 2007; 36: 377
(李新涛, 高学鹏, 李廷举, 李喜孟, 金俊泽, 殷国茂. 稀有金属材料与工程, 2007; 36: 377)
[9] Li J W, Momono T, Fu Y, Jia Z, Tayu Y. Trans Nonferrous Met Soc China, 2007; 17: 691
[10] Chirita G, Stefanescu I, Soares D, Silva F S. Mater Des, 2009; 30: 1575
[11] Liu X B, Osawa Y, Takamori S, Mukai T. Mater Sci Eng, 2008; A487: 120
[12] Gao X P, Li X T, QieXW, Wu Y P, Li X M, Li T J. Acta Phys Sin, 2007; 56: 1188
(高学鹏, 李新涛, 郄喜望, 吴亚萍, 李喜孟, 李廷举. 物理学报, 2007; 56: 1188)
[13] Zhai W, Hong Z Y, Wei B B. Sci China, 2007; 37G: 367
(翟薇, 洪振宇, 魏炳波. 中国科学, 2007; 37G: 367)
[14] Feng W J. Master Thesis, Dalian University of Technology, 2004
(冯伟骏. 大连理工大学硕士学位论文, 2004)
[15] Jackson K A, Hunt J D. Acta Metall, 1965; 13: 1212
[16] Shan B W, Lin X, Wei L, Huang W D. Acta Phys Sin, 2009; 58: 1132
(单博炜, 林 鑫, 魏雷, 黄卫东. 物理学报, 2009; 58: 1132)
[17] Zhai W, Wang N, Wei B B. Acta Phys Sin, 2007; 56: 2353
(翟薇, 王 楠, 魏炳波. 物理学报, 2007; 56: 2353)
[18] Kaya H, Cadirli E, Keslioglu K, Marasli N. J Cryst Growth, 2005; 276: 583
[19] Yoshioka H, Tada Y, Hayashi Y. Acta Mater, 2004; 52: 1515
[20] Huang W D, Lin X, Li T, Wang L L, Inatomi Y. Acta Phys Sin, 2004; 53; 3978
(黄卫东, 林鑫, 李涛, 王琳琳, Inatomi Y. 物理学报, 2004; 53: 3978)
[21] Zhao Z X. Hot Work Technol, 1999; 5: 10
(赵忠兴. 热加工工艺, 1999; 5: 10)
[22] Kuijpers M W A, Eck D V, Kemmere M F, Keurentjes J T F. Science, 2002; 298: 1969
[23] Rayleigh L. Philos Mag, 1917; 34: 94
[24] Campbell J. Int Met Rev, 1981; 26: 71
[25] Neppiras E A, Noltingk B E. Proc Phys Soc, 1951; 64B: 1032
[26] Feng R, Li H M. Sonochemistry and its Applications. Hefei: Anhui Science & Technology Publishing House, 1992: 87
(冯若, 李化茂. 声化学及其应用. 合肥: 安徽科学技术出版社, 1992: 87)
[27] Ma D Y. Acta Acustica, 1992; 17: 241
(马大猷. 声学学报, 1992; 17: 241)
.  ''y, 1992; 17: 241)
[28] Langer J S. M¨uller–Krumbhaar H. J Cryst Growth, 1977; 42: 11

Outlines

/

〈 〉