论文

EXPERIMENTAL RESEARCH ON MELTING SURFACE BEHAVIOR IN MOLD UNDER COMPOUND MAGNETIC FIELD

  • DENG An-Yuan ,
  • YU En-Gang ,
  • SHI Ji-Cheng ,
  • ZHANG Xin-Wu ,
  • XU Yong-Xi
Expand
  • Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819

Received date: 2010-02-02

  Revised date: 2010-03-05

  Online published: 2010-08-10

Supported by

Supported by National High Technology Research and Development Program of China (No.2007AA03Z519), National Natural Science Foundation of China (Nos.50604005 and 50834010) and the Program of Introducing Talents of Discipline to Universities (No.B07015)

Abstract

In order to control stability of molten metal surface during electromagnetic continuous casting, the stabilities of melting surface under applications of an alternating magnetic field and a compound magnetic field were investigated experimentally. The melting surface behavior of the Sn–32%Pb–52%Bi alloy with low–melting point was measured by using a laser displacement sensor and visualized by using a high–speed video camera. The Fourier analysis method was introduced to reveal the fluctuation characteristics of free surface. It is experimentally found that when only alternating field is applied, the free surface keeps fluctuating. However, with increasing the alternating magnetic flux density, two statuses of the free surface, the stable camber deformation and the swinging phenomenon, can be observed orderly, and during swinging, the square–like or triangular prism–like deformations appear stochastically. The Fourier analysis indicates that the dominant fluctuation frequency at free surface center increases with increasing the alternating magnetic flux density. After simultaneously superposing a transverse static magnetic field within 0—1.44 T, the unstable swinging behavior of free surface can be remarkably controlled. Increase of static magnetic flux density can make the swinging amplitude reduce. Also the static magnetic field can effectively damp the free surface fluctuation. The stretch phenomenon was observed due to application of high static magnetic field in compound field, also a series of regular surface fluctuations appeared on free surface. There is an appropriate range of the static magnetic flux density to obtain more stable free surface, lower fluctuation amplitude and dominant fluctuation frequency.

Cite this article

DENG An-Yuan , YU En-Gang , SHI Ji-Cheng , ZHANG Xin-Wu , XU Yong-Xi . EXPERIMENTAL RESEARCH ON MELTING SURFACE BEHAVIOR IN MOLD UNDER COMPOUND MAGNETIC FIELD[J]. Acta Metall Sin, 2010 , 46(8) : 1018 -1024 . DOI: 10.3724/SP.J.1037.2010.00066

References

[1] Vives C. Metall Trans, B, 1989; 20B(10): 623 [2] Zhu X R, Harding R A, Campbell J. Appl Math Modeling, 1997; 21: 207 [3] Zeng D H, Mao B, E X Q. Acta Metall Sin, 2000; 36(2): 162 (曾德鸿,毛斌,鄂学全. 金属学报, 2000; 36(2): 162) [4] Na X Z, Zhang X Z, Qiu S T, Gan Y. Acta Metal Sin, 2002; 38(1): 104(那贤昭,张兴中,仇圣桃,干勇. 金属学报,2002; 38(l):105) [5] Xia X J, Wang H M, Dai Q X, Li G R, Zhao Y T. The Chinese Journal of Nonferrous Metals, 2008; 18(3):529(夏小江,王宏明,戴起勋,李桂荣,赵玉涛. 中国有色金属学报,2008; 18(3):529) [6] He J C, Wang E G, Deng A Y, Yu G W, Wang Q, Zhang Y J, Chen Z P, Zhou Y M, Feng C B. 4th International Conference on Electromagnetic Processing of Materials, , Lylons:2003: 195 [7] Nakata H, Inoue T, Mori H, Ayata K, Murakami T, Kominami T. ISIJ Int, 2002; 42 (3): 264 [8] Park J, Kim H, Jeong H, Kim G, Cho M J, Chung J S, Yoon M, Kim K R, Choi J. ISIJ Int, 2003; 43(6): 813 [9] Fautrelle Y, Perrier D, Etay J. ISIJ Int, 2003; 43(6): 801 [10] Karcher C, Minchenya V. International Scientific Colloquium Modeling for Electromagnetic Processing, Hannover: 2008: 143 [11] Zhang B, Li T J, Jia F, Ji S H. Foundry Technology, 2002; 23(6): 388(张斌, 李廷举, 贾非, 季首华. 铸造技术, 2002; 23(6): 388) [12] Xu X J, Deng A Y, Wang E G, Zhang L T, Zhang X W, Zhang Y J, He J C. Acta Metall Sin, 2009; 45(4):464(许秀杰,邓安元,王恩刚,张林涛,张兴武,张永杰,赫冀成. 金属学报,2009; 45(4):464) [13] Zhang H X, Liang J G, He Q W, Han Y G. Laigang Science & Technology,2007;(4):26 (张海霞,梁建国,何庆文,韩永刚. 莱钢科技,2007;(4):26) [14] Wang W X, Wang Y,Chi J H. Iron Steel Vanadium Titanium, 2006; 27(3):63(王文学,王雨,迟景濒. 钢铁钒钛,2006; 27(3):63)
Outlines

/

〈 〉