论文

THE RELAXATION PHENOMENON DURING MELT SUPERHEATING TREATMENT OF DZ125 ALLOY

  • YU Chang-Shuai ,
  • ZOU Min-Meng ,
  • ZHANG Jun ,
  • FU Heng-Zhi ,
  • LIU Lin
Expand
  • State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi’an 710072

Received date: 2009-12-18

  Revised date: 2010-04-09

  Online published: 2010-06-11

Supported by

Supported by National Natural Science Foundation of China (No.50931004), National Basic Research Program of China (Nos.2006CB605202 and 2010CB631202) and National High Technology Research and Development Program of China (No.2007AA03Z552)

Abstract

As a precipitation hardened unidirectionally solidified Ni-based superalloy, DZ125 has been extensively applied as structural materials in advanced aeroengine for gas turbine blades and vanes operating at elevated temperatures. The solidification microstructure of alloy plays an important role in determining the alloy's mechanical properties. For a given alloy, the thermal history of alloy melt has an obvious influence on the final solidification microstructure. However, previous researches mainly focused on melt superheating temperature. There are few investigations about the influence of the relaxation process of alloy melt on the solidification structure. In this paper, under the same conditions of processing parameters, e.g.,  olid/liquid interface temperature gradient, withdrawing velocity, by changing the melt holding time, the relaxation phenomenon during melt superheating treatment of DZ125 was investigated. The melt was superheated to 1650 ℃ and kept for 30 min, and then it was rapidly cooled down to 1500 ℃. In order to study the relaxation phenomenon during melt superheating treatment, the melt was held for 15, 30 and 60 min, respectively, and then was withdrawn into the Ga-In-Sn liquid metal bath at a rate of 50 μm/s. The results show that dendrite arm spacing, segregation ratios, size and morphology of γ' phase and γ+γ' eutectic did not change with the increase of the holding time when melt holding time was less than 30 min. But, when melt holding time was prolonged to 60 min, the dendrite arm spacing, γ+γ' eutectic and the size of γ' phase in interdendrite area increased, and the segregation becomes serious, but the γ' phase on dendrite trunk was lightly refined. The morphology of MC carbide mainly showed disconnected blocky and nodule, and unchanged with the prolongation of holding time. These changes in solidification structure should be primarily attributed to the influence of relaxation process on melt structure. When the melt holding time was less than 30 min, there was no evidently change in melt structure. But, further prolonging melt holding time to 60 min, the melt structure had obvious variation. This variation affected the solidification processing and finally solidification structure. Therefore, the variation of melt holding time resulted in the change of solidification structure.

Cite this article

YU Chang-Shuai , ZOU Min-Meng , ZHANG Jun , FU Heng-Zhi , LIU Lin . THE RELAXATION PHENOMENON DURING MELT SUPERHEATING TREATMENT OF DZ125 ALLOY[J]. Acta Metall Sin, 2010 , 46(6) : 674 -680 . DOI: 10.3724/SP.J.1037.2009.00846

References

[1] Li L, Overfelt R A. J Mater Sci, 2002; 37: 3521
[2] Gui Z L. Aviat Product Eng, 1995; 4: 12
(桂忠楼. 航空制造工程, 1995, 4: 12)
[3] Liu L, Huang T W, Zhang J, Fu H Z. Mater Lett, 2007; 61: 227
[4] Kolotukhin E V, Kuleshova E A, Baryshev E E, Tyagnov G V. Met Sci Heat Treat, 1995; 37: 222
[5] Zou M M, Zhang J, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 59
(邹敏明, 张军, 刘林, 傅恒志. 金属学报, 2008, 44: 59)
[6] Saucedo E, Rudolph P, Dieguez E. J Cryst Growth, 2008; 310: 2067
[7] Gu Z H, Wang H Y, Zheng N, Zha M, Jiang L L, Wang W, Jiang Q C. J Mater Sci, 2008; 43: 980
[8] Cao P, Qian M, Stjohn D H. Scr Mater, 2007; 56: 633
[9] Popel P S, Calvo–Dahlborg M, Dahlborg U. J Non–Cryst Solids, 2007; 353: 3243
[10] Yin F S, Sun X F, Li J G, Gun H R, Hu Z Q. Scr Mater, 2003; 48: 425
[11] Zhang J, Li B, Zou M M, Wang C S, Liu L, Fu H Z. J Alloys Compd, 2009; 484: 753
[12] Cai Y W, Fan X H, Li J G, Fu H Z. J Northwestern Polytech Univ, 1996; 14: 323
(蔡英文, 范新会, 李建国, 傅恒志. 西北工业大学学报, 1996; 14: 323)
[13] Mao X M, Fu H Z, Zhou Y H. J Northwestern Polytech Univ, 1985; 3: 11
(毛协民, 傅恒志, 周尧和. 西北工业大学学报, 1985; 3: 11)
[14] Volkert C A, Spaepen F. Mater Sci Eng, 1988; 97: 449
[15] Maslov V V, Lad’yanov V I, Ilinsky A G, Nosenko V K. J Phys Conf Ser, 2008; 98: 072007
[16] Adam G, Gibbs J H. J Chem Phys, 1965; 43: 139
[17] Fredriksson H, Fredriksson E. Mater Sci Eng, 2005; A413–414: 455
[18] Zou M M, Zhang J, Liu L, Fu H Z. Mater Sci Technol, 2008; 16: 86
(邹敏明, 张军, 刘林, 傅恒志. 材料科学与工艺, 2008; 16: 86)
[19] Chen G, Yu J W, Xie F Q, Fu H Z. Acta Metall Sin, 2001; 37: 488
(陈光, 俞建伟, 谢发勤, 傅恒志. 金属学报, 2001; 37: 488)
[20] Zhang J, Yang M, Wang C S, Liu L, Fu H Z. Foundry Technol, 2009; 9: 1108
(张军, 杨敏, 王常帅, 刘林, 傅恒志. 铸造技术, 2009; 9: 1108)
[21] Gunduz M, C¸ ad?rl? E. Mater Sci Eng, 2002; A327: 167
[22] Flemings M C. Metall Trans, 1974; 5: 2121
[23] Geng X G, Chen G, Fu H Z. Acta Metall Sin, 2002; 38:225
(耿兴国, 陈光, 傅恒志. 金属学报, 2002; 38: 225)
[24] Li R S. Non–Equilibrium Thermodynamics and Dissipation Structure. Beijing: Tsinghua Universsity Press, 1986:55
(李如生. 非平衡态热力学和耗散结构. 北京: 清华大学出版社, 1986: 55)
[25] Yin F S, Sun X F, Guan H R, Hu Z Q. J Alloys Compd, 2004, 364: 225

Outlines

/