论文

COMPARISON ON PITTING CORROSION RESISTANCE OF NICKEL AND CHROMIUM IN TYPICAL SEA WATER RESISTANCE STEELS

  • CAO Guo-Liang
Expand
  • Department of Chemistry and Materials; College of Sciences; Naval University of Engineering; Wuhan 430033

Received date: 2009-12-07

  Revised date: 2010-03-29

  Online published: 2010-06-11

Abstract

Ni–Cu–P and Cr–Cu–P steels are well known as sea water resistance steels, but the effects of alloying elements in steels on corrosion resistance are still not clear. Generally, Cr and Ni are important alloying elements for corrosion resistance but their roles in resisting pitting corrosion still need investigating. In order to understand the effects of Cr and Ni on rust layers and resistance against pitting corrosion, Ni–Cu–P and Cr–Cu–P steels were smelted in vacuum induction melting furnace and examined in the laboratory. Pitting susceptibility of two sea water resistance steels was compared by means of potentiodynamic polarization tests in 3% (mass fraction) NaCl solution. In order to evaluate the pitting propagation of steels, the simulating occluded corrosion cell tests and indoor interval hanging plate tests were performed in artificial sea water and 3% sea salt solution, respectively. The composition of inclusions, corrosive feature and characteristic of rust layer were studied by OM, electron probe micro–analyzer (EPMA), SEM and XRD. The results indicate that Ni–Cu–P steels exhibit stronger pitting susceptibility than Cr–Cu–P steels, and pitting susceptibility of two kinds of steels is not influenced by deoxidizing degrees. The results also suggest that pitting propagation rate of Cr–Cu–P steels is obviously greater than that of Ni–Cu–P steels. In acidified pits, alloying element Ni helps to enhance thermodynamic stability of matrix and improve potential of matrix. However, addition of alloying element Cr tends to lower the potential of matrix in pits. The results of rust layer analysis indicate that the compositions of inner rust layer are Fe3O4, α–FeOOH and a small amount of amorphous oxides. However, the rust layer of Cr–Cu–P steels is much more compact than that of Ni–Cu–P steels. It can be observed by SEM and EPMA that Cr in Cr–Cu–P steels is enriched in inner rust layer close to the matrix, while Ni is not found enrichment in inner rust layer of Ni–Cu–P steels.

Cite this article

CAO Guo-Liang . COMPARISON ON PITTING CORROSION RESISTANCE OF NICKEL AND CHROMIUM IN TYPICAL SEA WATER RESISTANCE STEELS[J]. Acta Metall Sin, 2010 , 46(6) : 748 -754 . DOI: 10.3724/SP.J.1037.2009.00816

References

[1] Matsushima I. Translated by Jin Y K. Low Alloy Corrosion Resistant Steels—A History of Development Application and Research. Beijing: Metallurgical Industry Press, 2004: 100
(松岛岩 著, 靳裕康 译. 低合金钢耐蚀钢---开发、发展及研究. 北京: 冶金工业出版社, 2004: 100)
[2] Melchers R E. Corros Sci, 2004; 46: 1669
[3] Huang J Z, Zuo Y. Resistance to Corrosion and Corrosive Data of Materials. Beijing: Chemical Industry Press, 2003: 97
(黄建中, 左禹. 材料的耐蚀性和腐蚀数据. 北京: 化学工业出版社, 2003: 97)
[4] Southwell C R, Alexander A L. Mater Prot, 1970; 14: 9
[5] Huang G Q. Corros Sci Prot Technol, 2000; 12: 86
(黄桂桥. 腐蚀科学与防护技术, 2000; 12: 86)
[6] Liu D Y, Wei K J, Li W J, Huang Q. J Chin Soc Corros Prot, 2003; 23: 7
(刘大扬, 魏开金, 李文军, 黄桂桥. 中国腐蚀与防护学报, 2003; 23: 7)
[7] Townsend H E. Corrosion, 2001; 57: 497
[8] Suzuki S Y, Takahashi Y, Kamimura T, Miyuki H, Shinoda K, Tohji K, Waseda Y. Corros Sci, 2004; 46: 1751
[9] Yang W, Gu J X, Li Q S, Xiao J X. Localized Corrosion of etals. Beijin: Chemical Industry Press, 1995: 59
(杨武, 顾睿祥, 黎樵shen, 肖京先. 金属的局部腐蚀. 北京: 化学工业出版社, 1995: 59)
[10] Wang J M, Chen X Q, Chang W S, Zhu X. J Harbin Inst Technol, 2006; 38: 1143
(王建民, 陈学群, 常万顺, 朱锡. 哈尔滨工业大学学报, 2006; 38: 1943)
[11] Zhang C Y, Chen X Q, Chen D B, Pan R Y. J Chin Soc Corros Prot, 2001; 21: 265
(张春亚, 陈学群, 陈德斌, 潘瑞扬. 中国腐蚀与防护学报, 2001; 21: 265)
[12] Yang X Z, Yang W. Corrosive Electrochemical Thermodynamic Potential—pH Diagram and Application of Metals. Beijing: Chemical Industry Press, 1991: 138
(杨熙珍, 杨武. 金属腐蚀电化学热力学电位---pH图及其应用. 北京: 化学工业出版社, 1991: 138)
[13] Zhu W C, Leng W H, Zhang J Q, Cao C N. Acta Metall Sin (Engl Lett), 2006; 19: 91
[14] Szklarska–Smialowska Z. Corros Sci, 2002; 44: 1143
[15] Jae–bong Lee. Mater Chem Phys, 2006; 99: 224
[16] Wang J M, Chen X Q, Li G M. J Univ Sci Technol Beijing, 2004; 11: 555
[17] Dillmann P, Balasubramaniam R, Beranger G. Corros Sci, 2002; 44: 2231
[18] Choi Y S, Shim J J, Kim J G. Mater Sci Eng, 2004; A385: 148
[19] Chen X H, Dong J H, Han E H, Ke W. Mater Lett, 2007; 61: 4050