FRICTION AND WEAR PROPERTIES OF Ni–FREE Zr–BASED BULK METALLIC GLASSES IN SIMULATED BODY FLUID

  • HUANG Cai-Yun ,
  • CHEN Qi ,
  • LIU Lin
Expand
  • The State Key Laboratory of Material Processing and Die & Mould Technology; Deportment of Materials Science and Engineering; Huazhong University of Science and Technology; Wuhan 430074

Received date: 2009-11-16

  Revised date: 2010-03-17

  Online published: 2010-06-11

Supported by

Supported by Specialized Research Fund for the Doctoral Program of Higher Education (No.200804870033), Huazhong University of Science and Technology Innovation Research Fund (No.C2009Z018J) and The Tribology Science Fund of State Key Laboratory of Tribology

Abstract

In the last decade, bulk metallic glasses (BMGs) emerge as a new class of metallic materials with disordered atomic structure. Especially, Zr–based BMGs have attracted an increasing attention due to their distinct properties including ultrahigh strength, high elastic strain limit, relatively low Young’s modulus (50—100 GPa) and easy forming ability in viscous state. In addition, Zr–based BMGs displayed a superior corrosion resistance in artificial body fluids and a satisfactory biocompatibility. The combination of these unique properties makes them extremely promising for biomedical applications. The most promising applications for the BMGs are in dentistry and orthopaedics due to their mechanical superiority, where friction and wear properties are clinically important for the performance of the implants in the body. In the present study, a Ni–free BMG plate of Zr60Cu19Fe5Al10Ti6 with dimensions of 70 mm×12 mm×1.5 mm was successfully prepared by water–cooled copper mold casting. The friction and wear characteristics of the BMG under sliding in dry air, distilled water and phosphate buffered saline (PBS) have been investigated on a SRV friction and wear tester in a ball–on–plate contact configuration where the upper ball in motion was made of zirconia with 10 mm diameter and the lower stationary plate was made of the BMG. Ti6Al4V alloy was also tested under the same condition for comparison. The wear depth was investigated by a surface profiler and the wear volume was also calculated. The surface morphologes and the component of wear debris were examined by SEM and EDS Compared witte Ti alloy, the BMG exhibits much less volume loss in the PBS solution, demonstrating that the BMG has a better wear rsistance than the Ti alloy, though he former has a larger friction cefficient. The wear mechanism of thBMG is dominated by the corrosion wear with oxidation of the surface and fatigue flake mechanism.

Cite this article

HUANG Cai-Yun , CHEN Qi , LIU Lin . FRICTION AND WEAR PROPERTIES OF Ni–FREE Zr–BASED BULK METALLIC GLASSES IN SIMULATED BODY FLUID[J]. Acta Metall Sin, 2010 , 46(6) : 681 -686 . DOI: 10.3724/SP.J.1037.2009.00762

References

[1] Yang S H. Joint Replacement Surgery. Beijing: Tsinghua University Press, 2005: 1 (杨述华. 关节置换外科学. 北京: 清华大学出版社, 2005: 19) [2] Wang A, Sun D C, Yau S S, Edwards B, Sokol M, Essner A, Polineni V K, Stark C, Dumbleton J H. Wear, 1997; 230: 203 [3] Ge S R, Wang Q L, Zhang D K, Zhu H, Xiong D S, Huang C H, Huang X L. Wear, 2003; 255: 1069 [4] Chen W R, Wang Y M, Qiang J B, Xu W P, Wang D H, Dong C, Xu T, Zhang A M. Tribology, 2003; 23: 14 (陈伟荣, 王英敏, 羌建兵, 徐卫平, 王德和, 董闯, 徐洮, 张爱民. 摩擦学学报, 2003; 23: 14) [5] Xiao H X, Chen G, La P Q. Tribology, 2006; 26: 140 (肖华星, 陈光, 喇培清. 摩擦学学报, 2006; 26: 140) [6] Parlar Z, Bakkal M, Shih A J. Intermetallics, 2008; 16: 34 [7] Li G, Wang Y Q, Gao Y P. J Mater Res, 2002; 17: 1877 [8] Jin H W, Ayer R, Koo J Y. J Mater Res, 2007; 22: 264 [9] Blau P J. Wear, 2001; 250: 431 [10] Qiu C L, Chen Q, Liu L, Chan K C, Zhou J X, Chen P P, Zhang S M. Scr Mater, 2006; 55: 605 [11] Mischler S, Spiegel A, Landolt D. Wear, 1999; 225–229: 1078 [12] Wen S Z. Principles of Tribology. Beijing: Tsinghua University Press, 1990: 385 (温诗铸. 摩擦学原理. 北京: 清华大学出版社, 1990: 385) [13] Rabinowitcz E, Dunn L A, Russel P G. Wear, 1961; 4: 345 [14] Fu X, Kasai T, Falk M L, Rigney D A. Wear, 2001; 250: 409 [15] Tam C Y, Shek C H. Mater Sci Eng, 2004; A384: 138 [16] Ma M Z, Liu R P, Xiao Y, Lou D C, Liu L, Wang Q, Wang W K. Mater Sci Eng, 2004; A386: 326 [17] Ishida M, Takeda H, Nishiyama N, Kita K, Shimizu Y, Saotome Y, Inoue A. Mater Sci Eng, 2007; A449–451: 149 [18] Miyoshi K, Buckley D H. Wear, 1986, 110: 295 [19] Kishore U S, Sudarsan U, Chandran N, Chattopadhyay K. Acta Metall, 1987; 35: 1463
Outlines

/

〈 〉