论文

ULTRASONIC BONDABILITY AND ANTIOXIDATION PROPERTY OF TiN/Ag METALLIZATION ON Cu PAD

  • TIAN Yan-Hong
Expand
  • 1) 哈尔滨工业大学现代焊接生产技术国家重点实验室; 哈尔滨 150001 2) 四川西南电子设备研究所;  成都 610036

Received date: 2009-12-02

  Revised date: 2010-03-15

  Online published: 2010-05-11

Supported by

Supported by National Natural Science Foundation of China (No.50705021)

Abstract

Copper interconnect has become the only one option for the semiconductor manufacturing under 110 nm. However, there are some problems to be solved in the copper interconnect, especially the bad bondability due to the oxidation of the copper. In this paper, TiN/Ag metallization was fabricated as the protective layer of copper pad by magnetron sputtering. The amorphous TiN film as the barrier layer to prevent copper atoms diffusing from the copper pad to the surface, and the crystalline Ag film as the bonding layer to enhance the bond abilities. The TiN/Ag metallization was characterized by AFM, XPS, XRD and SEM, respectively, and then the ultrasonic bondability of Au wire and antioxidation property of the metallization were measured. The shear test of the Au ball bond was performed by micro-force tester. Ultrasonic bondability test shows that TiN/Ag metallization as the copper chip protective layer has good bonding performance. The bondability and shear strength of the Au ball bond on the metallization increased with the temperature increase from the room temperature to 180 ℃. The TiN/Ag metallization has 100% bondability at 180 ℃, and the shear failure occurred at the interface of Ag film and Au ball bond. High temperate storage test shows that TiN/Ag metallization has better antioxidation property than the Ag film, since the amorphous TiN layer plays an excellent role of diffusion barrier.

Cite this article

TIAN Yan-Hong . ULTRASONIC BONDABILITY AND ANTIOXIDATION PROPERTY OF TiN/Ag METALLIZATION ON Cu PAD[J]. Acta Metall Sin, 2010 , 46(5) : 618 -622 . DOI: 10.3724/SP.J.1037.2009.00807

References

[1] Nieolet M A. Appl Surf Sci, 1995; 91: 269
[2] Haneda P, Aramaki K. J Electrochem Soc, 1998; 145: 1856
[3] Aoh J N, Chuang C L. J Electron Mater, 2004; 33: 300
[4] Kajiwara R, Takahashi T, Tsubosaki K. Quart J Jpn Weld Soc, 1998; 16: 93
[5] Chuang C L, Aoh J N, Din R F. Microelectron Reliab, 2006; 46: 449
[6] Takeyama M, Noya A, Taguchi M. Jpn J Appl Phys, 1996; 35: 704
[7] Hu Y Z, Sharangpani R, Tay S P. J Vac Sci Technol, 2000; 18A: 2527
[8] Tran T A, Yong L, Williams B. In: Reston V A ed., 2000 HD International Conference on High–Density Interconnect and Systems Packaging. Colorado, USA: IMAPS, SPIE, 2000: 273
[9] Chuang C L. Microelectron Eng, 2007; 84: 551
[10] Manepalli R, Stepniak F, Allen S. IEEE Trans Adv Packag, 1999; 22(1): 4
[11] Hymes S, Murarka S P, Shepard C. J Appl Phys, 1992; 71: 4623
[12] Harman G G, Johnson C E. IEEE Trans Adv Packag, 2002; 25: 667
[13] Ho H M, Lam W, Stoukatch S. Microelectron Reliab, 2003; 43: 913
[14] Tran T A, Young L, Chenl S. In: Schaefer J, ed., IEEE Electronic Components and Technology Conf, Trenton, New Jersey: IEEE, 2000: 1674
[15] Rohan J F, O’riordan G, Boardman J. Appl Surf Sci, 2002; 185: 289

Outlines

/

〈 〉