论文

MODELLING AND SIMULATION OF THE MICROSTRUC- TURE FORMATION IN A STRIP CAST Al–Pb ALLOY

  • LI Hai-Li ,
  • DIAO Jiu-Zhou
Expand
  • 1.Weaponry Science Technology Research Center; Shenyang Ligong University; Shenyang 110159
    2.Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016

Received date: 2009-11-24

  Revised date: 2010-03-12

  Online published: 2010-06-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50771097 and u0837601)

Abstract

When a single–phase liquid is cooled into the miscibility gap, it decomposes into two liquid phases. Generally the liquid–liquid phase transformation causes the formation of a solidification microstructure with serious phase segregation. Many efforts have been made to use the liquid–liquid demixing phenomenon for the production of the finely dispersed metal–metal composite materials. It is demonstrated that the only effective method of preventing the formation of the microstructure with heavy phase segregation in monotectic alloys is using the rapid solidification processing techniques. Strip casting may have great potentials in the manufacturing of the bulk materials of this kind of alloys. In this paper, a model was developed to describe the microstructure formation in a strip cast monotectic alloy based on the population dynamic method. The model takes into account the concurrent actions of the nucleation, diffusional growth and motions of the minority phase droplets. The model was nmerically solved together with the controlling equations for the heat transfer, mass transport and momentum transfer to studthe microstructure development in the strip cast Al–Pb alloys. The effects of alloy composition, solidification velocity and melting temperature on the microstructure formation were investigated. The results indicate that with the increase of the solidification velocity, the nucleation position of the minority phase droplets moves towards the solidification interface, the nucleation rate and number density of droplets increase and the average droplet size decreases. All these are favorable for the formation of a well dispersed microstructure. With the increase of the Pb content,  the nucleation position of the minority phase droplets moves away form the solidification interface, the nucleation rate decreases, and the average droplet size increases. These are against the formation of a well dispersed microstructure. With the increase of the melting temperature, the nucleation rate and number density of droplets increase and the average droplet size decreases. These are favorable for the formation of a well dispersed microstructure. But the velocity of the minority phase droplets decreases with the increase of the melting temperature. When the velocity of droplets is negative, samples can not obtain steady state solidification and result in the formation of a microstructure with massive segregation.

Cite this article

LI Hai-Li , DIAO Jiu-Zhou . MODELLING AND SIMULATION OF THE MICROSTRUC- TURE FORMATION IN A STRIP CAST Al–Pb ALLOY[J]. Acta Metall Sin, 2010 , 46(6) : 695 -700 . DOI: 10.3724/SP.J.1037.2009.00782

References

[1] Pratt G C. Int Met Rev, 1973; 18: 62
[2] Zhao J Z, Kolbe M, Li H L, Gao J R, Ratke L. Metall Mater Trans, 2007; 38A: 1162
[3] Ozawa S, Motegi T. Mater Lett, 2004; 58: 2548
[4] Cao C D, Wei B B. J Mater Sci Technol, 2002; 18: 73
[5] Fujii H, Kitaguchi H, Kumakura H, Togano K. J Mater Sci, 1995; 30: 3429
[6] Cui H B, Guo J J, Su Y Q, Wu S P, Li X Z, Fu H Z. Acta Metall Sin, 2007; 43: 907
(崔红保, 郭景杰, 苏彦庆, 吴士平, 李新中, 傅恒志. 金属学报, 2007; 43: 907)
[7] Carlberg T, Fredriksson H. Metal Trans, 1980; 11A: 1665
[8] Huang Z. Scr Metall, 1991; 24: 149
[9] Kamio A, Kumai S, Tezuka H. Mater Sci Eng, 1991; A146: 105
[10] Prinz B, Romero A, Ratke L. J Mater Sci, 1995; 30: 4715
[11] He J, Zhao J Z, Li H L, Zhang X F, Zhang Q X. Metall Mater Trans, 2008; 39A: 1174
[12] Wecker J, Hehnolt R, Schulta L, Samwer K. Appl Phys Lett, 1993; 52: 1985
[13] Kolbe M, Brillo J, Egry I. Microgravity Sci Technol, 2006; 18: 174
[14] Li H L. PhD Thesis, Institute of Metal Research, Chinese Academy of ciences, Shenyang, 2009
(李海丽. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
[15] Granasy L, Ratke L. Scr Mater, 1993; 28: 1329
[16] Li H L, Zhao J Z, Zhang Q X, He J. Metall Mater Trans, 2008; 39A: 3308
[17] Rogers J R, Davis R H. Metall Trans, 1990; 2A: 59
[18] Thieringer W K. Acta Metall, 1985; 33: 1973
[19] Tao W Q. Numerical Heat Transfer. Xi’an: Xi’an Jiaotong University Press, 1988: 349
(陶文铨. 数值传热学. 西安: 西安交通大学出版社, 1988: 349)
[20] Patankar S V, Translated by Zhang Z. Numerical Heat Transfer and Fluid Flow. Beijing: Science Press, 1984: 27
(Patankar S V, 张 政译. 传热与流体流动计算. 北京: 科学出版社, 1984: 27)
[21] Li H L, Zhao J Z. Appl Phys Lett, 2008; 92: 241902

Outlines

/

〈 〉