论文

EFFECT OF AN ABRUPT GROWTH RATE ON PRIMARY Al2Cu PHASE IN DIRECTIONAL SOLIDIFICATION OF Al–40%Cu HYPEREUTECTIC ALLOY

  • QUAN Qiong-Juan ,
  • LI Shuang-Meng ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi’an 710072

Received date: 2009-10-26

  Revised date: 2010-03-18

  Online published: 2010-04-11

Supported by

Supported by National Natural Science Foundation of China (No.50971101), Program for New Century Execllent Talents in University (No.NCET–07–0692) and the Fund of the State Key Laboratory of Solidification Processing in NWPU (No.34–TP–2009)

Abstract

Intermetallics combining metal and ceramic properties exhibit colorfully complicated growth morphologies in solidification. Different from the solidus phase solidification, intermetallic solidification remains less understanding of the correlation between processing parameters and microstructure morphologies. In this paper, considering that the intermetallic compound Al2Cu phase has well–known thermophysical properties available for the theoretical and experimental research, we carried out the directional solidification experiments and focused on an Al–Al2Cu hypereutectic alloy, where the Al2Cu phase was solidified as a primary phase. The primary Al2Cu phase growth behavior in the experiments included phase competition growth between coupled eutectic and primary phase, faceted phase transition and its change in growth morphology. By using a high thermal gradient directional solidification apparatus, the directionally solidified microstructures of Al–40%Cu (mass fraction) hyereutectic alloy were investigated and discussed based on the competition growth model. As the growth rate was changed abruptly from 10 μm/s to 2 μm/s, the microstructure transition from a primary Al2Cu dendrite plus interdendritic eutectic to an entirely coupled eutectic occurred due to the interface growth temperature of the coupled eutectic exceeding that of the primary Al2Cu dendrite. Also, the alloy liquid composition ahead of the solid/liquid interface approaching the eutectic point caused this microstructure transition. Simultaneously, in the changing–growth rate experiments, the primary Al2Cu dendrites were firstly broken into small ones and then became the eutectic microstructure; it was interpreted rather by the decrease in liquid solute concentration ahead of the solid/liquid interface tan by te effect of the thermal–solutal convection. Moreover, the morphology change iphase growth from faceted primary Al2Cu phase to non–faceted phase was observed by reducing abruptly the growtrate from 10 μm/s to 2 μm/s, which can be explained by the Jackson fctor α decreasing with increasig the interface growth temperature of primary Al2Cu pase.

Cite this article

QUAN Qiong-Juan , LI Shuang-Meng , FU Heng-Zhi . EFFECT OF AN ABRUPT GROWTH RATE ON PRIMARY Al2Cu PHASE IN DIRECTIONAL SOLIDIFICATION OF Al–40%Cu HYPEREUTECTIC ALLOY[J]. Acta Metall Sin, 2010 , 46(4) : 500 -505 . DOI: 10.3724/SP.J.1037.2009.00706

References

[1] Moshksar M M, Mirzaee M. Intermetallics, 2004; 12: 1361
[2] Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T. Acta Mater, 2006; 54: 1077
[3] Li X Z, Fan J L, Guo J J, Su Y Q, Fu H Z. Acta Metall Sin, 2009; 45: 308
(李新中, 樊江磊, 郭景杰, 苏彦庆, 傅恒志. 金属学报, 2009; 45: 308)
[4] Zhong H, Li S M, Lu H Y, Zou G R, Liu L, Fu H Z. J Cryst Growth, 2008; 310: 3366
[5] Ozawa S, Satio T, Motegi T. J Alloys Compd, 2004; 363: 263
[6] Cheng C J, Zhu S G, Li J G, Li Y H. Mater Sci Eng, 2005; B122: 174
[7] Tiller W A. The Science of Crystallization: Microscopic Interface Phenomena, Cambridge: Cambridge University Press, 1991: 52
[8] Fu H Z, Guo J J, Liu L, Li J S. Directional Solidification and Processing of Advanced Materials, Beijing: Science Press, 2008: 17
(傅恒志, 郭景杰, 刘林, 李金山. 先进材料定向凝固, 北京: 科学出版社, 2008: 17)
[9] Walker H, Liu S, Lee J H, Trivedi R. Metall Mater Trans, 2007; 38A: 1417
[10] Gill S C, Kurz W. Acta Metall Mater, 1995; 43: 139
[11] Ourdjini A, Liu J C, Elliott R. Mater Sci Technol, 1994; 10: 312
[12] Yilmaz F, Elliott R. J Cryst Growth, 1984; 66: 465
[13] LEE J H, Liu S, Miyahara H, Trivedi R. Metall Mater Trans, 2004; 35B: 910
[14] LEE J H, Liu S, Trivedi R. Metall Mater Trans, 2005; 36A: 3111
[15] Ting L, Li S M, Fu H Z. Rare Met Mater Eng, 2007; 36: 617
(唐玲, 李双明, 傅恒志. 稀有金属材料与工程, 2007; 36: 617)
[16] Zhong H, Li S M, Lv H Y, Liu L, Zhou G R, Fu H Z. Sci China, 2007; 50G: 432
[17] Kurz W, Fisher D J. Fundamentals of Solidification, 4th ed. Zurich: Trans Tech Publications Ltd, 1998: 35
[18] Tiller W A. The Science of Crystallization: Macroscopic Phenomena and Defect Generation. Cambridge: Cambridge University Press, 1992: 144
[19] Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209
[20] Burden M H, Hunt J D. J Cryst Growth, 1974; 22: 109
[21] Magnin P, Trivedi R. Acta Mater, 1991; 4: 453
[22] Li S M, Ma B L, Li X L, Liu L, Fu H Z. Sci China, 2005; 48E: 270
[23] Jackson K A, Hunt J D. Trans Metall Soc AIME, 1966; 236: 1129
[24] Karma A, Srkissian A. Metall Mater Trans, 1996; 27A: 635
[25] Stefanescu D M. Science and Engineering of Casting Solidification, 2nd ed. Berlin: Springer, 2009: 176

Outlines

/