SALT SPRAY CORROSION BEHAVIOUR OF CrN COATINGS DEPOSITED BY ARC ION PLATING
Received date: 2009-11-13
Revised date: 2010-01-15
Online published: 2010-05-11
CrN coatings were deposited onto 38CrA substrate using arc ion plating (AIP) method. The microstructures of CrN coatings were investigated by XRD and SEM. The corrosion behaviour affected by deposition parameters was studied by salt spray corrosion test in a neutral mist of NaCl solution at (35±2) ℃ for 300 h. The results show that all of the CrN coatings contain primarily fcc-CrN along with hcp-Cr2N and bcc-Cr phases. CrN phase in coating deposited under lower N2 pressure exhibited {100} preferred orientation, while {110} preferred orientation under higher N2 pressure. Under the deposition condition of higher bias voltage and lower N2 pressure, the CrN coating achieves dense microstructure with less residual stress and porosity, which leads to better corrosion resistance in salt spray test. The corrosion product of salt spray test was investigated by SEM and EDS, and the corrosion mechanism was discussed.
Key words: CrN; arc ion plating; salt spray corrosion; potentiodynamic polarization
WAN Xian-Song , SHI Yu-Yang , MA Jun , LI Hai-Qiang , GONG Jun , XUN Tiao . SALT SPRAY CORROSION BEHAVIOUR OF CrN COATINGS DEPOSITED BY ARC ION PLATING[J]. Acta Metall Sin, 2010 , 46(5) : 600 -606 . DOI: 10.3724/SP.J.1037.2009.00759
[1] Navinsek B, Panjan P. Surf Coat Technol, 1995; 74: 155
[2] Holleck H. J Vac Sci Technol, 1986; 4A: 2661
[3] Liu C, Bi Q, Matthews A. Corros Sci, 2001; 43: 1953
[4] M¨unz W D. J Vac Sci Technol, 1998; 4A: 2717
[5] Navinsek B, Panjan P. Thin Solid Films, 1993; 223: 4
[6] Ren M, Yang Z G, Shaw L L. Nanostruct Mater, 1999; 11: 25
[7] Ehiasarian A P, Wen J G, Petrov I. J Appl Phys, 2007; 101: 054301
[8] Volz K, Kiuchi M, Ensinger W. Surf Coat Technol, 1998; 108: 303
[9] Kacsich T, Perry A J. J Phys, 1995; 28D: 424
[10] Kondo A, Oogami T, Sato K, Tannka Y. Surf Coat Technol, 2006; 177: 238
[11] Ljungcrantz H, Hultman L, Sundgren J E, Hakansson G, Karlsson L. Surf Coat Technol, 1994; 63: 123
[12] Wang Q M, Kim K H. J Vac Sci Technol, 2008; 26A: 1267
[13] Liu C, Bi Q, Ziegele H, Leyland A, Matthews A. J Vac Sci Technol, 2002; 20A: 772
[14] Janssen G C A M. Thin Solid Films, 2007; 515: 6654
[15] Zhao S S. PhD Thesis, Graduate University of Chinese Academy of Sciences, Beijing, 2009
(赵升升. 中国科学院研究生院博士学位论文, 北京, 2009)
[16] Wan X S, Zhao S S, Yang Y, Gong J, Sun C. Surf Coat Technol, doi: 10.1016/j.surfcoat.2009.11.021
[17] Davis C A. Thin Solid Films, 1993; 226: 30
[18] Zhang B H, Cong W B, Yang P. Electrochemical Corrosion and Protection of Metal. Beijing: Chemical Industry Press, 2005: 86
(张宝宏, 从文博, 杨萍. 金属电化学腐蚀与防护. 北京: 化学工业出版社, 2005: 86
[19] Cao C N. Principles of Electrochemical Corrosion. 2nd ed, Beijing: Chemical Industry Press, 2004: 99
(曹楚南. 腐蚀电化学原理. 第二版, 北京: 化学工业出版社, 2004: 99)
[20] Conde A, Navas C, Cristobal A B, Housden J, Damborenea J D. Surf Coat Technol, 2006; 201: 2690
[21] William V K G, Harish C B, Selvi V E, Kalavati, Rajam K S. Thin Solid Films, 2006; 514: 204
[22] Aromaa J, Ronkainen H, Mahiout A, Hannula S P, Leyland A, Matthews A, Matthes B, Broszeit E. Mater Sci Eng, 1991; A140: 722
[23] Tato W, Landolt D. J Electrochem Soc, 1998; 145: 4173
/
| 〈 |
|
〉 |