论文

EARLY INTERFACIAL REACTION AND UNDERCOOLING SOLIDIFICATION BEHAVIOR  OF Sn-3.5Ag/Cu SYSTEM

  • ZHOU Min-Bei ,
  • LI Xun-Beng ,
  • MA Xiao ,
  • ZHANG Xin-Beng
Expand
  • School of Materials Science and Engineering; South China University of Technology; Guangzhou 510640

Received date: 2009-08-31

  Revised date: 2010-01-27

  Online published: 2010-05-11

Supported by

Supported by Program of New Century Excellent Talents in University (No.NCET-04-0824) and Science and Technology Major Project of Guangdong Province (No.2009A080204005)

Abstract

For electronic packaging technologies using lead-free solders, one of the major problems related to reliability for the solder interconnects is the existence of the interfacial intermetallic compound (IMC). The interfacial failures between IMC and solder alloy often lead to loss of function in interconnects and result in product failure. Therefore, considerable attention has been focused on study of formation, growth and control of IMC during solder process. In this paper, the early interfacial reaction in Sn-3.5Ag/Cu (UBM) system and the system's melting and solidification characteristics were investigated using differential scanning calorimeter incorporating with reflow process. The results show that during heating the diffusion of Cu atom into Sn-3.5Ag solder results in the formation of Sn-Ag-Cu ternary alloy at the interface before melting of Sn-3.5Ag solder and the ternary eutectic system melts at a temperature nearly 4 ℃ lower than Sn-3.5Ag solder's melting temperature. The early interfacial reaction also leads to earlier wetting of the liquid solder alloy at the interface, and consequently brings about formation of scallop-type Cu-Sn intermetallics layer with a certain thickness as well as makes the initial Sn-3.5Ag/Cu system changed into Sn-Ag-Cu/Cu system, which makes the undercooling of the solder alloy decrease obviously.

Cite this article

ZHOU Min-Bei , LI Xun-Beng , MA Xiao , ZHANG Xin-Beng . EARLY INTERFACIAL REACTION AND UNDERCOOLING SOLIDIFICATION BEHAVIOR  OF Sn-3.5Ag/Cu SYSTEM[J]. Acta Metall Sin, 2010 , 46(5) : 569 -574 . DOI: 10.3724/SP.J.1037.2009.00566

References

[1] Laurila T, Vuorinen V, Kivilahti J K. Mater Sci Eng, 2005; R49: 1
[2] Tu K N. Mater Chem Phys, 1996; 46: 217
[3] Kajihara M. Acta Mater, 2004; 52: 1193
[4] Sakama T, Kajihara M. J Alloy Compd, 2009; 475: 608
[5] Zeng K, Tu K N. Mater Sci Eng, 2002; R38: 55
[6] Gong J C, Liu C Q, Conway P P, Silberschmidt V V. Acta Mater, 2008; 56: 4291
[7] Gong J C, Liu C Q, Conway P P, Silberschmidt V V. Scr Mater, 2009; 60: 333
[8] Deng X, Piotrowski G, Williams J J, Chawla N. J Electron Mater, 2003; 32: 1403
[9] Yao P, Liu P, Liu J. Microelectron Eng, 2009; 86: 1969
[10] Lehman L P, Kinyanjui R K, Zavalij L, Zribi A, Cotts E J. In: Howell W, Noctor D, eds., Proceedings of 53rd Electronic Components and Technology Conference, New Orleans, LA: IEEE, 2003: 1215
[11] Kang S K, Choi W K, Shih D Y, Henderson D W, Gosselin T, Sarkhel A, Goldsmith C, Puttlitz K J. In: Howell W, Noctor D, eds., Proceedings of 53rd Electronic Components and Technology Conference, New Orleans, LA: IEEE, 2003: 64
[12] Kang S K, Shih D Y, Leonard D, Henderson D W, Gosselin T, Cho S I, Yu J, Choi W K. J Miner Met Mater Soc, 2004; 56: 34
[13] Kim K S, Huh S H, Suganuma K. Microelectron Relia, 2003; 43: 259
[14] KimD H, Cho M G, Seo S K, Lee HM. J Electron Mater, 2009; 38: 39
[15] Cho M G, Kim H Y, Seo S K, Lee H M. Appl Phys Lett, 2009; 95: 021905
[16] Kang S K, Cho M G, Lauro P, Shih D Y. J Mater Res, 2007; 22: 557
[17] Cho M G, Kang S K, Lee H M. J Mater Res, 2008; 23: 1147
[18] Cho M G, Kang S K, Seo S K, Shih D Y, Lee H M. J Mater Res, 2009; 24: 534
[19] Loomans M E, Fine M E. Metall Mater Trans, 2000; 31A: 1155
[20] Baker H, Okamoto H. ASM Handbook. Vol.3. Alloy Phase Diagrams: Section 2. Materials Park, Ohio: ASM International, 1992: 28
[21] Moon K W, Boettinger W J, Kattner U R, Biancaniello F S, Handwerker C A. J Electron Mater, 2000; 29: 1122
[22] Alam M O, Chan Y C, Tu K N. J Appl Phys, 2003; 94: 7904
[23] Callister W D. Materials Science and Engineering–An Introduction. 7th Ed, New York: John Wiley & Sons, 2007: 313
[24] Wang H Q, Gao F, Ma X, Qian Y Y. Scr Mater, 2006; 55: 823

Outlines

/

〈 〉