THREE DIMENSIONAL FEMSIMULATION OF TITANIUM HOLLOW MONOLITHIC STRUCTURE PROCESS BASED ON VISCO–PLASTIC CONSTITUTIVE
Received date: 2010-01-19
Revised date: 2010-02-10
Online published: 2010-04-11
A three dimensional finite element model (FEM) was established to simulate the forming process of titanium alloy hollow monolithic structure. The influence of process parameters on this process was analyzed by finite element method code MSC.Marc in which a rigid–viscoplatic constitutive equation was implemented. The results demonstrated that with the increase of twisting velocity, the torque on the hollow structure changes indistinctively. In case of increasing die velocity and target strain rate, the forming force of hot forming and gas pressure of superplastic forming will increase. On the contrary, along with the increasing of temperature, the forming force decreased. In case of temperature above 900 ℃, the influence of temperature on the forming force and gas pressure was weaken. Based n FEM, at the conditions oprocess paramtrs, like torsions speed of 4.376×10−3 rad/s, hot forming die velocity of 2.12×10−1 mm/starget strain rate o1.0×10−3 s−1, as well as at the temperature of 925 ℃, a simulacrum f hollow mnolithic structure ftitanium alloy was prepared, the thickness distribution of the ace sheet of the obtained part was in good agreement with the simulated results.
DIAO Bing , BO Bing-Zhe . THREE DIMENSIONAL FEMSIMULATION OF TITANIUM HOLLOW MONOLITHIC STRUCTURE PROCESS BASED ON VISCO–PLASTIC CONSTITUTIVE[J]. Acta Metall Sin, 2010 , 46(4) : 396 -403 . DOI: 10.3724/SP.J.1037.2010.00035
[1] Blenkinsop P A. J de Phys IV, 1993; 3(7): 161
[2] Liang C H. Aeroengine, 2006; 32(3): 48
(梁春华. 航空发动机, 2006; 32(3): 48)
[3] Fitzpatrick G A, Loyd A D. Intelligent Processing of High Performance Materials, Neuilly–Sur–Seine: Research and Technology Organization, 1999: 41
[4] Wood R D, Bonet J. J Mater Process Technol, 1996; 60: 45
[5] Rusz S, Lapkowski W, Sinczak J, Boruta J. J Mater Process Technol, 1996; 60: 697
[6] Bonet J, Antonio G, Richard D W. Comput Methods Appl Mech Eng, 2006; 195: 6580
[7] Zhang K F, Zhao Q Y, Wang C W, Wang Z R. J Mater Process Technol, 1995; 55: 24
[8] Kim Y H, Hong S S, Lee J S, Wagoner R H. J Mater Process Technol, 1996; 62: 90
[9] Lee K S, Huh H, Choy Y J. J Mater Process Technol, 1997; 63: 684
[10] Chen Y, Kibble K, Hall R, Huang X. Mater Des, 2001; 22: 679
[11] Li C C, Cheng J H. Mater Sci Eng, 2002; A333: 146
[12] Tao J, Keaveyb M A. J Mater Process Technol, 2004; 147: 111
[13] Lee K S, Huh H. J Mater Process Technol, 2001; 113: 754
[14] Bonet J, Bhargava P, Wood R D. Int J Numer Methods Eng, 1997; 40: 3205
[15] Bonet J, Bhargava P. Comput Methods Appl Mech Eng, 1995; 122: 51
[16] Li G Y, Tan M J, Liew K M. J Mater Process Technol, 2004; 150: 76
[17] Hambli R, Potiron A. Comput Methods Appl Mech Eng, 2001; 190: 4871
[18] Li G Y, Tan M J, Liew K M. J Mater Process Technol, 2004; 150: 76
[19] Wu W, Zhang K F, Song Q F. Acta Aeronaut Astronaut Sin, 2000; 21: 364
(吴 为, 张凯锋, 宋全峰. 航空学报, 2000; 21: 364)
[20] Zhang K F, Han W B, Wu W, Wang G F, Wu D Z. J Mater Sci Technol, 2003; 19: 46
[21] Xing H L, Zhang K F, Wang Z R. J Mater Process Technol, 2004; 151: 284
[22] Hwang Y M, Lay H S. J Mater Process Technol, 2003; 140: 426
[23] Adam L, Ponthot J P. J Mater Process Technol, 2003; 139: 295
[24] Lee K S, Huh H. J Mater Process Technol, 1999; 89–90: 92
[25] Seshacharyulu T, Medeiros S C, Frazier W G. Mater Sci Eng, 2000; A284: 184
[26] Bonet J, Wargadipura A H S, Wood R D. Commun Appl Num Meth, 1998; 5: 121
[27] Cheng J H. Int J Mech Sci, 1994; 36: 981
[28] Huh H, Han S S. In: Chenot J L ed., Proceedings of the Numerical Methods of Industrial Forming Processes. France: Valbonne, 1992: 861
[29] Akkus N, Kawahara K M, Nishimura H. J Mater Process Technol, 1997; 68: 21
/
| 〈 |
|
〉 |