论文

A TRAINING-FREE CAST Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY BASED ON FORMATION OF MARTENSITE IN A DOMAIN MANNER I. Idea and realization

  • PENG Hua-Bei ,
  • LIU Gang ,
  • WEN Yu-Hua ,
  • XUN Pan-Pan ,
  • LI Ning
Expand
  • College of Manufacturing Science and Engineering; Sichuan University; Chengdu 610065

Received date: 2009-09-24

  Revised date: 2009-12-18

  Online published: 2010-03-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50501015 and 50871072) and Program for New Century Excellent Talents in University (No.NCET-06-0793)

Abstract

Low cost Fe-Mn-Si based shape memory alloys (SMAs) has not got widely applications because of their poor shape memory effect (SME) and the need of thermo-mechanical training, so developing training-free Fe-Mn-Si based SMAs with high memory property is significant. In the present study, it was put forth that the formation of stress-induced ε martensite in a domain manner could improve the SME of Fe-Mn-Si based SMAs and it could be realized through subdividing austenite γ grains into smaller domains using the residual lathy δ ferrite phase. According to Hammar's equivalents, a cast Fe-18Mn-5.5Si-9.5Cr-4Ni alloy with Cr/Ni equivalent ratio of 1.85 was prepared. OM and VSM (vibrating sample magnetometer) examination showed that the as-cast microstructure consists of γ austenite and lathy δ ferrite phase, and the lathy δ ferrite subdivided the austenite grains into smaller domains, which makes the stress-induced ε martensite bands form in a domain manner. Because the collisions between domain-like martensite bands were reduced, a high recovery strain of 4.9% was attained in the as-cast Fe-18Mn-5.5Si-9.5Cr-4Ni alloy. This result provides a novel way of developing training-free Fe-Mn-Si based SMAs. It can be expected that the SME of cast Fe-Mn-Si based SMAs will be further improved through modifying and optimizing alloy compositions, solidification parameters and heat treatment process.

Cite this article

PENG Hua-Bei , LIU Gang , WEN Yu-Hua , XUN Pan-Pan , LI Ning . A TRAINING-FREE CAST Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY BASED ON FORMATION OF MARTENSITE IN A DOMAIN MANNER I. Idea and realization[J]. Acta Metall Sin, 2010 , 46(3) : 282 -287 . DOI: 10.3724/SP.J.1037.2009.00643

References

[1] Sato A, Chishima E, Soma K, Mori T. Acta Metall Mater, 1982; 30: 1177
[2] Sato A, Chishima E, Soma K, Mori T. Acta Metall Mater, 1984; 32: 539
[3] Sato A, Yamaji Y, Mori T. Acta Metall Mater, 1986; 34: 287
[4] Otsuka H, Yamada H, Maruyama T, Tanahashi H, Matsuda S, Murakami M. ISIJ Int, 1990; 30: 674
[5] Yang J H, Chen H, Wayman C M. Metall Mater Trans, 1992; 23A: 1431
[6] Inagaki H. Z Metall, 1992; 83: 90
[7] Wang X X, Zhao L C. Scr Mater Metall, 1992; 26: 1451
[8] Wang D F, Chen Y R, Gong F Y, Liu D Z, Liu W X. J Phys France IV, 1995; 5: 527
[9] Kajiwara S. Mater Sci Eng, 1999; A273–275: 67
[10] Matsumura O, Furusako S, Sumi T, Furukawa T, Otsuka H. Mater Sci Eng, 1999; A272: 459
[11] Sato A, Masuya T, Morishita M, Kumai S, Inoue A. Mater Sci Forum, 2000; 327–328: 223
[12] Wang D F, Liu D Z, Dong Z Z, Liu W X, Chen J M. Mater Sci Eng, 2001; A315: 174
[13] Wen Y H, Yan M, Li N. Scr Mater, 2004; 50: 835
[14] Wen Y H, Yan M, Li N. Scr Mater, 2004; 50: 441
[15] Baruj A, Kikuchi T, Kajiwara S, Shinya N. Mater Sci Eng, 2004; A378: 333
[16] Farjami S, Hiraga K, Kubo H. Acta Mater, 2005; 53: 419
[17] Wen Y H, Zhang W, Li N. Acta Metall Sin, 2006; 42: 1217
(文玉华, 张伟, 李宁. 金属学报, 2006; 42: 1217)
[18] Wen Y H, Zhang W, Li N, Peng H B, Xiong L R. Acta Mater, 2007; 55: 6526
[19] Wen Y H, Xiong L R, Li N, Zhang W. Mater Sci Eng, 2008; A474: 60
[20] Yang J H, Wayman C M. Acta Metall Mater, 1992; 40: 2011
[21] Inagaki H. Z Metall, 1992; 83: 97
[22] Inagaki H. Z Metall, 1992; 83: 304
[23] Suutala N, Takalo T, Moisio T. Metall Mater Trans, 1979; 10A: 512
[24] Leone G L, Kerr H W. Weld J, 1982; 61: 13
[25] Suutala N. Metall Mater Trans, 1982; 13A: 2121
[26] Stanford N, Dunne D P. J Mater Sci, 2006; 41: 4883
[27] Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1998; A242: 77
[28] Gu Q, Humbeeck J V, Delaey L. J Phys France IV, 1994; 4: 135
[29] Folkhard E. Welding Metallurgy of Stainless Steel. Wien: Springer–Verlag, 1988: 39

Outlines

/

〈 〉