PRECISE DETERMINATION OF THE IRRATIONAL PREFERRED INTERFACE ORIENTATION BY TEM

  • MENG Yang ,
  • GU Lin ,
  • ZHANG Wen-Zheng
Expand
  • 1. Laboratory of Advanced Materials; Department of Materials Science and Engineering; Tsinghua University; Beijing 100084
    2. Max Planck Institute for Metals Research; Stuttgart D–70569

Received date: 2009-09-04

  Revised date: 2010-01-27

  Online published: 2010-04-11

Supported by

Supported by National Natural Science Foundation of China (No.50671051) and Specialized Research Fund for the Doctoral Program of Higher Education (No.20050003005)

Abstract

This paper presents a method for precise determination of the orientation of the irrational preferred interface by using TEM. The interface trace and the edge–on orientations are measured careflly and separately to minimize systematic error of thrsults. Tis method was developed according to the error analysis and the fact that te accuracy of the measurement is higher when the measurement is made directly on an interface trace tan on its project on an edge–on orientation, and whn the angle between the trace and the beam direction along the an edge–on orientation is larger. Compard with xisting methods, the present method has minimized the measurement errors and its resuts show better convergence.

Cite this article

MENG Yang , GU Lin , ZHANG Wen-Zheng . PRECISE DETERMINATION OF THE IRRATIONAL PREFERRED INTERFACE ORIENTATION BY TEM[J]. Acta Metall Sin, 2010 , 46(4) : 411 -417 . DOI: 10.3724/SP.J.1037.2009.00577

References

[1] Zhang W Z, Weatherly G C. Prog Mater Sci, 2005; 50: 181
[2] Howe J M. Interfaces in Materials: Atomic Structure, Thermodynamics and Kinetics of Solid–vapor, Solid–liquid and Solid–solid Interfaces. New York: John Wiley & Sons, Inc., 1997: 428
[3] Wayman C M, Hanafee J E, Read T A. Acta Metall, 1961; 9: 391
[4] Greninger A B, Troiano A R. Trans AIME. 1940; 140: 307
[5] Dunne D P, Bowles J S. Acta Metall, 1969; 17: 201
[6] Edington J W. Electron Diffraction in the Electron Microscope (Monographs in Practical Election Microscopy in Materials Science). London: Macmillan, 1975: 54
[7] Hirsh P, Howie A, Nicholson R B, Pashley D W, Whelan M J. Electron Microscopy of Thin Crystals. Malabar, Florida: Robert E. Krieger Publishing Company, 1977:311
[8] Kelly P M, Jostsons A, Blake R G, Napier J G. Phys Status Solidi, 1975; 31A: 771
[9] Zhang M X, Kelly P M, Gates J D. Mater Charact, 1999; 43: 11
[10] Liu Q. J Appl Crystallogr, 1994; 27: 762
[11] Young C, Steele J, Lytton J. Metall Mater Trans, 1973; 4B: 2081
[12] Zhou D, Shiflet G. Metall Mater Trans, 1992; 23A: 1259
[13] Zhang W Z, Purdy G R. Acta Metall Mater, 1993; 41: 543
[14] Qiu D, Zhang W Z. Acta Mater, 2007; 55: 6754

Outlines

/

〈 〉