论文

EFFECT OF DIFFERENT Nb–V CONTENTS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF CR8–TYPE COLD WORK DIE STEEL

  • CHI Hong-Xiao ,
  • MA Dang-Can ,
  • LIU Jian-Hua ,
  • CHEN Zai-Qi ,
  • YONG Qi-Long
Expand
  • 1. Faculty of Materials Science and Engineering; Kunming University of Science and Technology; Kunming 650093
    2. Institute for Structural Materials; Central Iron and Steel Research Institute; Beijing 100081

Received date: 2009-07-06

  Revised date: 2009-10-18

  Online published: 2010-02-10

Supported by

Supported by National Key Technologies R&D Program of China (No.2007BAE510B04)

Abstract

Cr8–type cold work die steels have been widely used in recent years. These steels have obvious secondary hardening effect due to high V content. Now it has been successfully used in high speed steel that Nb is substituted for V. However, it has been not widely applied in cold work die steel yet. In order to investigate the effect of different Nb–V contents on the microstructure and mechanical properties of this kind steel and the role of Nb in tool and die steels, in this paper the microstructure and morphology of three Cr8–type cold work die steels with different Nb–V contents were investigated by OM, SEM and EDS analysis, the mechanical properties including the hardness and impact toughness were measured at room temperature. Experimental results indicate that the precipitation temperature of MC–eutectic carbides increase with the increase of Nb content, and the improvement of their properties is closely related with Nb content. Moreover, the increase of Nb content causes the increase of metatectic and eutectic temperature and the disequilibrium of C distribution in primary γ phase. The granular carbides appear near the grain boundary of primary  phase when Nb content reaches to 1.32%; the variation in Nb/V ratio with the increase of Nb content will change the type of MC–eutectic carbides, the type of MC–eutectic carbides from mainly VC change to VC and a small amount of (Nb, V)C and then to mainly NbC and (Nb, V)C. So the shape of ledeburite is more straight. If Nb content reaches to 1.32%, the substitution of Nb for V increases quenching hardness, the peak of quenching hardness moves to low temperature region; the substitution of Nb for V is beneficial for secondary hardening in tested steels, and higher hardness and temper softening resistance can be obtained in them. In addition, their impact toughness decreases with the increase of Nb content.

Cite this article

CHI Hong-Xiao , MA Dang-Can , LIU Jian-Hua , CHEN Zai-Qi , YONG Qi-Long . EFFECT OF DIFFERENT Nb–V CONTENTS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF CR8–TYPE COLD WORK DIE STEEL[J]. Acta Metall Sin, 2010 , 46(2) : 206 -212 . DOI: 10.3724/SP.J.1037.2009.00450

References

[1] Chen Z Z, Lan D N. Die and Mould Steel Manual. Beijing: Metallurgical Industry Press, 2002: 18
(陈再枝, 蓝德年. 模具钢手册. 北京: 冶金工业出版社, 2002: 18)
[2] Ma D S, Liu J H, Chen Z Z, Kang A J, Chi H X. Iron Steel, 2008; 43(9): 67
(马党参, 刘建华, 陈再枝, 康爱军, 迟宏宵. 钢铁, 2008; 43(9): 67)
[3] Jeglitsch F. In: Minerals, Metals and Materials Society ed., Proceedings of the International Symposium Niobium 2001, Bridgeville: Niobium 2001 Ltd, 2002: 1001
[4] Liebfahrt W, Lichtenegger G, Schweiger H, Stamberger J. BHM, 2000; 145: 103
[5] Meyer L. In: Minerals, Metals and Materials Society ed., Proceedings of the International Symposium Niobium 2001, Bridgeville: Niobium 2001 Ltd, 2002: 359
[6] Geller Y A, Grishina Y L. Mach Tool, 1976; 47(6): 30
[7] Pacyna J, Strack M. Archives Metall, 1992; 37: 387
[8] Dobrzanski L A, Zarychta A. J Mater Process Technol, 1998; 77: 180
[9] Dobrzanski L A, Zarychta A, Ligarski M. J Mater Process Technol, 1995; 53: 109
[10] Dobrzanski L A, Zarychta A, Ligarski M. J Mater Process Technol, 1997; 63: 531
[11] Keown S R, Kudielka E, Heisterkamp F. Met Technol, 1980; 7(2): 50
[12] Riedl R, Karag¨oz S, Fischmeister H, Jeglitsch F. Steel Res, 1987; 58: 339
[13] Shi R X, Yang R C, Yin Y S, Zhou C H. Res Iron Steel, 2004; 2: 34
(师瑞霞, 杨瑞成, 尹衍升, 周春华. 钢铁研究, 2004; 2: 34)
[14] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 93, 117
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 93, 117)
[15] Hulka K, Guimar˜aes J R C. Companhia Brasileira de Metalurgia e Minerac˜ao Report, Sao Paula, Brazil, 1993: 1