论文

SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION

  • DIAO Xian-Wu ,
  • CHU Wu-Yang ,
  • QIAO Li-Jie
Expand
  • 1.Department of Mechanics and Aerospace Engineering; Peking University; Beijing 100871
    2.Corrosion and Protection Center; University of Science and Technology Beijing; Beijing 100083

Received date: 2009-04-30

  Revised date: 2009-11-17

  Online published: 2010-02-10

Supported by

Supported by National Natural Science Foundation of China (Nos.50632010 and 50572006)

Abstract

BaTiO3 single crystal with superior dielectric, pyroelectric, piezoelectric and electro–optic properties has triggered much attention due to numerous potential applications in microelectronic devices, sensors and micro/nanoelectromechanical systems. However, one of the main disadvantages for BaTiO3 single crystal is that after long–term working under mechanical field or electric field, cracks may be nucleated and propagated. The crack nucleation and propagation in ferroelectric materials are closely related to the domain configurations, and their relationship with crack propagation, nucleation and domain switching, is not known clearly, so it is imperative to take more effort to research this relationship. Here, the relationship of domain switching with crack propagating quickly as well as sub–critical crack growth in ambient air for constant deflection sample of BaTiO3 single crystal has been in situ tudied using a polarized light microscopy. The results indicate that domain switching occurs first and he volume fraction of swiched bnds increases dring loading. When the load reaches to a critical value, crack will be initiaed nd propagated qickly. Keeping the constant deflection, the domain switch could still occur but very slowly, i.e., adsorption of water in air is able to promote domain switchng. As a result of adsorption–enhanced domain switching, cracks are propagated lowly n air, that s say, sub–critical crack growth or stress corrosion cracking in air could occur for BaTiO3 single crystal under constant deflection.

Cite this article

DIAO Xian-Wu , CHU Wu-Yang , QIAO Li-Jie . SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION[J]. Acta Metall Sin, 2010 , 46(2) : 167 -171 . DOI: 10.3724/SP.J.1037.2009.00281

References

[1] Zhao X W, Chu W Y, Su Y J, Li J X, Gao K W, Qiao L J. Acta Metall Sin, 2006; 42: 13
(赵显武, 褚武扬, 宿彦京, 李金许, 高克玮, 乔利杰. 金属学报, 2006; 42: 13)
[2] Hao T H, Gong X, Suo Z. J Mech Phys Solids, 1996; 44: 23
[3] Jiang B, Bai Y, Chu W Y, Su Y J, Qiao L J. Appl Phys Lett, 2008; 93: 152905
[4] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102
[5] Yang W, Fang F, Tao M. Int J Solids Struct, 2001; 38: 2203
[6] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207
[7] Fang F, Yang W. Mater Lett, 2002; 57: 198
[8] Kreher W S. J Mech Phys Solids, 2002; 50: 1029
[9] Fang D N, Jiang Y J, Li S, Sun C T. Acta Mater, 2007; 55: 5758
[10] Jiang Y J, Fang D N, Li F X. Appl Phys Lett, 2007; 90: 222907
[11] Wang R M, Chu W Y, Su Y J, Li J X, Qiao L J. Mater Sci Eng, 2006; B135: 141
[12] Fang F, Yang W, Zhang F C. J Am Ceram Soc, 2005; 88:2491
[13] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583
[14] Su Y J, Wang Y, Chu W Y, Gao K W, Qiao L J. Acta Mater, 2004; 52: 3713
[15] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811
[16] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B95: 263
[17] Micjhalske T A, Freiman S W. J Am Ceram Soc, 1983; 66: 284

Outlines

/

〈 〉