ESTABLISHMENT AND APPLICATION OF FIXTURE CONSTRAINT MODELS IN FINITE ELEMENT ANALYSIS OF WELDING PROCESS

  • ZHANG Ceng-Lei ,
  • SHI Qing-Yu ,
  • YAN Dong-Xiang ,
  • SA Zhi-Peng ,
  • LI De-Cheng
Expand
  • 1.Department of Mechanical Engineering; Tsinghua University; Beijing 100084
    2.China Academy of Launch Vehicle Technology; Capital Aerospace Machinery Corporation; Beijing 100076

Received date: 2009-03-30

  Revised date: 2009-10-14

  Online published: 2010-02-10

Supported by

Supported by National High Technology Research and Development Program of China (No.2006AA04Z139)

Abstract

The mechanical interaction between welded panel and fixture has a remarkable influence on the distribution of weld–induced residual stress and distortion. Unfortunately, the influence of fixture is not generally included in conventional numerical simulations of welding process. In the present study, it is proposed that the numerical models in which the mechanical interaction between welded panel and fixture is considered as contact pair in the finite element analysis (FEA) of welding process. This could make the FEA of welding process more scientific and accurate. The fixture constraint plays an important role in accurate modeling of welding process. In the simulations, various mechanical constraint boundary conditions in welding process were thought about to establish the relationships of the normal and tangential mechanical interactions between welded panel and fixture. In Free model, the fixture restraint was not considered. In Mech model, the displacements of nodes where welded panel contacted with fixture were restricted in x, y, z directions. Hard model and Tabular model were contact models which included the fixture. In the normal direction, once welded panel and fixture were in contact, the transmitted contact pressure could be infinite in Hard model. While data pairs of contact pressure vs over–closure or clearance were specified to define a piecewise–linear relationship in the normal direction in Tabular model. A penalty friction coefficient of 0.3 was applied in tangential direction in both Hard and Tabular models. Fixture and welded panel were separated and the contact relationships were removed after the welding process in both Hard and Tabular models. The simulation results of contact models including fixture were more accurate, compared to models containing only welded panel with rigid retrictions. The distortiomode of welded panels under different fixture constrait conditions corresponded well with xperimental results. The differences between the distributions of transverse sresses on top and bottom surfaces f welded panel at the beginning of welding process had a crucial influence on the distortion mode f welded panel.

Cite this article

ZHANG Ceng-Lei , SHI Qing-Yu , YAN Dong-Xiang , SA Zhi-Peng , LI De-Cheng . ESTABLISHMENT AND APPLICATION OF FIXTURE CONSTRAINT MODELS IN FINITE ELEMENT ANALYSIS OF WELDING PROCESS[J]. Acta Metall Sin, 2010 , 46(2) : 189 -194 . DOI: 10.3724/SP.J.1037.2009.00198

References

[1] Dong P. Sci Technol Weld Joining, 2005; 10: 389
[2] Liu C, Zhang J X. Sci Technol Weld Joining, 2009; 14: 26
[3] Preston R V, Shercliff H R, WitherP J, Smith S. Acta Mater, 2004; 52: 4973
[4] Deng D, Murakawa H. Comput Mater Sci, 2008; 43: 591
[5] Li T, Shi Q Y, Li H K. Sci Technol Weld Joining, 2007; 12: 664
[6] Yang J G, Li J, Liu X S, Fang H Y. China Weld, 2008; 17: 39
[7] Tian X T. Weld Structure. Beijing: China Machine Press, 1995: 10
(田锡唐. 焊接结构. 北京: 机械工业出版社, 1995: 10)
[8] Preston R V, Shercliff H R, Withers P J, Smith S D. Sci Technol Weld Joining, 2003; 8: 10
[9] Schmidt H, Hattel J. Modell Simul Mater Sci Eng, 2005; 13: 77
[10] Abid M, Siddique M. Modell Simul Mater Sci Eng, 2005; 13: 919
[11] Zhang L, Silvanus J, Li H K, Shi Q Y. Sci Technol Weld Joining, 2008; 13: 422
[12] Zhang G D, Zhou C Y. Acta Metall Sin, 2008; 44: 848
(张国栋, 周昌玉. 金属学报, 2008; 44: 848)
[13] Yu S R, Fan D, Xiong J H. Trans Chin Weld Inst, 2008; 29: 25
(余淑荣, 樊 丁, 熊进辉. 焊接学报, 2008; 29: 25)
[14] Yan D Y, Si Q Y, Wu A P, Silvanus J, Liu Y, Zhang Z L. Acta Metall Sin, 2009; 45: 183
(鄢东洋, 史清宇, 吴爱萍, Silvanus J, 刘园, 张增磊. 金属学报, 2009; 45: 183)
[15] Nishikawa H, Serizawa H, Murakawa H. Sci Technol Weld Joining, 2007; 12: 147
[16] Zhang S L, Ren S Z. A Concise Handbook of Aluminum Alloy. 2nd Ed., Shanghai: Shanghai Scientific and Technological Literature Press, 2006: 9
(张士林, 任颂赞. 简明铝合金手册(第2版). 上海: 上海科学技术文献出版社, 2006: 9)
[17] Hibbitt, Karlsson & Sorensen, Inc.. ABAQUS/Standard User’s Manuals. Vol.3, Version 6.3, 2003: 120

Outlines

/

〈 〉