Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (11): 1154-1158    DOI:
Current Issue | Archive | Adv Search |
FIM STUDY ON (D0)3 ORDERING IN Fe3Al ALLOY
WENG Jun; ZHU Fengwu; WANG Wendong; ZHI Rentao; ZHANG Dezhi;XIAO Jimei (University of Science and Technology Beijing; Beijing 100083)
Cite this article: 

WENG Jun; ZHU Fengwu; WANG Wendong; ZHI Rentao; ZHANG Dezhi;XIAO Jimei (University of Science and Technology Beijing; Beijing 100083). FIM STUDY ON (D0)3 ORDERING IN Fe3Al ALLOY. Acta Metall Sin, 1996, 32(11): 1154-1158.

Download:  PDF(480KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Samples of Fe3Al with (D0)3 structure after annealing at 500℃ for 5 days were studied with field-ion microscope (FIM). Although the overall FIM ring structures of the treated Fe3Al are much developed, the ring structure of <111> pole is rather confused while that of the <100> pole is very clear. By successive observation, it was found that the <100> pole has a simple field evaporation sequence, while the <111> pole possesses a rather complicated one. This indicates that the ordering of type SI occurred in the (D0)3 order transformation tends to end, but the ordering of type SII is not completed.Prolonging the annealing time to 20 days under the same temperature did not result in a better <111> pole contrast. Correspondent: ZHI Rentao, professor, Department of Materials Physics, University of Science and Technology Beijing, Beijing 100083
Key words:  Fe3Al      field-ion microscopy      ordering     
Received:  18 November 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I11/1154

1SauthoffGZ.ZMetallk,1986;77:6542MckameyCG,DeVanJH,TortorelliPF,SikkaVK.JMaterRes,1991;4:17793KrauseHJ,WittigJE,FrommegerG.ZMetallk,1987;78:5764KrauseHJ,FrommeyerG,WittigJE,KrauseM.JPhysColloq,1988;C6-49:3655FrommeyerG,HabrockH-J,WittigJE,CzarnowskiP,GeenenJ,KreussM.ScrMetall,1990;24:516WengJ,ZhuF,XiaoJ.ZMetallk,1994;85:4327翁军,朱逢吾,职任涛,王双全,肖纪美.金属学报,1996;32:6958RudmanPS.ActaMetall,1960;8:3219翁军.北京科技大学博士学位论文,199510AnthonyL,FultzB.JMaterRes,1989;4:114011MendirattaMG,EhlersSK,ChatterjeeDK,LipsittHA.MetallTrans,1987;18A:28312MckameyCG,HortonJA,LiuCT.JMaterRes,1989;4:115613MorrisDG,DadrasMM,MorrisMA.ActaMetallMater,1993;41:9714StoloffNS,DavisRG.ActaMetall,1864;12:47315OkiK,HasakaM,EguchiT.TransJIM,1974;15:14316HasakaM,OkiK,EguchiT.TransJIM,1977;18:75017MarcinkowskiMJ,BrownN.ActaMetall,1961;9:764
[1] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[2] Yuanke MO,Zhihao ZHANG,Jianxin XIE,Hongjiang PAN. EFFECTS OF RECRYSTALLIZATION ON THE MICROSTRUCTURE, ORDERING AND MECHANICALPROPERTIES OF COLD-ROLLED HIGH SILICON ELECTRICAL STEEL SHEET[J]. 金属学报, 2016, 52(11): 1363-1371.
[3] WU Erdong GUO Xiumei SUN Kai. NEUTRON DIFFRACTION STUDY OF DEUTERIUM OCCUPANCY OF DEUTERIDE OF LAVES PHASE ALLOY Ti0.68Zr0.32MnCrD3.0[J]. 金属学报, 2009, 45(5): 513-518.
[4] ZHAO Yan CHEN Zheng WANG Yongxin HUO Jinliang ZHANG Lipeng ZHANG Mingyi . A MICROSCOPIC PHASE–FIELD STUDY FOR THE INFLUENCE OF ORDERING ENERGY ON Cr SUBSTITUTION BEHAVIOR IN Ni75Al15Cr10 ALLOY[J]. 金属学报, 2009, 45(5): 635-640.
[5] ZHANG Xinghua; LI Zhiqing; JIANG Enyong. INFLUENCE OF La DOPING ON THE STRUCTURE,MAGNETIC AND ELECTRICAL TRANSPORT PROPERTIES OF Pr0.75Na0.25MnO3[J]. 金属学报, 2006, 42(9): 974-978 .
[6] WANG Juan; LI Yajiang; MA Haijun. PRECIPITATE AT DIFFUSION-BONDED INTERFACE BETWEEN Fe3Al ALLOY AND STEEL Q235[J]. 金属学报, 2005, 41(9): 989-993 .
[7] GU Biao;NIE Yifan;GAO Kewei;CHU guyana (University of Science and Technology Beijing; Beijing 100083). IN SITU TEM OBSERVATION OF HYDROGEN-INDUCED CRACKING AND STRESS CORROSION CRACKING FOR Fe_3Al[J]. 金属学报, 1997, 33(7): 709-717.
[8] WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18). FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY[J]. 金属学报, 1996, 32(7): 695-699.
[9] YU Hingquan; SUN Yangshan; HUANG Haibo(Southeast University; Nanjing 210096)(Manuscript received 1994-11-18; in revised form 1995-03-30). EFFECT OF HOT-ROLLING ON MICROSTRUCTURE AND TENSILE PROPERTIES OF Fe_3Al BASED ALLOY[J]. 金属学报, 1995, 31(20): 368-373.
[10] WAN Hiaojing; ZHU Jiahong; HUANG Shengbiao(Shanghai University; Shanghai200072)(Manuscript received 1994-09-05). SURFACE REACTION OF Fe_3Al WITH WATER VAPOUR OR OXYGEN[J]. 金属学报, 1995, 31(16): 183-187.
[11] REN Xiaobing; Xiaotian(Xi'an Jiaotong University); SHIMIZU Ken'ichi(Kanazawa Institute of Technology;Japan) TADAKI Tsugio(Osaka University; Japan). CARBON ORDERING IN Fe-C MARTENSITE Ⅱ. Crystal Structure of Long-Period Ordered Phase[J]. 金属学报, 1994, 30(8): 337-343.
[12] REN Xiaobing; WANG Xiaotian (Xi'an Jiaotong University); SHIMIZU Ken'ichi (Kanazawa institute of Technology; Japan); TADAKI Tsugio (Osaka University;Japan)(Manuscript received 27 October; 1993; in revised form 4 January; 1994). CARBON ORDERING IN Fe-1.83C MARTENSITE Ⅰ. Crystal Structure of a Conventional Ordered Phase[J]. 金属学报, 1994, 30(7): 296-301.
[13] WANG Jinguo;CHEN Guoliang; SUN Zuqing (State Key Laboratory for Advanced Metal Materials; University of Science and Technology Beijing; Beijing)YE Hengqiang (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang)(Manuscript received 1 December; 1993; in revised form 13 July; 1994). STRUCTURE OF A NEW ORDERED TERNARY INTER- METALLIC COMPOUND IN TiAl+Nb SYSTEM[J]. 金属学报, 1994, 30(11): 525-53.
[14] WANG Jixin Baotou Research Institute of Rare Earth. SHORT RANGE ORDERING OF LIQUID ALLOY FOR Ag-Ln(Ln=La, Ce, Gd) SYSTEMS[J]. 金属学报, 1993, 29(11): 60-65.
[15] CHEN Shuchuan;XU Zuyao T. Y. Hsu; YANG Fan Shanghai Jiaotong University; ZHANG Jihua Shanghai Institute of Metallurgy; Academia Sinica. STABILIZATION OF MARTENSITE AND PARENT PHASE ORDERING IN A Cu-Zn-Al ALLOY[J]. 金属学报, 1991, 27(4): 5-10.
No Suggested Reading articles found!