| ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM |
| ZHANG Peng;CUI Jianzhong;ZHANG Qizhi;DU Yunhui;FU Jiangtao;BA Limin (Northeastern University;Shenyang 110006)(Manuscript received 1996-05-21;in revised form 1996-07-11) |
|
Cite this article:
ZHANG Peng;CUI Jianzhong;ZHANG Qizhi;DU Yunhui;FU Jiangtao;BA Limin (Northeastern University;Shenyang 110006)(Manuscript received 1996-05-21;in revised form 1996-07-11). ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM. Acta Metall Sin, 1996, 32(12): 1275-1278.
|
|
|
Abstract Effects of concentration of flux solution,temperature of liquid aluminium,temperature of tools and pressure on shearing strength in solid-liquid pressure bonding of stainless steel and aluminium were investigated by means of artificial neural networks. The optimum bonding parameters were optimized with a genetic algorithm.
|
|
|
| 1富江涛.东北大学硕士论文,19962HopfieldJJ.ProcNatAcadSciUSA,1982;79:25543PsaltisD,SiderisA,TamanmuyaA.IEEEControlSystMag,1988;8:174严六明,钦佩,李重河.科学通报,1994;39(1):945王殿辉,诸良银.有色金属,1994;46(1):296SongRG,ZhangQZ,TsengMK,ZhangBJ.MaterSciEng,1995;C3:39t |
| No Suggested Reading articles found! |
|
|