PREPARATION OF NANOCRYSTALLINE METALLIC α-Co BY γ-RAY RADIATION
CHEN Zuyao; ZHANG Guochun;ZHU Yurui (Structure Research Laboralory; Science & Technology of China; Chinese academy of Sciences; Hefei 230026)
Cite this article: 

CHEN Zuyao; ZHANG Guochun;ZHU Yurui (Structure Research Laboralory; Science & Technology of China; Chinese academy of Sciences; Hefei 230026). PREPARATION OF NANOCRYSTALLINE METALLIC α-Co BY γ-RAY RADIATION. Acta Metall Sin, 1997, 33(10): 1110-1114.

Download:  PDF(1744KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Ultrafine particles and powders of metallic α-Co were prepared in an aqueous solution of Co2+ by γ-ray radiation. The ultrafines appear as nanocrystallined particles according to X-ray and electron diffraction. The average size of particles is 30 nm while concentration of cobalt acetate solution, irradiation dose and solution pH are in the range of 0.005-0.2 mol / L, 2.3×104-3.9 ×105 Gy and 6.0-10.0 respectively.
Key words:  α-Co ultrafine particle      γ-ray radiation      microwave radiation     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1110

1 Gibson C P,Putzer K J,Science,1995;267:1338
2 Haneda K.Can J Phys,1987;65:1233
3 Lion H.Chien C L.J appl Phys, 1988;63:4240
4 Bridger K, Watts J, Chien C L,J appl Phys, 1988;63:3233
5 Harriman a Pickering I J, Thomas J M, Christensen P a.J Chem Soc Faraday Trans,1988;1842795
6罗红梅.中国科学技术大学硕士学位论文,1994
7 Xiao J Q.Jiang J S ,Chien C L,Phys Rev Lett,1992;68:3749
8 Tsoukatos a,Wan H,Hadijipanayis G C,Li Z G.appl Phys Lett,1992;61:3059
9 Chen J P,Lee K M.J appl Phys,1994;75:5876
10 Chow G M,Kurihara L K,Kemner K M,Schoen P E,Elam W T、J Mater Res;1995;10:1546
11 Vasilikov a Y,olenin a Y,Titova E F,Sergeev V a.J Colloid Inter face Sci,1995;169:356
12 Jin Gu,Zhu Yu-rui,jiang Wan-quan.Submitted to analyst
13张曼维编著,辐射化学入门,合肥:中国科学技术大学出版社,1993
14张国春,陈祖耀,朱玉瑞等,硅酸盐学报(待发表)
15 Katsumura Y, Jiang P Y,Nagaishi R, J Phvs Chem,1991:95:4435
16陈祖耀,陈波,钱逸泰,张曼维,杨丽、范成高.金属学报1992;28:B169
[1] CHEN Zuyoo; CHEN Min;ZHU Yurui; CHEN Wenming; QIAN Yitai;YANG Li(Structure Research Laboratory; University of Science & Technology of China;Chinese Academy of Sciences; Hefei 230026)(University of Soience & Technology of China; Hefei 230026). PREPARATION OF Cu_2O ULTRAFINES BY ULTRAVIOLET RADIATION AND THEIR MACRO-DYNAMICS[J]. 金属学报, 1997, 33(3): 330-336.
[2] CHEN Zuyao;CHEN Bo;QIAN Yitai;ZHANG Manwei;YANG Li;FAN Chenggao University of Science and Technology of China; Hefei. PREPARATION OF ULTRAFINE METALLIC PARTICLES BY γ-RAY RADIATION HYDROTHERMAL CRYSTALLIZATION COMBINED METHOD[J]. 金属学报, 1992, 28(4): 73-76.
No Suggested Reading articles found!