Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (8): 852-857    DOI:
Current Issue | Archive | Adv Search |
A NEW ASSEMBLY AND EVALUATION OF DYNAMIC FRACTURE TOUGHNESS K_(1d) OF HIGH STRENGTH STEEL AT HIGH VELOCITY IMPACT
LI Qiang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)LAI Zuhan(International Centre for Material Physics; The Chinese Academy of Sciences; Shenyang 110015)MA Changxiang(College of Sciences; Northeastern University; Shenyang 110006)Correspondent: LI Qiang; Tel: (024)23843531-55659; Fax: (024)3891320; E-mail: qli imr ac.cn
Cite this article: 

LI Qiang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)LAI Zuhan(International Centre for Material Physics; The Chinese Academy of Sciences; Shenyang 110015)MA Changxiang(College of Sciences; Northeastern University; Shenyang 110006)Correspondent: LI Qiang; Tel: (024)23843531-55659; Fax: (024)3891320; E-mail: qli imr ac.cn. A NEW ASSEMBLY AND EVALUATION OF DYNAMIC FRACTURE TOUGHNESS K_(1d) OF HIGH STRENGTH STEEL AT HIGH VELOCITY IMPACT. Acta Metall Sin, 1998, 34(8): 852-857.

Download:  PDF(453KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new assembly with a long impact bar for measuring the dynamic fracture toughness K1d under the condition of fast fracture is described in this paper. The basic principle and the method evaluating K1d under the condition of the fracture time tf being less than the oscillation period of the specimen (τ) are given which include not only the impact velocity but also the impact load. An example is presented for measuring K1d of high strength armour steel 30MnCrNiMoB quenched and tempered at 200 - 600℃. The results show that Kid increases with the loading time under high velocity impact, which are similar to those of 4340 AVR steel reported.
Key words:  dynamic fracture toughness      high velocity impact      high strength armour steel     
Received:  18 August 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I8/852

1 Donald A. Dynamic Fracture Testing, Metals Handbook Vo1.8, New York: ASM, 1985: 259
2 Kobayashi T. Eng Fract Mech, 1984; 19: 49
3 Kobayashi T. Eng Fract Mech 1984; 19: 67
4 Kishimoto K, Aoki S, Sakata M. Eng Fract Mech 1980; 13: 501
5 Nash G E. Int J Fract Mech, 1969; 15: 269
6 Lee Y, Prakash V. Metoll Mater Trans, 1995; 26A: 2527
7 Tang C A, Xu X H. Eny Fract Mech 1990; 35(4/5): 783
8 Kalthoff J F. Int J Fract, 1985; 27: 277
9 Martin E, Mack T, Quenisset J M. Eng Fract Mech 1986; 24: 821
10 Liu Y N, Zhu J H, Zhou H J. Eng Fract Mech 1991; 39: 955
[1] Xiangli FENG,Lei WANG,Yang LIU. STUDY ON MICROSTRUCTURE AND DYNAMIC FRACTURE BEHAVIOR OF Q460 STEEL WELDING JOINTS[J]. 金属学报, 2016, 52(7): 787-796.
[2] XU Zejian; LI Yulong; LI Na; LIU Yuanyong. EFFECT OF LOADING RATE ON MODE I DYNAMIC FRACTURE TOUGHNESS OF HIGH STRENGTH STEELS 40Cr AND 30CrMnSiNi2A[J]. 金属学报, 2006, 42(9): 965-970 .
[3] LIN Junshan;YAN Wenbin;TU Mingjing Xi'an Jiaotong University. CRACK INITIATION POINT DETERMINATION AND DYNAMIC FRACTURE TOUGHNESS FOR CHARPY PRE-CRACKED SPECIMEN[J]. 金属学报, 1992, 28(4): 28-33.
[4] XU Changgan;ZENG Zhongping Beijing University of Aeronautics and Astronautics. DYNAMIC FRACTURE TOUGHNESS OF ULTRA-STRENGTH STEELS FOR AIRCRAFT USE[J]. 金属学报, 1990, 26(6): 63-67.
No Suggested Reading articles found!