TRANSFORMATION MECHANISM OF FINE FULLY LAMELLAR MICROSTRUCTURE IN TiAl ALLOYS
ZHANG Ji; ZHANG Zhihong; SHI Jiandong; ZOU Dunxu; ZHONG Zengyong (Department of Superalloys; Central Iron and Steel Research Institute; Beijing 100081)Correspondent: ZHANG Ji; Doctor; Tel. (010)62181009; Fax: (010)62172725;E-mail: htmrd@public. bta.net.cn
Cite this article:
ZHANG Ji; ZHANG Zhihong; SHI Jiandong; ZOU Dunxu; ZHONG Zengyong (Department of Superalloys; Central Iron and Steel Research Institute; Beijing 100081)Correspondent: ZHANG Ji; Doctor; Tel. (010)62181009; Fax: (010)62172725;E-mail: htmrd@public. bta.net.cn. TRANSFORMATION MECHANISM OF FINE FULLY LAMELLAR MICROSTRUCTURE IN TiAl ALLOYS. Acta Metall Sin, 1998, 34(9): 919-922.
Abstract The fine fully lamellar (FFL) microstructure and intermedium microstructures in the process of forming FFL microstructure were examined under optical and transmission electronic microscopes. Based on the observation results, the transformation mechanism of FFL microstructure was analyzed and proposed as that the fine γ/α lamellar colonies form at the high temperature in the α single phase region through the precipitating of the α plates on the four equivalent habit planes {111}γ, in each γ matrix grain and then evolve to the γ/α2 lamellar colonies of the FFL microstructure.
1 Kim Y W, Dimiduk M JOM, 1991; 43(8): 40 2 Kim Y W Acta Metall, 1992 40: 1121 3 Chan K S, Kim Y W. Metall Trans, 1992 23A: 1663 4 张继,张志宏,邹敦叙,仲增墉.金属学报,1996,32A:1044(Zhang J,Zhang Z H,Zou D X,Zhong Z Y.Acta Metall Sin, 1996 32A:1663) 5 Zhang J, Zou D X, Wang Y, Zhang Z Y. In: Kim S W, Park S J eds. Proc 3rd IUMRS Int Conf in Asia, vol. 1, Seoul, Korea:MRS of Korea, 1995: 403 6 张继,马万青,邹敦叙,仲增墉,张志宏,曾梅光.金属热处理学报,1996;17(3):16(Zhang J,Ma W Q,Zou D X,Zhong Z Y,Zhang Z H,Zeng M G. Trans Met Heat Treat, 1996;17(3):16) 7 Yang Y S, Wu S K Scr Metall, 1990 24: 1801 8 Jones S A, Kanfman M J. Acta Metall Mater, 1993; 41: 387"