3D ATOM PROBE CHARACTERAZATION OF ALLOY CARBIDES IN TEMPERING MARTENITE  III. Coarsening
LIU Qingdong1; 2);  CHU Yuliang1);  PENG Jianchao1);   LIU Wenqing1);   ZHOU Bangxin1)
1) Instrumental Analysis & Research Center; Shanghai University; Shanghai 200444
2) Institute of Research of Iron and Steel; Jiangsu Province and Sha-Steel; Suzhou 215625
Cite this article: 

LIU Qingdong CHU Yuliang PENG Jianchao LIU Wenqing ZHOU Bangxin. 3D ATOM PROBE CHARACTERAZATION OF ALLOY CARBIDES IN TEMPERING MARTENITE  III. Coarsening. Acta Metall Sin, 2009, 45(11): 1297-1302.

Download:  PDF(1353KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

It has been confirmed that the fcc MC-type carbides such as VC and NbC have plate-like morphology and are mutually soluble when precipitated in tempering steel with martensite microstructure. Over-tempering makes the plate--like carbide change to spherical shape because of Ostwald coarsening. As coarsening is strongly linked to the diffusion rate of the carbide-forming elements, it is easy to understand that inhomogeneous structure may be formed when more kinds of elements were added, such as V, Nb and Mo. Besides, non-carbide-forming elements such as Si and Al tend to diffuse toward matrix. The morphology and lattice structure of carbide change simultaneously companying with the compositional redistribution of alloy elements. The detail compositional and nano-structural informations of the carbide can be obtained by 3DAP and HRTEM. In this paper, 3DAP and HRTEM were applied to characterize the composition, morphology and nanostructure of the carbide precipitated during 650 ℃ tempering of as-quenched Nb-V microalloyed steel. The results indicated that the martensite lath morphology was replaced by defect--free polygonal ferrite due to the recovery and recrystallization of the as-quenched microstructure. Simultaneously, the carbide-forming elements Mo and V diffused from smaller carbides to larger ones, resulting in the co-existence of carbides with different sizes and compositions. With the diffusion and redistribution of alloy elements, the prior-formed plate-like carbides grew along the radial direction, and a kind of transition carbide (Pouter) which is semi-coherent with ferrite matrix (Mbcc) was consequently formed. 3DAP constructional atom map demonstrated that Si and Al are rejected from the alloy carbide, whereas Mn and V were inhomogeneously distributed. That is, the coarsening carbide has a core-shell complex nanostructure, the core contains V, Mn, Mo and Nb, and the external shell contains Mo and Nb.

Key words:  3D atom probe (3DAP)      tempering martensite      alloy carbide      coarsening     
Received:  29 April 2009     
ZTFLH: 

TG113.25

 
Fund: 

Supported by Key Project of National Natural Science Foundation of China (No.50931003), Shanghai Leading Academic Discipline Project (No.S30107) and Shanghai Committee of Science and Technology Project (No.09520500100)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I11/1297

[1] Pickering F B. Physical Metallurgy and the Design of Steels. London: Applied Science Publishers, Ltd., 1978: 60
[2] Honeycombe R W K. Steels, Microstructure and Properties. London: Edward Arnold, 1980: 65
[3] Yong Q L. Secondary Phase in Steel. Beijing: Metallurgical Industry Press, 2006: 415
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 415)

[4] Kaori M, Tomohiro O, Takahiro K, Yuichi K. Metall Mater Trans, 2003; 34A: 1565
[5] Hu Z F, Wu X F, Wang C X. Acta Metall Sin, 2003; 39: 585
(胡正飞, 吴杏芳, 王春旭. 金属学报, 2003; 39: 585)

[6] Miller M K. Atom Probe Tomography. NewYork: Plenum Press, 2000: 19
[7] Zhu C, Xiang X Y, Cerezo A, Hardwicke R, Krauss G, Smith G D W. Ultramicroscopy, 2007; 107: 808
[8] Caballero F G, Miller M K, Garcia–Mateo C, Capdevila C, Babu S S. Acta Mater, 2008; 56: 188
[9] Miyamoto G, Oh J C, Hono K, Furuhara T, Maki T. Acta Mater, 2007; 55: 5027
[10] Liu Q D, Chu Y L, Wang Z M, Liu W Q, Zhou B X. Acta Mater Sin, 2008; 44: 1281
(刘庆冬, 褚于良, 王泽民, 刘文庆, 周邦新. 金属学报, 2008; 44: 1281)

[11] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2008; 44: 786
(刘庆冬, 刘文庆, 王泽民, 周邦新. 金属学报, 2008; 44: 786)

[12] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2009; 45: 1281
(刘庆冬, 刘文庆, 王泽民, 周邦新. 金属学报, 2009; 45: 1281)

[1] Mingfang ZHU, Like XING, Hui FANG, Qingyu ZHANG, Qianyu TANG, Shiyan PAN. Progresses in Dendrite Coarsening During Solidification of Alloys[J]. 金属学报, 2018, 54(5): 789-800.
[2] Yu ZHANG, Qing WANG, Honggang DONG, Chuang DONG, Hongyu ZHANG, Xiaofeng SUN. Nickel-Based Single-Crystal Superalloys (Ni, Co)-Al-(Ta, Ti)-(Cr, Mo, W) Designed by Cluster-Plus-Glue-Atom Model and Their 1000 h Long-Term Ageing Behavior at 900 ℃[J]. 金属学报, 2018, 54(4): 591-602.
[3] Ke ZHANG, Xinjun SUN, Qilong YONG, Zhaodong LI, Gengwei YANG, Yuanmei LI. EFFECT OF TEMPERING TIME ON MICROSTRUC- TURE AND MECHANICAL PROPERTIES OF HIGH Ti MICROALLOYED QUENCHED MARTENSITIC STEEL[J]. 金属学报, 2015, 51(5): 553-560.
[4] DI Xinjie, XING Xixue, WANG Baosen. NUCLEATION AND COARSENING MECHANISM OF δ PHASE IN INCONEL 625 DEPOSITED METAL[J]. 金属学报, 2014, 50(3): 323-328.
[5] WANG Xue, YU Shumin, REN Yaoyao, LIU Hong, LIU Hongwei, HU Lei. LAVES PHASE EVOLUTION IN P92 STEEL DURING AGEING[J]. 金属学报, 2014, 50(10): 1195-1202.
[6] DONG Qiyi, SHEN Leinuo, CAO Feng, JIA Yanlin, WANG Mingpu. STUDY OF THE COARSENING AND HARDENING BEHAVIORS OF COHERENT g-Fe PARTICLES IN Cu-2.1Fe ALLOY[J]. 金属学报, 2014, 50(10): 1224-1230.
[7] TAN Meilin, WANG Changshuai, GUO Yongan, GUO Jianting, ZHOU Lanzhang. INFLUENCE OF Ti/Al RATIOS ON γ′ COARSENING BEHAVIOR AND TENSILE PROPERTIES OF GH984G ALLOY DURING LONG-TERM THERMAL EXPOSURE[J]. 金属学报, 2014, 50(10): 1260-1268.
[8] ZHAO Yan, ZHANG Hongyu, WEI Hua, ZHENG Qi, JIN Tao, SUN Xiaofeng. A PHASE FIELD STUDY FOR SCALING RULES OF GRAIN COARSENING IN POLYCRYSTALLINE SYSTEM CONTAINING SECOND-PHASE PARTICLES[J]. 金属学报, 2013, 49(8): 981-988.
[9] ZENG Qiang, YAN Ping, SHAO Chong, ZHAO Jingchen, HAN Fengkui,ZHANG Longfei. INVESTIGATION ON COARSENING BEHAVIORS OF SERRATED GRAIN BOUNDARIES IN K480 NICKEL BASE SUPERALLOY DURING LONG TERM AGING AT 900 ℃[J]. 金属学报, 2013, 49(1): 63-70.
[10] ZHOU Guangzhao, WANG Yongxin, CHEN Zheng. PHASE-FIELD METHOD SIMULATION OF THE EFFECT OF ELASTIC STRAIN ENERGY ON COARSENING DYNAMICS DURING THE α2→ O PHASE TRANSFORMATION IN Ti-Al-Nb ALLOYS[J]. 金属学报, 2012, 48(4): 485-491.
[11] Gong Bo WEN Shengping HUANG Hui NIE Zuoren. EVOLUTION OF NANOSCALE Al3(ZrxEr1-x) PRECIPITATES IN Al-6Mg-0.7Mn-0.1Zr-0.3Er ALLOY ALLOY DURING ANNEALING[J]. 金属学报, 2010, 46(7): 850-856.
[12] WANG Xiaojing ZHU Qingsheng WANG Zhongguang SHANG Jianku. MODELING OF Ag3Sn COARSENING AND ITS EFFECT ON CREEP IN Sn-Ag-Cu SOLDER[J]. 金属学报, 2009, 45(8): 912-918.
[13] JIANG Qingwei LIU Yin WANG Yao CHAO Yuesheng LI Xiaowu . MICROSTRUCTURAL INSTABILITY OF ULTRAFINE--GRAINED COPPER UNDER ANNEALING AND HIGH--TEMPERATURE DEFORMING[J]. 金属学报, 2009, 45(7): 873-879.
[14] LEI Wenping SHEN Jian MAO Baiping LI Junpeng YAN Liangming. STUDY ON AGING PRECIPITATION BEHAVIOR OF Al–5.2Cu–0.4Mg–1.02Ag ALLOY[J]. 金属学报, 2009, 45(5): 579-584.
[15] LIU Qingdong; LIU Wenqing; WANG Zemin; ZHOU Bangxin. 3D ATOM PROBE CHARACTERAZATION OF ALLOY CARBIDES IN TEMPERING MARTENITE   I. Nucleation[J]. 金属学报, 2009, 45(11): 1281-1287.
No Suggested Reading articles found!