| EXPERIMENTAL INVESTIGATION ON FORMING PROCESS OF HUMPING BEAD IN HIGH SPEEDMAG ARC WELDING |
| HU Zhikun;WU Chuansong |
| Institute for Materials Joining; Shandong University |
|
Cite this article:
HU Zhikun WU Chuansong. EXPERIMENTAL INVESTIGATION ON FORMING PROCESS OF HUMPING BEAD IN HIGH SPEEDMAG ARC WELDING. Acta Metall Sin, 2008, 44(12): 1445-1449.
|
|
|
Abstract High-speed metal-active gas (MAG) arc welding experiments were conducted to determine the critical welding speeds at which humping defects occur, the spacing between two adjacent humps along the welding direction, and the cross-section morphologies of the hump and the valley in a humping bead. Based on the weld pool images sensed during high-speed MAG welding process, the forming mechanism of humping bead is analyzed and verified through up-hill and down-hill welding experiments. Meanwhile, the effect of the compositions of shielding gas on the weld bead formation in high--speed MAG welding is also analyzed.
|
|
Received: 31 March 2008
|
|
|
[1]Guan Q,Lin S Y.In:China Welding Society,ed.,Proc New Fusion Welding Technologies and Applications,Bei- jing:China Welding Society,2003:11 (关桥,林尚扬.中国焊接学会主编,熔焊新技术及应用研讨会论文集,北京:中国焊接学会,2003:11) [2]Wu C S,Zhang M X,Li K H,Zhang Y M.Acta Metall Sin,2007;43:663 (武传松,张明贤,李克海,张裕明.金属学报,2007;43:663) [3]Tusek J.Weld Rev Int,1996;15:102 [4]Mills K C,Keene B J.Int Mater Rev,1990;35:185 [5]Mendez P F,Eagar T W.Weld J,2003;82:296 [6]Gratzke U,Kapadiat P D,Dowdent J.J Phys,1992;25D: 1640 [7]Feng L.PhD Thesis,Beijing University of Technology, 1999 (冯雷.北京工业大学博士学位论文,1999) [8]Nguyen T C,Weckman D C.Sci Technol Weld Join,2005; 10:447 [9]Nguyen T C,Weckman D C.Sci Technol Weld Join,2007; 12:634 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|