Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (2): 177-182     DOI:
Research Articles Current Issue | Archive | Adv Search |
Preparation Of High Temperature Proton Conductor Tube CaZr0.9In0.1O3-α And Its Properties
东北大学
Cite this article: 

. Preparation Of High Temperature Proton Conductor Tube CaZr0.9In0.1O3-α And Its Properties. Acta Metall Sin, 2008, 44(2): 177-182 .

Download:  PDF(462KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  High temperature proton conducotor CaZr0.9In0.1O3-α was prepared by direct synthesis method, and the average grain diameter of the powder was 1.88μm. Hot pressure casting method was used for preparing the tube, whose density was 97.44% relative to theoretical density. SEM fracture analysis showed the grain size was 1~3μm. EDS and XRF showed that the material had In elelment lost after sintered. This is because In2O3 sublimed and decomposed when temperature was higher than 1200℃. The conductivity of CaZr0.9In0.1O3-α was 0.91×10-4~1.21×10-2 S•cm-1 at the temperature range of 931~1300K in air. The value was a little small than the value in H2 and larger than the value of CaZr0.97In0.03O3-α in air in the literature. This was corresponded with theoretical conjecture.
Key words:  CaZrO3 doped      CaZr0.9In0.1O3-α      AC impedance spectroscopy      high temperature proton conductor      
Received:  28 March 2007     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I2/177

[1]Iwahara H,Esaka T,Uchida H,Maeda N.Solid State Ion- ics,1981;3-4:359
[2]Uchida H,Maeda N,Iwahara H.Solid State lonics,1983; 11:117
[3]Iwahara H,Esaka T,Uchida H,Yarnauchi T,Ogaki K. Solid State Ionics,1986;18-19:1003
[4]Iwahara H.Solid State Ionics,1988;28-30:573
[5]Iwahara H,Uchida H,Ondo K,Ogaki K.J Electrochem Soc,1988;135:529
[6]Iwahara H.Proc Int Seminar Solid State Ionic Devices, Singapore,1988;18-23:289
[7]Uchida H,Yoshikawa H,Esaka T,Ohtsu S,Iwahara H. Solid State Ionics,1989;36:89
[8]Yajima T,Koide K,Yamamoto K,Iwahara H.Denki Ka- gaku,1990;58:547 (Yajima T,Koide K,Yamamoto K,Iwahara H.电气化学工业物理化学,1990;58:547)
[9]Yajima T,Iwahara H,Koide K,Yamamoto K.Sensors Actuators B:Chemical,1991;5B:145
[10]Yajima T,Iwahara H,Uchida H.Solid State Ionics,1991; 47:117
[11]Yajima T,Kazeoka H,Yogo T,Iwahara H.Solid State Ionics,1991;47:271
[12]Yajima T,Suzuki H,Yogo T,Iwahara H.Solid State Ion- ics,1992;51:101
[13]Hibino T,Mizutani K,Yajima T,Iwahara H.Solid State Ionics,1992;57:303
[14]Iwahara H,Yajima T,Hibino T,Ozaki K,Suzuki H.Solid State Ionics,1993;61:65
[15]Iwahara H.Solid State Ionics,1995;77:289
[16]Yajima T,Koide K,Takai H,Fukatsu N,Iwahara H.Solid State Ionics,1995;79:333
[17]Xu X G,Wang C Z,Yu H L,Liu H B.J Northeast Univ (Nat Sci),1996;17:374 (徐秀光,王常珍,于化龙,刘宏波.东北大学学报(自然科学版),1996;17:374)
[18]Yang N R,Yue W H.The Handbook of Inorganic Metal- loid Materials Atlas.Wuhan:Wuhan University of Tech- nology Press,2000:211 (杨南如,岳文海.无机非金属材料图谱手册.武汉:武汉工业大学出版社,2000:211)
[19]Fedorov B E,Akchurin P X.Translated by Zhang Q Y, Xu K M.Indium Chemistry Handbook.Beijing:Peking University Press,2005:24 (著.张启运,徐克敏译.铟化学手册.北京:北京大学出版社,2005:24)
[1] WANG Dong LIU Chunming WANG Changzhen. PREPARATION AND CHARACTERISTICS OF HIGH TEMPERATURE PROTON CONDUCTOR Ba3Ca1.18Nb1.82O9-δ[J]. 金属学报, 2009, 45(3): 345-350.
No Suggested Reading articles found!