ANALYSIS OF REDUCTION EFFICIENCY IN SOFT REDUCTION FOR CONTINUOUS CASTING SLAB |
LIN Qi-Yong |
东北大学 |
|
Cite this article:
LIN Qi-Yong. ANALYSIS OF REDUCTION EFFICIENCY IN SOFT REDUCTION FOR CONTINUOUS CASTING SLAB. Acta Metall Sin, 2007, 43(12): 1301-1304 .
|
Abstract Based on the analysis of continuous casting slab soft reduction process, a expression to calculate soft reduction efficiency was deduced, and the effects of soft reduction amount and liquid core thickness on reduction efficiency were investigated. The results show that the reduction efficiency increases linearly with the increase of liquid core thickess as reduction amout is the same, and as the reduction amount is bigger than 2.3mm, the relationship of reduction efficiency η and reduction amount △H can be expressed by η=-0.00902+0.01155△H. For the same thickness of liquid core, the increase of reduction amount will induce the increase of reduction efficiency as reduction amount is less than 2.3mm, while the reduction amount has little effect on reduction efficiency as reduction amount is bigger than 2.3mm.
|
Received: 14 June 2007
|
|
[1]Sivesson P,Hallen G,Widell B.Ironmaking Steelmaking, 1998;25:239 [2]Raja V R,Pal N,Jayaswal N P.Steel Times Int,2005; 29:41 [3]Scholes A.Ironmaking Steelmaking,2005;32:101 [4]Flemings M C.ISIJ Int,2000;40:833 [5]Yim C H,Park J K,You B D,Yang S M.ISIJ Int,1996; 36:S231 [6]Lin Q Y,Zhu M Y.Acta Metall Sin,2007;43:847 (林启勇,朱苗勇.金属学报,2007;43:847) [7]Ito Y,Yamanaka A,Watanabe T.Rev Metall,2000;97: 1171 [8]Han H N,Lee J E,Yeo T,Won Y M.ISIJ Int,1999;39: 445 [9]Won Y M,Kim K H,Yeo T,Oh K H.ISIJ Int,1998;38: 1093 [10]Zhang J Q,Cui L X,Chen Z P,Chen S Q.J Univ Sci Technol Beijing,2004;26:373 (张家泉,崔立新,陈志平,陈素琼.北京科技大学学报,2004;26:373) [11]Lin Q Y.Master Dissertation,Northeastern University, Shenyang,2004 (林启勇,东北大学硕士学位论文,沈阳,2004) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|