Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (5): 557-560     DOI:
Research Articles Current Issue | Archive | Adv Search |
PREPARATION OF MICRO-NANO METAL MATERIAL WITH BIOLIMITED FORMING TECHNOLOGY
;;
Cite this article: 

. PREPARATION OF MICRO-NANO METAL MATERIAL WITH BIOLIMITED FORMING TECHNOLOGY. Acta Metall Sin, 2007, 43(5): 557-560 .

Download:  PDF(269KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Cu nano-particles and homogeneous Cu coating on Nocadia surface studied by microbiological method and surface analysis technology were prepared by electroless deposition method with appropriate surfactant. It was found that surfactant A was superior to some other kind surfactant under the same other conditions. Nocadia dispersed in pre-processes solutions and electroless plating solutions in the synergistic action of surfactant A and agitation. Cu particles with the size of 20nm deposited on Nocadia surface successfully and formed homogeneous Cu coating with the thickness of 200nm. Nocadia remained their original rod shape after Cu nano-particles deposition. Micro-rod metal material formed of Cu nano-particels was obtained.
Key words:  biolimited forming technology      micro-nano material      Nocadia      
Received:  06 September 2006     
ZTFLH:  O641  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I5/557

[1] Zhang D Y, Li Y Q. In: Yang H Y, Li W, eds., 4th Int Conf on Frontiers of Design and Manufacturing, Beijing: International Academic Publishers, 2000: 17
[2] Sleytr U B, Messner P, Sara M, Pum D. Syst Appl Microb, 1986; 7: 301
[3] Shenton W, Pum D, Sleytr U B, Mann S. Nature, 1997; 389: 585
[4] Whaley S R, English D S, Hu E L, Barbara P F, Belcher A M. Nature, 2000; 405: 665
[5] Lee S W, Mao C B, Flynn C E, Belcher A M. Science, 2002; 296: 892
[6] Matsui H, Gologan B. J Phys Chem, 2000; 104B: 3383
[7] Matsui H, MacCuspie R. Nano Lett, 2001; 1: 671
[8] Matsui H, Porrata P, Douberly G E. Nano Lett, 2001; 1: 461
[9] Li X F , Li Y Q , Cai J, Zhang D Y. Sci Chin, 2003; 46E: 161
[10] Li X F, Li Y Q, Cai J, Zhang D Y. Chin Sci Bull, 2003; 48: 145 (黎向锋,李雅芹,蔡军,张德远.科学通报,2003;48:145)
[11] Cai J, Li Y Q, Li X F, Zhang D Y. J Magn Magn Mater, 2002; 246: 36
[12] Tay B Y, L. Liu, Loh N H, Tor S B, Murakoshi Y, Maeda R. Mater Character, 2006; 57(2): 80
[13] Zhang Y S, Wang L S, Liu X H, Yan Y J, Chen C Q, Zhu J. J Phys Chem, 2005; 109B: 13091
[14] Zhang S G, Marini D M, Hwang W, Santoso S. Curr Opin Chem Biology, 2002; 6: 865
[15] Hu C X. Handbook of Surface Pre- Processing in Practice. Beijing: Chemical Industry Press, 2003: 392 (胡传炘.实用表面前处理处理手册.北京:化学工业出版社, 2003:392)
[1] ZHANG Weihu ZHANG Fuchun ZHANG Zhiyong YAN Junfeng . FIRST–PRINCIPLE ANALYSYS ON FINE STRUCTURE OF Pb0.5Sr0.5TiO3[J]. 金属学报, 2009, 45(2): 217-222.
[2] TONG Guo-Xing. PREPARATION OF LIGHT RADAR ABSORBING MATERIALS WITH BROAD BANDWIDTH BY MIXING IRON NANOFIBERS WITH CARBONYL IRON PARTICLES[J]. 金属学报, 2008, 44(8): 1001-1005 .
[3] TONG Guo-Xing. INFLUENCES OF PYROLYSIS TEMPERATURE ON STATIC MAGNETIC AND MICROWAVE ELECTROMAGNETIC PROPERTIES OF POLYCRYSTALLINE IRON FIBERS[J]. 金属学报, 2008, 44(7): 867-870 .
[4] . [J]. 金属学报, 2001, 37(4): 445-448 .
No Suggested Reading articles found!