| HORIZONTAL CONTINUOUS CASTING OF Al-1wt%Si ALLOY CAST INGOTS UNDER ULTRASONIC FIELD |
| Xue-Peng GAO;;;;; |
| 大连理工大学材料科学与工程学院原材料特种制备重点实验室 |
|
Cite this article:
Xue-Peng GAO. HORIZONTAL CONTINUOUS CASTING OF Al-1wt%Si ALLOY CAST INGOTS UNDER ULTRASONIC FIELD. Acta Metall Sin, 2007, 42(1): 17-22 .
|
|
|
Abstract ABSTRACT In this paper, the effect of ultrasonic field during horizontal continuous casting of ?0mm Al-1wt%Si alloy bonding wire on the solidification has been investigated and the phenomenon has been theoretically interpreted. Experimental results showed that when the ultrasonic power of 1000W was imposed, the surface quality was improved, the surface roughness decreased from 40祄 to 10祄; the solidification structure was refined, the average grain size reduced from 94.1祄 to 31.2祄 and the mechanical properties were enhanced, not only the tensile strength and elongation increased by 20.5% and 37.5% respectively, but the hardness value increased by 23.9%. Meanwhile, the uniformity of the distribution of Si in ?(Al) was improved and the boundary segregation was suppressed, the fine globular microstructure of Si could be effectively obtained.
|
|
Received: 14 April 2006
|
|
|
[1] Qi G J,Zhang S.J Mater Process Technol,1997;68:288 [2] Strandjord A,Popelar S,Jauernig C.Microelect Reliab, 2002;42:265 [3] Ramminger S,Seliger N,Wachutka G.Microelect Reliab, 2000;40:1521 [4] Bai X Q,Li D H,Zhang L,He J C.Acta Metall Sin,2002; 38:483 (白晓清,李东辉,张林,赫冀成.金属学报,2002;38:483) [5] Abramov V,Abramov O,Bulgakov V,Sommer F.Mater Lett,1998;37:27 [6] Eskin G I.Ultrason Sonochem,2001;8:319 [7] Seifert J,Fischer F.Ultrasonics,1977;15:154 [8] Zhang H B,Zhai Q J,Qi F P,Gong Y Y.Trans Nonfer- rous Met Soc Chin, 2004;14:302 [9] Li X T,Li T J,Li X M,Jin J Z.Ultrason Sonochem,2006; 13:121 [10] Li X T,Li Q L,Li T J,Song Y Q,Zhang J L,Jin J Z.Chin J Nonferrous Met, 2004;14:2060 (李新涛,李丘林,李廷举,宋艳琴,张金利,金俊泽.中国有色金属学报,2004;14:2060) [11] Li Q L,Li X T,Li T J,Jin J Z,Liu W,Bao C G.J Xi'an Jiaotong Univ,2005;39:1003 (李丘林,李新涛,李廷举,金俊泽,刘伟,鲍崇高.西安交通大学学报,2005;39:1003) [12] Li X T,Li Q L,Li T J,Jin J Z.Rare Met Mater Eng, 2005;34(Suppl.2):80 (李新涛,李丘林,李廷举,金俊泽.稀有金属材料与工程,2005; 34(增刊2):80) [13]Kuijpers M W A,van.Eck D,Kemmere M F,Keurentjes J T F.Science,2002;298:1969 [14】Campbell J.Int Met Rev,1981;26:71 [15] Qi P X.Squeeze Casting.Beijing:National Defence In- dustry Press,1984:16 (齐丕骧.挤压铸造.北京:国防工业出版社, 1984:16) [16] Li S S,Zhao A M,Mao W M,Zhong X Y,Han Y F.Acta Metall Sin,2000;36:545 (李树索,赵爱民,毛卫民,钟雪友,韩雅芳.金属学报,2000; 36:545) [17] Xiong Y H,Li P J,Yang A M,Yan W D,Zeng I) B,Liu L.Acta Metall Sin,2002;38:534 (熊玉华,李培杰,杨爱民,严卫东,曾大本,刘林金属学报,2002;38:534) [18] Gong L Q,Li J G,Zhou P,Wang F Q,Tong Z S,Tao Z D. Chin J Nonferrous Met,2004;14:2003 (龚丽勤,李建国,周鹏,王发奇,仝仲盛,陶古东.中国有色金属学报, 2004;14:2003) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|