| SEM IN SITU OBSERVATIONS TO THE EFFECTS OF INCLUSIONS ON INITIATION AND PROPAGATION OF THE LOW CYCLIC FATIGUE CRACK IN SUPER STRENGTH STEEL |
| WANG Xishu; LIANG Feng; ZENG Yanping; XIE Xishan |
| Department of Engineering Mechanics; Tsinghua University; Beijing 100084 |
|
Cite this article:
WANG Xishu; LIANG Feng; ZENG Yanping; XIE Xishan. SEM IN SITU OBSERVATIONS TO THE EFFECTS OF INCLUSIONS ON INITIATION AND PROPAGATION OF THE LOW CYCLIC FATIGUE CRACK IN SUPER STRENGTH STEEL. Acta Metall Sin, 2005, 41(12): 1272-1276 .
|
|
|
Abstract SEM in situ observations for the effects of inclusions on the fatigue
crack initiation and propagation behaviors of super strength steel
indicate that the inclusion size and shape affect not only on the fatigue
crack initiation location but also on the crack growth behavior. At the
same time, the effects of inclusions on the fatigue crack initiation
are discussed by finite element method (FEM) analysis. The critical size
of inclusion in low cyclic fatigue crack propagation is proposed and the
influence of fatigue crack growth rate is estimated.
|
|
Received: 28 March 2005
|
| ZTFLH: |
TG111.8
|
|
| |
TB302.3
|
|
| |
O346.1
|
|
|
[1] Zhou S, Murakami Y, Beretta S, Fukushima Y. Mater Sci Technol, 2002; 18: 1535 [2] Pan T, Yang Z G, Bai B Z, Fang H S. Acta Metall Sin, 2003; 39: 1037 (潘涛,杨志刚,白秉哲,方鸿生.金属学报,2003;39:1037) [3] Goto H, Miyazawa K, Tanaka T. ISIJ Int, 1995; 5: 286 [4] Shih T Y, Araki T. Trans Irons Steel Inst Jpn, 1973; 13:11 [5] Wang X S, Li Y Q. Acta Mech Solid Sin, 2003; 16: 327 [6] Zhang J M, Zhang J F, Yang Z G, Li S X, Hui W J, Weng Y Q, Acta Metall Sin, 2004; 40: 846 (张继明,张建锋,杨振国,李守新,惠卫军,翁宇庆.金属学 报,2004;40:846) [7] Yang Z G, Zhang J M, Li S X, Chu Z M, Hui W J, Weng Y Q. Acta Metall Sin, 2004; 40: 367 (杨振国,张继明,李守新.褚作明,惠卫军,翁宇庆.金属学 报,2004;40:367) [8] Hui W J, Dong H, Weng Y Q, Shi J, Nie Y H, Chu Z M, Chen Y B. Acta Metall Sin, 2004; 40: 561 (惠卫军,董瀚,翁宇庆,时捷,聂义宏,褚作明,陈蕴博. 金属学报,2004;40:561) [9] Wang X S, Zhu S Q, Kawagoishi N, Nisitani H. Acta Metall Sin (Engl Lett), 2001; 14: 271 [10] Wang X S, Kawagoishi N. J Iron Steel Res Int, 2003; 10(2): 58 [11] Wang X S, Lu X, Wang D H. Mater Sci Eng, 2004; A364: 11 [12] Wang X S, Fan J H. J Mater Sci, 2004; 39: 2617 [13] Wang X S, Xu Y, Xu X Q. J Appl Comp Mater, 2004; 11: 145 [14] Wang X S, Xu Y. J Nucl Mater, 2004; 328(2-3): 243 [15] Wang X S, Li Y Q, Yu S W. J Exp Technol, 2003; 27(2): 31 [16] Murakami Y, Endo M. Eng Fract Mech, 1983; 17: 1 [17] Wu C Z, Shih T S. Mater Trans, 2003; 44: 995 [18] Murakami Y, Endo M. Int J Fatigue, 1994; 16; 163 [19] Yates Y, Shi G, Atkinson H V, Sellars C M, Anderson C W. Fatigue Fract Eng Mater Struct, 2002; 25: 667 [20] Wang X S, Zhang L N, Xie X S. J Mater Sci Technol, in press [21] Melander A. Int J Fatigue, 1990; 12: 154 [22] Tanaka T, Mura T. J Appl Mech, 1981; 48: 97 [23] Patton E M, Santare M H. Int J Fract, 1990; 46: 71 [24] Santare M H, Keer L M. Trans ASME, 1986; 53: 3821 |