CALCULATION OF SINGLE CRYSTAL MAGNETIC INDUCTION COEFFICIENTS IN A GRAIN ORIENTED SILICON STEEL STRIP
SHA Yuhui; LI Song; ZHOU Shichun; WANG Yandong; GAO Xiuhua; LIANG Zhide; ZUO Liang
School of Materials and Metallurgy; Northeastern University; Shenyang 110004
Cite this article: 

SHA Yuhui; LI Song; ZHOU Shichun; WANG Y; ong; GAO Xiuhua; LIANG Zhide; ZUO Liang. CALCULATION OF SINGLE CRYSTAL MAGNETIC INDUCTION COEFFICIENTS IN A GRAIN ORIENTED SILICON STEEL STRIP. Acta Metall Sin, 2004, 40(4): 445-448 .

Download:  PDF(135KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The calculation of single crystal magnetic induction coefficients from measured texture and magnetic induction data in a grain--oriented silicon steel strip has been discussed. A new method, based on an accurate reliability evaluation of measured magnetic property data and the fitting of texture components, was proposed. It was also shown that, instead of the experimental texture data obtained with X--ray diffraction technique, the fitted texture coefficients according to a Gaussian distribution model should be used in calculation.
Key words:  grain--oriented silicon steel      magnetic induction      single crystal property coefficient      
Received:  20 June 2003     
ZTFLH:  TG113.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I4/445

[1] Hutchinson W B, Seift J G. Texture, 1973; 1: 117
[2] Morris P R, Flowers J W. Texture of Crystalline Solids,1981; 4: 129
[3] Szpunar B, Szpunar J A. IEEE Trans on Magnetics, 1984;5: 1490
[4] Liang Z D, Xu J Z, Wang F. ODF Analysis of TexturedMaterials. Shenyang: Northeastern University Press,1986: 123(梁志德,徐家桢,王福.织构材料的三维取向分析术.沈阳:东北工学院出版社, 1986:123)
[5] Hirsch J, Lucke K. Textures Microstruct, 1988; 8-9: 131
[6] He Z Z. Electrical Steels. Beijing: Metallurgy Industry Press, 1996: 26(何忠治.电工钢.北京:冶金工业出版社, 1996:26)
[1] ZHENG Jincan, LIU Runcong, WANG Xiaodong. Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process[J]. 金属学报, 2020, 56(7): 929-936.
[2] Ming HE, Xianliang LI, Qingwei WANG, Lianyu WANG, Qiang WANG. Influence of Magnetic Shielding on the Power Loss of Induction Heating Power Supply in the Electro-magnetic Induction Controlled Automated Steel Teeming System[J]. 金属学报, 2019, 55(2): 249-257.
No Suggested Reading articles found!