| OXYGEN RERISING PHENOMENON DURING DEOXIDATION WITH SOLID ELECTROLYTE DEOXIDATION UNITS IN STEEL MELTS |
| LI Fushen; JIN Congjin; LU Xionggang; ZHOU Guozhi; ZHU Lixin; HU Xiaojun;LI Zeya; WANG Feng; SHEN Qiang |
| Department of Inorganic and Non-metal Materials; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
LI Fushen; JIN Congjin; LU Xionggang; ZHOU Guozhi; ZHU Lixin; HU Xiaojun; LI Zeya; WANG Feng; SHEN Qiang. OXYGEN RERISING PHENOMENON DURING DEOXIDATION WITH SOLID ELECTROLYTE DEOXIDATION UNITS IN STEEL MELTS. Acta Metall Sin, 2004, 40(7): 673-676 .
|
|
|
Abstract Deoxidation experiments using improved deoxidation unit are carried out
in 20 kg induction furnace. Experimental results prove that deoxidization
process is fast and effective. But the oxygen in melt
can not be decreased below 20X10-6 because oxygen in
melt is recovered by some experimental conditions such as
existing oxidizing slag and refractory or closed experimental system was
destroyed while measuring oxygen in melts and replacing deoxidation
unit.
|
|
Received: 28 July 2003
|
|
|
[1] Hu X J, Xiao L, Li F S, Li L F, Zhou G Z. Acta Metall Sin, 1999; 35(3) : 316(胡晓军,肖莉,李福燊,鲁雄刚,李丽芬,周国治.金属学报, 1999;35(3) :316) [2] Li F S, Lu X G, Li L F, Ou T, Zhou G Z. J Chin Rare Earth Soc. 2000;18(Spec. Issue): 258(李福燊,鲁雄刚,李丽芬,区铁,周国治.中国稀土学报,2000;18(专辑):258) [3] Li F S, Lu X G, Jin C J, Zhou G Z, Zhu L X, Hu X J, Li Z Y, Wang F, Shen Q. Acta Metall Sin, 2003; 39(3) : 287(李福燊,鲁雄刚,金从进,周国治,朱立新,胡晓军,李泽亚,王峰,沈强.金属学报,2003;39(3) :287) [4] Liang Y J, Che Y C. Thermodynamic Data Handbook of Inorganic Compounds. Shenyang: Northeastern University Press, 1993: 506, 507, 459, 464(梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:506,507,459,464) [5] Qu Y. Principle of Steelmaking, Beijing: Metallurgy Industry Press, 1980: 250(曲英.炼钢学原理.北京:冶金工业出版社, 1980:250) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|