| TWO DIMENTIONAL DISTRIBUTION OF FRICTION COMPONENTS FOR PLATE ROLLING |
| WANG MEI-YING Peking Institute of Iron and Steel |
|
Cite this article:
WANG MEI-YING Peking Institute of Iron and Steel. TWO DIMENTIONAL DISTRIBUTION OF FRICTION COMPONENTS FOR PLATE ROLLING. Acta Metall Sin, 1956, 1(3): 295-300.
|
|
|
Abstract This paper demonstrates a method of obtaining the surface distribution offriction components for plate rolling from the“rule of gradient”and experimentalpressure surface.An example was worked out.It appears that the surface dis-tribution of friction components is continuous except at the no-slip point,which isthe singular point for the case of slipping friction.The surface thus obtained serves as the boundary condition for the threedimentional problem of plate rolling.This result appears to be the first twodimentional distribution of friction components for plate rolling,and this methodis applicable to other cases such as forging.
|
|
Received: 18 March 1956
|
[1] Karman,T.H.,Z.ang.Math.u.Mech.,5,1925,p.p.139-41,On the Theory of Rolling. [2] #12 [3] Nadai,A.,Jourual of Applied Mechanics,p.p.A54-A62,Amer.Soc.Mech.Engs.,June 1939,The Forces Required for Rolling Steel Strip under Tension. [4] #12 [5] Orowan,E,Proc.I.Mech.E.,150(1943) ,No.4,p.p.140-67,The Calculation of Rolling Pressure in Hot and Cold Plat Rolling. [6] Brown,G.M.,Report to the Rolling Mill Research Sub-committee of the Iron and Steel Industrial Research Council,见Underwood,The Rolling of Metals. [7] 刘叔仪,物理学报十二卷一期,1956. [8] 刘叔仪,钢院学报第一辑,1955. [9] Hoff und Dall,Grundlagen Des Walzverfahrens,1950,Düsseldof. [10] Siebel,E.and Lueg,W.,Mitt.K.W.,Inst.Eisenf.,15(1933) ,p.p.1-14,Investigation into the Distribution of Pressure at the Surface of the Material in Contact with the Rolls. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|