| THE FORMATION OF CHI PHASE IN A Mo-BEARING STAINLESS STEEL |
| CHUANG YU-CHIH;LIU CHIA-LO;CHANG CHING-CHUNG Institute of Metal Research Academia Sinica |
|
Cite this article:
CHUANG YU-CHIH;LIU CHIA-LO;CHANG CHING-CHUNG Institute of Metal Research Academia Sinica. THE FORMATION OF CHI PHASE IN A Mo-BEARING STAINLESS STEEL. Acta Metall Sin, 1957, 2(1): 89-105.
|
|
|
Abstract The decompsition of δ-ferrite in the temperature range 550°—1000℃ inquenched 17/5/6 Cr-Ni-Mo Stainless steel specimens has been studied by meansof microscopic and X-ray diffraction method. It is shown that the nature of thedecomposition product of δ-ferrite varies with the reheating temperature, Chi andaustenite appeared in the temperature range 700—1000℃, Whereas below 700℃Fe_3Mo_3C and (Cr, Fe, Mo)_23C_6 were formed from δ-ferrite instead of Chi. The morphology and mechanism of Chi formation are also dependent on thereheating temperature. Above 900℃, δ-ferrite was found to decompose into Chiand austenite as eutectoid, the leading phase being probably Chi. Between 700℃and 900℃, it is likely that the nucleation of austenite couldnot keep pace withthat of Chi, thus Chi was found to precipitate first and the remaining δ-ferritethen transformed to austenite. Below 700℃ the precipitation of carbides in δ-ferrite was accompanied bymartensite formation in the austenitic matrix. This may be caused by the diffu-sion of carbon from the austenitic matrix to δ-ferrite to supply the carbon re-quired for the carbide precipitation.
|
|
Received: 18 January 1957
|
[1] Andrews, K. W., Nature, No. 4180 (1949) , 1015. [2] Andrews, K. W. and Brookes, P. E., Metal Treatment and Drop Forging (1951) , 301. [3] McMullin, J. G., Reiter, S. F. and Ebeling, D. G., Trans. Amer. Soc. Metals, 46 (1954) , 799. [4] Kasper, J. S., Acta Metallurgia, 2 (1954) , 456. [5] Koh, P. K. (郭本坚), Trans. Amer. Inst. Mining & Metallurgical Eng., 197 (1953) , 339. [6] Ver Snyder, F. L., Beattie, H. J., Trans. Amer. Soc. Metals, 47 (1955) , 211. [7] Birtalan, J. & Bloom, R. A., Journal of Metals, Feb. (1956) , 210. [8] Vacher, H. C. & Bechtoldt, C. J., Journal of Research, 53 (1954) , 67. [9] 庄育智、刘嘉乐,金属学报,1 (1956) ,385. [10] Gilman, J. J., Trans. Amer. Soc. Metals, 44 (1952) , 566. [11] Smith, C. S. Trans. Amer. Soc. Metals, 45 (1953) , 533. [12] Smoluchowski, R., Imperfections in Nearly Periect Crystals (Wiley, 1952) , 451. [13] Clark, C. L., High Temperature Alloys (Pitman, 1953) , 2. [14] Krivozok, V. N. & Grossman, M. A., Trans. Amer. Soc. Steel Treating, 18 (1930) , 760.
[15] Avery, H. S., Wilke, C. R & Fellows, J. A., Trans. Amer. Soc. Metals, 44 (1952) , 57. [16] Gilman J. J., Koh, P. K. (郭本坚) & Zmeskal, O., Trans. Amer Soc. Metals, 41 (1949) , 1371. [17] Bindari, A. E., Koh, P. K. (郭本坚) & Zmeskal, O., Trans. Amer. Soc. Metals. 43 (1951) , 226. [18] Morley, J. I., Symposium on High Temperature Steels and Alloys for Gas Turbines (London, 1951) , 195. [19] Jackson, J. H., Symposium on the Nature, Occurence & Effects of σ-phase (Philadelphia, 1951) , 110. [20] Nehrenberg, A. E. & Lilly, P., Trans. Amer. Soc. Metals, 46 (1954) , 1176. [21] Kuo, K. (郭可信), Journal of Iron & Steel Inst., 181 (1955) , 134. [22] Kuo, K. (郭可信), Journal of Iron and Steel Inst., 176 (1954) , 433. [23] Kuo, K. (郭可信), Journal of Iron & Stee1 Inst, 181 (1955) , 128. [24] Braumann, F. & Kraeter, H., Archiv Eisenhuettenw., 25 (1954) , 479. [25] Mehl, R. F. & Hagel, W. C., Progress in Metal Physics, No. 6 (London, 1956) , 74. [26] Nicholson, N. E., Journal of Metals, Sept. (1954) , 1071. [27] Koch, V. W. & Ilschner-Gensch, C., Archiv Eisenhuettenw, 27 (1956) , 453. [28] Goldschmidt, H. J., Trans. Amer. Soc. Metals, Discussions, 46 (1954) . [29] Cina, B., Journal Iron & Steel Inst., Disc., 184 (1956) , 58. [30] Nehrenberg, A. E., Journal Iron & Steel Inst., Disc., 184 (1956) , 60. |
| No Suggested Reading articles found! |
|
|